Abstract

An optimization method for a directional preparation technique and efficient use of semi-coke for blast furnace injection. Firstly, the volatile and the ash content of target semi-coke are preset, and then the volatile and the ash removal percentages of a raw coal are calculated; after ash removal, several sets of dry distillation carbonization temperatures and carbonization times are obtained according to the volatile removal percentage, and the relationships between a combustion rate, abrasiveness, explosiveness and jet flow property and the carbonization temperature are respectively established to obtain the optimal actual carbonization temperature; and semi-coke for blast furnace injection is obtained at an actual carbonization temperature. The directional preparation is suitable for the semi-coke for blast furnace injection, and an optimal coal-compounding scheme is obtained, thus achieving the efficient and safe injection of blast furnace iron-making fuels, and energy conservation and emission reduction.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (9 — 1 Independent, 8 Dependent)

  1. Claim 1Independent Claim

    A directional preparation technology of semi-coke for blast furnace injection, comprising performing dry distillation on raw coal to remove a portion of a volatile matter to prepare the semi-coke for blast furnace injection, and comprising the following steps: S11. according to a target value W A standard of an ash percentage of target semi-coke, obtaining a relational expression between an ash removal percentage W A removal in the raw coal and a volatile matter removal percentage W B removal during dry distillation, as shown in Formula (1): W A removal = W A coal - W A standard (1 - W B removal) 1 - W A standard (1) in the formula, W A coal represents a percentage of ash in the raw coal; the target value of the ash percentage meets W A standard ≤ 12%; S12. according to Formula (1) obtained in step S11, presetting a volatile matter removal percentage during dry distillation, wherein if the preset volatile matter removal percentage W B removal meets Formula (2), the raw coal is first subjected to ash removal treatment before carbonization; if the preset volatile matter removal percentage W B removal does not meet Formula (2), the raw coal is directly subjected to carbonization: W B removal ≥ W A standard - W A coal W A standard; (2) wherein a method for determining a carbonization temperature of dry distillation comprises: based on the preset volatile matter removal percentage W B removal, preliminarily determining a plurality of groups of carbonization temperatures and carbonization times of dry distillation through the pyrolysis behavior of dry distillation charring of the raw coal in a charring furnace, then, according to the plurality of groups of the carbonization temperatures and carbonization times, performing dry distillation and carbonization on the raw coal at different carbonization temperatures and carbonization times to prepare semi-coke, and respectively obtaining relationships between parameters comprising combustion rate, grindability index, explosibility index and jet flow index of the semi-coke and the carbonization temperature; wherein according to the relationship between the explosibility index and the carbonization temperature, selecting a carbonization temperature with an explosibility index ≤ 200 mm as a lower limit value of the carbonization temperature, and then, in a temperature intervals higher than the lower limit value of the carbonization temperature, according to the relationships between the combustion rate, the grindability index and the jet flow index and the carbonization temperature, selecting a temperature interval in which the combustion rate ≥ 80%, the grindability index ≥ 60 and the jet flow index ≥ 70 as an actual carbonization temperature of dry distillation of the raw coal, and then selecting an actual carbonization time based on the actual carbonization temperature; S13. if the preset volatile matter removal percentage W B removal meets Formula (2), first subjecting the raw coal to ash removal treatment, then performing dry distillation and carbonization at the actual carbonization time and the actual carbonization temperature determined in step S12, followed by cooling to obtain the semi-coke for blast furnace injection; if the preset volatile matter removal percentage W B removal does not meet Formula (2), performing dry distillation and carbonization of the raw coal at the actual carbonization temperature and actual carbonization time determined in step S12, followed by cooling to obtain the semi-coke for blast furnace injection.

  2. Claim 2Depends on #1

    The directional preparation technology of semi-coke for blast furnace injection according to claim 1, wherein in step S11, the target value of the ash percentage meets W A standard ≤ 9%.

