Method and systems for metal doping on battery cathode materials
Abstract
Methods and systems are provided for a battery cathode material comprising greater than or equal to 60% nickel content, the cathode material having at least one metal doped therein. In one example, a method comprises doping the at least one metal into the cathode material using water as a solvent, wherein the at least one metal has an ionic radii greater than 60 picometers. The at least one metal may be selected from strontium (Sr), barium (Ba), rubidium (Rb), cesium (Cs), zirconium (Zr), niobium (Nb), molybdenum (Mo), technetium (Tc), ruthenium (Ru), tungsten (W), platinum (Pt), neodymium (Nd), yttrium (Y), and cerium (Ce).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A method, comprising: dissolving a dopant salt in water, the dopant salt comprising one or more metals having ionic radii greater than 60 picometers; forming a nickel, manganese, and cobalt oxide (NMC) cathode material by mixing an NMC precursor with a lithium salt and sintering; after sintering to form the NMC cathode material, forming a mixture of the NMC cathode material with the dissolved dopant salt in the water; and heating the mixture to form a doped cathode material, wherein heating the mixture occurs immediately after forming the mixture and gradually evaporates the water, and wherein the dopant salt is uniformly deposited at a surface of the NMC cathode material as an amount of water decreases and lithium re-enters the NMC cathode material.
- Claim 2Depends on #1
The method of claim 1, wherein the one or more metals are selected from one or more of strontium (Sr), barium (Ba), rubidium (Rb), cesium (Cs), zirconium (Zr), niobium (Nb), molybdenum (Mo), technetium (Tc), ruthenium (Ru), tungsten (W), platinum (Pt), neodymium (Nd), samarium (Sm), cerium (Ce), yttrium (Y), praseodymium (Pr), and lanthanum (La).
- Claim 3Depends on #1
The method of claim 1, wherein the ionic radius of each of the one or more metals is 1.5 times greater than an ionic radius of nickel.
- Claim 4Depends on #3
The method of claim 3, wherein the doped cathode material comprises greater than or equal to 60% nickel by weight.
- Claim 5Depends on #1
The method of claim 1, wherein the dopant salt is NdI 3.
- Claim 6Depends on #1
The method of claim 1, wherein the dopant salt is Nd(NO 3) 3.
- Claim 7Depends on #1
The method of claim 1, wherein the dopant salt is Y(NO 3) 3.
- Claim 8Depends on #1
The method of claim 1, wherein the dopant salt is Y(CH 2 COOH) 3.
Technical Overview & Description
CROSS REFERENCE TO RELATED APPLICATIONS The present application is a US National Phase Application of International Patent Application Serial No. PCT/US2018/062134 entitled “ METHOD AND SYSTEMS FOR METAL DOPING ON BATTERY CATHODE MATERIALS, ” filed on Nov. 20, 2018. International Patent Application Serial No. PCT/US2018/062134_claims priority to U.S. Provisional Application No. 62/590,175, entitled “ METHOD AND SYSTEMS FOR METAL DOPING ON BATTERY CATHODE MATERIALS ” , and filed on Nov. 22, 2017. The entire contents of the above-listed applications are hereby incorporated by reference for all purposes. FIELD The present description relates generally to methods to synthesize and implement cathodes comprising metal doping and a high concentration of Ni in lithium ion batteries. BACKGROUND AND SUMMARY Lithium (Li) ion batteries may be desired due to their high energy density. Li ion batteries have become ubiquitous and may be found in a wide range of electrically powered or electrically assisted devices, such as vehicles, phones, audio devices, laptops, and the like. During the charging process of a Li ion battery, a power source may promote the movement of Li ions from a cathode material crystal structure, to an adjacent electrolyte, and finally to an anode surface, where the Li may intercalate into an anode material structure. The forced movement of the Li ions from cathode to anode may cause collapse of the cathode crystal structure and leave nickel (Ni) ions in a highly reactive valence state. The vacant Li ion sites may be prone to Ni ion migration, where the Ni may migrate from a metal oxide layer of the cathode to form a rock salt phase during the charging. As a result, a structure of the cathode may be degraded and may block Li ion transport back to the cathode during a discharge, thereby decreasing an overall power output and longevity of the Li battery. At an end of charge process, Li extraction from the cathode may not provide enough electrons demanded by a p
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (20)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (10)
- Wawrzynczyk et al. (
- “
- Neodymium(III) doped fluoride nanoparticles as non-contact optical temperature sensors
- ”
- , Nanoscale, 2012, 4, 6959-6961) (Year: 2012).
- Breviglieri et al. (
- “
- Correlation between ionic radius and thermal decomposition of Fe(II), Co(II), Ni(II), Cu(II) and Zn(II) diethanoldithiocarbamates
- ”
- , Thermochimica Acta 356 (2000) 79-84) (Year: 2000).