hottub.patents
US 12,482,802 B2#2218486 Most CitedActiveUnited States (USPTO)Utility

Method for tuning lithium wettability of an anode current collector using plasma surface modification

1Forward Citations (#2218486 Global)
1.0/yrCitation Velocity (#2218486 Global)
0.17Citation PageRank (#2218486 Global)
11Prior Art Cited
20Claims (3 Indep. · 17 Dep.)
6Drawings / Sheets

Abstract

A method for manufacturing an anode electrode includes supplying an anode current collector; coating a first portion of the anode current collector with a precursor coating; not coating a second portion of the anode current collector with the precursor coating; treating the anode current collector with plasma to at least one of decrease lithium wettability of the first portion and to increase lithium wettability of the second portion; and coating the anode current collector with lithium metal to form an anode active material layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.

Claims (20 — 3 Independent, 17 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing an anode electrode, comprising: supplying an anode current collector; coating a first portion of the anode current collector with a lithiophilic coating; not coating a second portion of the anode current collector with the lithiophilic coating; treating the anode current collector with plasma to at least one of decrease lithium wettability of the first portion by facilitating a chemical reaction of the lithiophilic coating and to increase lithium wettability of the second portion; and coating the anode current collector with lithium metal to form an anode active material layer, wherein coating the anode current collector with the lithium metal comprises supplying lithium metal powder at spaced intervals on the anode current collector using an engraved roller including a plurality of cavities and heating the lithium metal powder to melt the lithium metal powder.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the first portion corresponds to an edge of the anode current collector.

  3. Claim 3Depends on #1

    The method of claim 1, wherein coating the anode current collector with lithium metal comprises passing the anode current collector through a bath including molten lithium metal.

  4. Claim 4Depends on #3

    The method of claim 3, further comprising directing gas at the anode current collector after the anode current collector passes through the bath to at least one of remove excess molten lithium metal and improve thickness uniformity of the molten lithium metal.

  5. Claim 5Depends on #4

    The method of claim 4, wherein the gas is selected from a group consisting of molecular nitrogen and argon.

  6. Claim 6Depends on #1

    The method of claim 1, further comprising injecting a secondary gas into the plasma, wherein the secondary gas includes at least one element that creates bonds on a surface of the anode current collector that increases wettability to lithium.

  7. Claim 7Depends on #1

    The method of claim 1, wherein coating the anode current collector with the lithium metal comprises supplying molten lithium metal onto the anode current collector using a coating device.

  8. Claim 8Depends on #1

    The method of claim 1, further comprising heating the engraved roller to melt the lithium metal powder.

  9. Claim 9Depends on #1

    The method of claim 1, wherein heating the lithium metal powder comprises heating using at least one of plasma, infrared heating, a furnace, an oven, and induction heating.

  10. Claim 10Depends on #1

    The method of claim 1, further comprising supplying a plasma gas for the plasma that includes one or more elements selected from a group consisting of nitrogen (N), phosphorus (P), oxygen (O), a halogen, and/or combinations thereof.

  11. Claim 11Depends on #1

    The method of claim 1, further comprising supplying a plasma gas for the plasma selected from a group consisting of molecular nitrogen (N 2), ammonia (NH 3), an amine compound, a silazane, and/or combinations thereof.

  12. Claim 12Depends on #1

    The method of claim 1, further comprising treating the anode current collector with plasma comprising molecular oxygen prior to coating the first portion of the anode current collector with the lithiophilic coating.

  13. Claim 13Depends on #1

    The method of claim 1, wherein the anode current collector is made of stainless steel and further comprising heating the second portion of the anode current collector to a temperature in a range from 250 ° C. to 400 ° C. prior to treating the anode current collector with plasma.

  14. Claim 14Depends on #13

    The method of claim 13, further comprising cooling the first portion of the anode current collector to a temperature in a range from 10 ° C. to 25 ° C. prior to treating the anode current collector with plasma.

