Method for producing high nickel lithiated metal oxide for battery
Abstract
A method for preparing high nickel lithiated metal oxides that includes selecting one or more nickel precursors; at least one non-corrosive lithium salt; and a plurality of metal oxide or hydroxide precursors. The metal precursors and lithium salts are mixed together to form a mixture comprising: Li x Ni y M z N (1 − y − z) O (2 − a) Fa (F-1) wherein x=1.0-1.1, 0.80 ≤ y ≤ 0.90, 0.03 < z ≤ 0.15, and 0 ≤ a ≤ 0.05; M is Co or Fe; and N is Al, Mn, Fe, Ca, Mg, Ti, Cr, Nb, Mo, W, B, or a mixture thereof provided N may be Fe when M is Co. The mixture is subjected to sintering (1st step) in air at ≥ 750 ° C. to form a powder. The powder is subjected to a 2 nd sintering step in O 2 at ≤ 750 ° C. to form the high nickel lithiated metal oxides.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.
Claims (16 — 1 Independent, 15 Dependent)
- Claim 1Independent Claim
A process for preparing high nickel lithiated metal oxides, the process comprising: a. Selecting one or more nickel precursors; b. Providing at least one non-corrosive lithium salt; c. Delivering a plurality of metal oxide or hydroxide precursors; wherein at least one of the metal oxide/hydroxide precursors comprises cobalt (Co), iron (Fe) or a combination thereof and at least another metal oxide/hydroxide precursor includes aluminum (Al), manganese (Mn), calcium (Ca), magnesium (Mg), titanium (Ti), chromium (Cr), niobium (Nb), molybdenum (Mo), tungsten (W), boron (B), or a combination thereof; d. Mixing the one or more nickel precursors, the at least one non-corrosive lithium salt, and the plurality of metal oxide/hydroxide precursors together to form a mixture; e. Spray drying the mixture to form a powder; and f. Subjecting the powder to a 1 st sintering step and then to a 2 nd sintering step to form the high nickel lithiated metal oxides comprising: Li x Ni y M z N (1 − y − z) O (2 − a) Fa (F-1) wherein x=1.0-1.1, 0.80 ≤ y ≤ 0.90, 0.03 < z ≤ 0.15, and 0 ≤ a ≤ 0.05, M is Co or Fe; and N is Al, Mn, Fe, Ca, Mg, Ti, Cr, Nb, Mo, W, B, or a mixture thereof, provided N may be Fe when M is Co; wherein the 1 st sintering step is performed in an air environment at a temperature ≥ 750 ° C.; and wherein the 2 nd sintering step is performed in an O 2 environment at a temperature ≤ 750 ° C.
- Claim 2Depends on #1
The process according to claim 1, wherein the M in formula (F-1) is cobalt.
- Claim 3Depends on #2
The process according to claim 2, wherein the y in formula (F-1) is 0.80 ≤ y ≤ 0.87.
- Claim 4Depends on #3
The process according to claim 3, wherein the y in formula (F-1) is 0.80 ≤ y ≤ 0.85.
- Claim 5Depends on #2
The process according to claim 2, wherein N in formula (F-1) is Al.
- Claim 6Depends on #2
The process according to claim 2, wherein N in formula (F-1) is Mn.
- Claim 7Depends on #2
The process according to claim 2, wherein N in formula (F-1) is Al and Mn with a molar ratio of Al/Mn ranging from 0.99/0.01 to 0.01/0.99.
- Claim 8Depends on #2
The process according to claim 2, wherein N in formula (F-1) is Al, Mn, and either Fe or Mo with a molar ratio of Al/Mn/(Fe — Mo) ranging from 0.99/0.05/0.05 to 0.05/0.99/0.05 to 0.05/0.05/0.99.
- Claim 9Depends on #1
The process according to claim 1, wherein the O 2 environment of the 2 nd sintering step is pure oxygen.
- Claim 10Depends on #1
The process according to claim 1, wherein the 1 st sintering step has a temperature that is ≥ 750 ° C. and ≤ 1000 ° C.
- Claim 11Depends on #10
The process according to claim 10, wherein the temperature in the 1 st sintering step is ≥ 800 ° C. and ≤ 950 ° C.
- Claim 12Depends on #11
The process according to claim 11, wherein the temperature in the 1 st sintering step is ≥ 850 ° C. and ≤ 900 ° C.
- Claim 13Depends on #1
The process according to claim 1, wherein the 1 st sintering step is performed with a sintering time that is in a range of 2 hours to 24 hours.
- Claim 14Depends on #1
The process according to claim 1, wherein the temperature in the 2 nd sintering step is ≤ 750 ° C. and ≥ 700 ° C.
- Claim 15Depends on #14
The process according to claim 14, wherein the 2 nd sintering step is performed with a sintering time that is in a range of 2 hours to 24 hours.
- Claim 16Depends on #14
The process according to claim 14, wherein the sintering time of the 2 nd sintering step is longer than the sintering time of the 1 st sintering step.
Technical Overview & Description
CROSS REFERENCE TO RELATED APPLICATIONS This application claims the benefit of the filing date under 35 U.S.C. § 119 (e) of U.S. Provisional Application No. 63/227,483 filed Jul. 30, 2021, the entire contents of which is hereby incorporated herein by reference. FIELD This invention generally relates to a method of manufacturing cathode active materials for use in an electrochemical cell, such as a battery. More specifically, the present disclosure describes a method for producing high nickel or nickel-rich lithiated metal oxides. BACKGROUND The statements in this section merely provide background information related to the present disclosure and may not constitute prior art. In conventional processes used to manufacture lithium ion batteries, high nickel cathode materials, such as Li x Ni y CO z M (1 − y − z) O 2 , where M is aluminum (Al) and/or manganese (Mn), x ≥ 0.8, and y ≤ 0.15, are required to be produced using lithium hydroxide (LiOH) as the lithium source in an oxygen (O 2 ) environment at a high temperature (e.g., ≥ 700 ° C.). In a typical production process, Ni(II) sulfate, Co(II) sulfate, Al (III) sulfate, and/or Mn (II) sulfate is dissolved in water and then co-precipitated upon the addition of a mixture of sodium hydroxide and ammonium hydroxide. The hydroxide materials that precipitate are then washed, dried, and blended with LiOH*H 2 O. The resulting blend or mixture is sintered at 750 ° C. in an O 2 environment to form the lithiated high nickel metal oxides. In this process, O
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (10)
Non-Patent Literature (10)
- Machine Translation of CN-112125353-A (Mar. 3, 2025) (Year: 2025).
- Machine Translation of CN-104051709-A (Mar. 3, 2025) (Year: 2025).
- Machine Translation of KR-20180027261-A (Mar. 3, 2025) (Year: 2025).
- Ge Wujie et al:
- “
- Effects of reheating temperature on the structure, morphology and electrochemical performance of Ni-rich cathode materials,
- ”
- Journal of Alloys and Compounds, vol. 876, Apr. 24, 2021.
- Park Nam-Yung et al:
- “