Method of surface structuring a substrate body and substrate body
Abstract
A method for preparing and/or carrying out the structuring of a predetermined or predeterminable distinguished surface of a substrate body having a substrate material includes exposing the substrate material in at least one curved effective area to an electromagnetic field which in each of the at least one curved effective area causes a non-linear interaction between the electromagnetic field and the substrate material, and thus at least partially influencing the substrate material arranged in the curved effective area. After the structuring of the distinguished surface the distinguished surface has at least in certain areas at least one first curved progression which is at least partially determined and/or influenced by the curved shape of the at least one curved effective area. The nonlinear interaction causes at least one nonlinear absorption of the electromagnetic field in the substrate material.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A method for preparing and/or carrying out a structuring of a predetermined or predeterminable distinguished surface of a substrate body comprising a substrate material, the method comprising: exposing at least one curved effective area of the substrate material to an electromagnetic field which causes a non-linear interaction between the electromagnetic field and the substrate material in the at least one curved effective area, and thus at least partially influencing the substrate material arranged in the at least one curved effective area; and increasing or decreasing at least one property selected from the group consisting of: the refractive index, the etch rate, and the density of the substrate material, at least in certain areas, wherein, after the structuring, the distinguished surface comprises, at least in certain areas, at least one first curved progression which is at least partially determined and/or influenced by the curved shape of the at least one curved effective area, w
- Claim 2Depends on #1
The method according to claim 1, wherein the substrate material is exposed to an electromagnetic field in a plurality of curved effective areas, and wherein (i) the distinguished surface has the same first curved progression at several areas, determined or influenced by the curved shape of the plurality of curved effective areas, and/or has the first curved progression everywhere, and/or (ii) the curved effective areas are selected to be arranged at a distance from one another, wherein in a cross-sectional plane of the substrate body the centers or centroids of the intersecting surfaces of the plurality of curved effective areas with the cross-sectional plane extend along a straight line or along any desired circular, curve, and/or successive effective areas have a distance from one another which is between either 30% and 100% or between 100% and 200% of the maximum extent of the plurality of curved effective areas in the cross-sectional plane.
- Claim 3Depends on #1
The method according to claim 1, further comprising: at least partially removing and/or displacing the substrate material from the at least one curved effective area.
- Claim 4Depends on #3
The method according to claim 3, wherein the distinguished surface is formed by at least partially removing the substrate material by the influencing and/or by at least partially removing at least the influenced substrate material by at least one subsequent etching process or by an acid and/or by a caustic solution.
- Claim 5Depends on #1
The method according to claim 1, wherein the laser beam is provided by an ultrashort pulse laser, wherein the phase of the laser beam is adjusted and/or adapted by a spatial light modulator, of a diffractive optical element and/or a combination of several cylindrical lenses, wherein the laser beam is focused onto the substrate body by a microscope objective or a Fourier lens, wherein the focusing takes place after adjusting or adapting the phase of the laser beam and/or forms the line focus, wherein the line focus is that of an accelerated laser beam, wherein the wavelength of the laser beam is 1064 nm, the microscope objective or the Fourier lens has a focal length of 10-20 mm, the coefficient of the cubic phase (laser parameter beta) has a value between 0.5 × 10 3 /m and 5 × 10 3 /m, the diameter of the raw beam (laser parameter coo) has a value between 1 mm and 10 mm, the pulse duration (laser parameter c) has a value of 0.1-10 ps, the pulse energy (laser parameter Ep) has a value b
- Claim 6Depends on #1
The method according to claim 1, wherein, at least during the non-linear interaction, at least one auxiliary substrate body is arranged at the substrate body and the curved effective area and/or the line focus extends at least partially into the auxiliary substrate body, wherein two or more auxiliary substrate bodies are arranged at the substrate body on opposite sides of the substrate body, and the curved effective area and/or the line focus extends at least partially into two or more auxiliary substrate bodies.
- Claim 7Depends on #1
The method according to claim 1, wherein at least one and/or all of the curved effective areas of the at least one curved effective area is completely enclosed within the substrate body at least during the non-linear interaction, and the method further comprising: removing at least along a major direction of extension of the at least one curved effective area within the substrate body, and thereby making the substrate material influenced in the enclosed curved effective area at least partially and/or in certain areas accessible from the outside, wherein the removal of material from the substrate body is carried out by etching.
- Claim 8Depends on #1
The method according to claim 1, wherein the at least one curved effective area is a plurality of curved effective areas, wherein the substrate material is exposed to the electromagnetic field successively or wholly or partially in parallel in each of the plurality of curved effective areas, wherein the entire substrate material within a curved effective area is simultaneously exposed to the electromagnetic field, and wherein the plurality of curved effective areas each have a maximum deflection from a straight progression of more than 20 μ m, and/or wherein the length of the plurality of curved effective areas is respectively more than 0.1 mm.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS The present application claims priority to European Patent Application EP20194675.3, filed on Sep. 4, 2020, and European Patent Application EP21159715.8, filed on Feb. 26, 2021, the entire contents of each of which are incorporated by reference herein. BACKGROUND OF THE DISCLOSURE 1. Field of the Disclosure The present disclosure relates to a method for preparing and/or performing the structuring of a surface of a substrate body. The disclosure also relates to a substrate body. 2. Description of the Related Art In order to process a starting substrate so that a predetermined surface, such as a separation surface, is formed, prior art separation processes by scoring and breaking, wheel cutting, laser-based thermal separation, i.e. mechanically pre-damaging the substrate and guiding a crack through a thermal stress field in the material, and laser-based perforation separation, i.e. filamenting along a contour and subsequent mechanical or thermal separation along the perforation, are known. However, these processes have the disadvantage that the predetermined target surface is often not achieved. This is sometimes due to the pre-damages of the substrate material, which are also deliberately introduced, which, however, cannot be adequately controlled. It is therefore an object of the present disclosure to be able to reliably form a planned surface in a substrate body. SUMMARY OF THE DISCLOSURE The object is achieved according to a first aspect of the disclosure in that a method for preparing and/or carrying out the structuring of a predetermined or predeterminable distinguished surface of a substrate body comprising a substrate material, wherein the method comprises exposing the substrate material in at least one curved effective area to an electromagnetic field which in each of the at least one curved effective area causes a non-linear interaction between the electromagnetic field and the substrate material, and thus at least par
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (11)
| Patent | Title | Year | Citations |
|---|---|---|---|
| WO 2021/076432 A1 | Foldable apparatus and methods of making | — | 0 |