  15. Claim 15Independent Claim

    A method for manufacturing an anode electrode, comprising: supplying an anode current collector; coating a first portion of the anode current collector with a lithiophilic coating wherein the first portion corresponds to an edge of the anode current collector; not coating a second portion of the anode current collector with the lithiophilic coating, wherein the second portion corresponds to a location where an anode active material layer of the anode current collector is arranged; treating the anode current collector with plasma to at least one of decrease lithium wettability of the first portion by facilitating a chemical reaction of the lithiophilic coating and to increase lithium wettability of the second portion, wherein a plasma gas for the plasma includes one or more elements selected from a group consisting of molecular nitrogen (N 2), ammonia (NH 3), an amine compound, a silazane, and/or combinations thereof; and coating the anode current collector with lithium metal to form the anode active material layer by passing the anode current collector through a bath including molten lithium metal, wherein coating the anode current collector with the lithium metal comprises supplying lithium metal powder at spaced intervals on the anode current collector using an engraved roller including a plurality of cavities and heating the lithium metal powder to melt the lithium metal powder.

  16. Claim 16Depends on #15

    The method of claim 15, further comprising directing gas at the anode current collector after the anode current collector passes through the bath to at least one of remove excess molten lithium metal and improve thickness uniformity of the molten lithium metal, wherein the gas is selected from a group consisting of molecular nitrogen and argon.

  17. Claim 17Depends on #15

    The method of claim 15, further comprising injecting a secondary gas into the plasma.

  18. Claim 18Depends on #15

    The method of claim 15, further comprising treating the anode current collector with oxygen plasma prior to coating the first portion of the anode current collector with the lithiophilic coating.

  19. Claim 19Independent Claim

    A method for manufacturing an anode electrode, comprising: supplying an anode current collector; coating a first portion of the anode current collector with a lithiophilic coating; not coating a second portion of the anode current collector with the lithiophilic coating; treating the anode current collector with plasma to at least one of decrease lithium wettability of the first portion by facilitating a chemical reaction of the lithiophilic coating and to increase lithium wettability of the second portion; and coating the anode current collector with lithium metal to form an anode active material layer, wherein the method further includes cooling the first portion of the anode current collector to a temperature in a range from 10 ° C. to 25 ° C. prior to treating the anode current collector with plasma.

  20. Claim 20Depends on #19

    The method of claim 19, wherein coating the anode current collector with the lithium metal comprises: supplying lithium metal powder at spaced intervals on the anode current collector using an engraved roller including a plurality of cavities; and heating the lithium metal powder to melt the lithium metal powder.

Technical Overview & Description

INTRODUCTION The information provided in this section is for the purpose of generally presenting the context of the disclosure. Work of the presently named inventors, to the extent it is described in this section, as well as aspects of the description that may not otherwise qualify as prior art at the time of filing, are neither expressly nor impliedly admitted as prior art against the present disclosure. The present disclosure relates to battery cells, and more particularly to a method for manufacturing anode electrodes. Electric vehicles (EVs) such as battery electric vehicles (BEVs), hybrid vehicles, and/or fuel cell vehicles include one or more electric machines and a battery system including one or more battery cells, modules, and/or packs. A power control system is used to control charging and/or discharging of the battery system during charging and/or driving. Battery cells include one or more cathode electrodes, anode electrodes, and separators. The cathode electrodes include a cathode active material layer (including cathode active material) arranged on a cathode current collector. The anode electrodes include an anode active material layer (including anode active material) arranged on an anode current collector. SUMMARY A method for manufacturing an anode electrode includes supplying an anode current collector; coating a first portion of the anode current collector with a lithiophilic coating; not coating a second portion of the anode current collector with the lithiophilic coating; treating the anode current collector with plasma to at least one of decrease lithium wettability of the first portion and to increase lithium wettability of the second portion; and coating the anode current collector with lithium metal to form an anode active material layer. In other features, the first portion corresponds to an edge of the anode current collector. Coating the anode current collector with lithium metal comprises passing the anode current collector through a bat

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (10)

  • Lin
  • “
  • New strategy to significantly improve the wettability of various metals by molten lithium
  • ”
  • (2024).
  • Wang et al.
  • “
  • Fundamental study on the wetting property of liquid lithium
  • ”
  • (2018).