Lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material and preparation method therefor

0Forward Citations (#3386835 Global)
0.0/yrCitation Velocity (#3386835 Global)
0.00Citation PageRank (#3386835 Global)
23Prior Art Cited
3Structured Claims
0Drawings / Sheets

Abstract

A method of preparing lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material comprises the following steps: mixing and ball milling nickel cobalt manganese hydroxide with a lithium source, zirconium oxide, tungsten oxide, and sodium carbonate, then performing primary sintering, pulverizing, and then obtaining an lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material intermediate, the temperature of the primary sintering being 50-150 ° C. higher than a normal sintering temperature; and evenly mixing the lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material intermediate and a coating agent, and then performing secondary sintering to obtain the lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 0.

Claims (3)

  1. Claim 1Independent Claim

    A method for preparing a lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material, wherein the method comprises the following steps: mixing and ball milling nickel cobalt manganese hydroxide with a LiOH · H 2 O, zirconium oxide, tungsten oxide and sodium carbonate, then performing primary sintering, pulverizing and then obtaining a lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material intermediate, wherein: a molar ratio of the nickel cobalt manganese hydroxide to zirconium oxide, tungsten oxide, and sodium carbonate is 1:0.002:0.0016:0.002, the chemical composition of the nickel cobalt manganese hydroxide is Ni 0.80 Co 0.10 Mn 0.10 (OH) 2; a molar ratio of the nickel cobalt manganese hydroxide to lithium in the LiOH · H 2 O is 1:1.05, and the temperature of the primary sintering is 950 ° C., a time of the primary sintering is 15 h; evenly mixing the lithium nickel manganese cobalt oxide high-nickel single-cryst

  2. Claim 2Depends on #1

    The method for preparing a lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material according to claim 1, wherein the primary sintering process and the secondary sintering process are all preformed under oxygen conditions.

  3. Claim 3Independent Claim

    A method for preparing a lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material, wherein the method comprises the following steps: mixing and ball milling nickel cobalt manganese hydroxide with a LiOH · H 2 O, zirconium oxide, tungsten oxide and sodium carbonate, then performing primary sintering, pulverizing and then obtaining a lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material intermediate; wherein a molar ratio of the nickel cobalt manganese hydroxide to zirconium oxide, tungsten oxide, and sodium carbonate is 1:0.002:0.0016:0.002; the chemical composition of the nickel cobalt manganese hydroxide is Ni 0.80 Co 0.10 Mn 0.10 (OH) 2; a molar ratio of the nickel cobalt manganese hydroxide to lithium in the LiOH · H 2 O is 1:1.02; the temperature of the primary sintering is 950 ° C.; a time of the primary sintering is 15 h; evenly mixing the lithium nickel manganese cobalt oxide high-nickel single-crystal po

Technical Overview & Description

PRIORITY CLAIM This is a U.S. national stage of application No. PCT/CN2022/108807, filed on Jul. 29, 2022. Priority is claimed on the following application: China Patent Application No.: 202111653919.7 filed on Dec. 30, 2021, the entire content of which is incorporated here by reference. TECHNICAL FIELD The present application relates to the technical field of lithium batteries, and in particular to a lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material and a preparation method thereof. BACKGROUND LiNi x Co y Mn 1-x-y O 2 ternary positive electrode materials have been widely used in lithium-ion secondary batteries due to their high specific capacity and energy density, low cost and relatively environmentally friendly characteristics. Especially in the current context, they have broad development space in the automotive power battery market. With the increase in cruising range, the current positive electrode materials are gradually developing towards high nickel and high voltage. Single-crystal positive electrode materials have attracted much attention due to their advantages of relatively high electrode plate compaction and low gas production. However, there are two problems in the sintering process of high-nickel single-crystal materials: first, when the sintering temperature is slightly lower, although the discharge specific capacity is high, the single-crystals are aggregated and the dispersion is poor, resulting in a decreased cycle performance and increased gas production; second, when the sintering temperature is high, the single-crystal size is large and the dispersion is good, but the discharge specific capacity is significantly reduced. Therefore, how to prepare high-nickel single-crystal positive electrode materials with high capacity, large size and high dispersibility remains a huge challenge. SUMMARY OF THE INVENTION The purpose of the present invention is to overcome the above-mentioned technical deficiencies, pr

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (23)

PatentTitleYearCitations

Non-Patent Literature (7)

  • International Search Report issued on Oct. 26, 2022 for related PCT /CN2022/108807.
  • Written Opinion issued on Oct. 26, 2022 for related PCT /CN2022/108807.
  • First Office Action issued on Apr. 26, 2023 for related China Patent Application No. 202111653919.7.
  • Second Office Action issued on Dec. 27, 2023 for related China Patent Application No. 202111653919.7.
  • Office Action issued on Nov. 8, 2024 for related Korean Patent Application No. 10-2024-7025021.
  • Office Action issued on Jan. 28, 2025 for related Japanese Patent Application No. 2 0 2 4-5 3 9 6 1 5.
  • Search Report dated Jun. 17, 2025 for European patent application No. 22913338.4.