  3. Claim 3Depends on #1

    The directional preparation technology of semi-coke for blast furnace injection according to claim 1, wherein in step S12, the method for ash removal treatment is heavy media coal processing technology treatment.

  4. Claim 4Depends on #1

    The directional preparation technology of semi-coke for blast furnace injection according to claim 1, wherein in step S12, CFD numerical simulation is used to establish a relationship between a heating gas temperature and the carbonization temperature, and then, heating gas temperatures corresponding to different carbonization temperatures are obtained according to the relationship between the heating gas temperature and the carbonization temperature.

  5. Claim 5Depends on #1

    The directional preparation technology of semi-coke for blast furnace injection according to claim 1, wherein in step S12, the explosibility index is a length of a return flame generated after ignition of the semi-coke determined by a long-tube type coal powder explosibility determining device.

  6. Claim 6Depends on #1

    The directional preparation technology of semi-coke for blast furnace injection according to claim 1, wherein in step S12, the actual carbonization temperature is 400-600 ° C.

  7. Claim 7Depends on #1

    The directional preparation technology of semi-coke for blast furnace injection according to claim 1, wherein in step S15, the cooling comprises adopts a dry quenching process, resulting in semi-coke for blast furnace injection with a full moisture content < 5%.

  8. Claim 8Depends on #1

    The directional preparation technology of semi-coke for blast furnace injection according to claim 1, wherein the directional preparation technology further comprises the following step: pulverizing the semi-coke for blast furnace injection to obtain pulverized semi-coke for blast furnace injection.

  9. Claim 9Depends on #8

    The directional preparation technology of semi-coke for blast furnace injection according to claim 8, wherein a mass percentage of the pulverized semi-coke for blast furnace injection with a particle size of less than 0.074 mm is not less than 75%.

Technical Overview & Description

CROSS REFERENCE TO RELATED APPLICATIONS This application is a 35 U.S.C. § 371 National Phase conversion of International (PCT) Patent Application No. PCT/CN2020/102745, filed on Jul. 17, 2020, the entire content of which is incorporated into this application herein by reference. The PCT International patent Application was filed and published in Chinese. TECHNICAL FIELD The disclosure belongs to the technical field of metallurgy, and particularly relates to a directional preparation technology of semi-coke for blast furnace injection and an optimization method for efficient use of semi-coke for blast furnace injection. BACKGROUND Blast furnace iron-making is currently under great pressure to meet the requirements of energy saving and emission reduction. Blast furnace coal injection is an important technical means to reduce coke consumption in blast furnace iron-making, and is of great significance for blast furnace iron-making to reduce the consumption of scarce coking coal resources and reduce pollution emissions during the coke production process. However, traditional blast furnace coal injection mainly uses high-quality anthracite resources. Anthracite has very few reserves in China and is a non-renewable resource, and its scarcity continues to become prominent. Therefore, Chinese iron smelters have been working hard to extend the scope of fuels for blast furnace injection. As a by-product from low-rank coal after oil extraction and modification in the coal chemical industry, semi-coke is much cheaper than coke, and has a large production capacity in China. In recent years, researchers have proposed the use of semi-coke as a raw material for blast furnace injection based on the advantages of high fixed carbon content, low sulfur content, low ash content, and the like of the semi-coke. For example, Chinese invention patent CN201210018465.0 has disclosed a low-cost blast furnace iron-making method, in which semi-coke is introduced into blast furnace injection for s

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (10)

Non-Patent Literature (7)

  • English-language machine translation of CN 105907413 A (Year: 2016).
  • English-language machine translation of CN 107189794 A (Year: 2017).
  • Chong Zou, Bao Li, Junxue Zhao, Xiaoming Li,
  • “
  • Effects of Pyrolysis Temperature on Grindability of Char Using Pulverized Coal Injection in Blast Furnace
  • ”
  • , Clean Coal Technology, Jan. 2016, pp. 71-76, vol. 22, Issue No. 1, China Academic Journal Electronic Publishing House.