Composite treatment and remediation technology for polluted water and soil
Abstract
The present invention relates to a composite treatment and recovery technique of polluted water body and soil. Iron-rich straw biomass, after being crushed, is mixed and granulated with sludge, and is pyrolytic charred by programmed heating, to obtain bulk loaded zero-valent iron biochar and sludge biochar composite particles, which are packed as fillers in a filled bed or as filters in filter cells of a fixed bed, for effective recovery of complex polluted water, polluted by heavy metals, organics, nitrogen, phosphorus, and the like.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.
Claims (13 — 1 Independent, 12 Dependent)
- Claim 1Independent Claim
A process comprising: passing polluted water through either a) a filled bed of bulk loaded composite particles or through b) a filter cell of a fixed bed of bulk loaded composite particles to yield decontaminated water; heavy metal ions and organics being retained in the composite particles; wherein each composite particle comprises zero-valent iron biochar and sludge biochar.
- Claim 2Depends on #1
The process according to claim 1, wherein the bulk loaded zero-valent iron biochar and sludge biochar composite particles are obtained by mixing crushed iron-rich biomass with sludge, and granulating, followed by programmed heating and pyrolytic charring under nitrogen atmosphere, wherein the iron-rich biomass is rice straw grown in acidic red soil.
- Claim 3Depends on #1
The process according to claim 1, said programmed heating comprising three stages: first heating stage: heating to 300 ° C. at a rate of 5-10 ° C./min and maintaining at this temperature for 30-40 minutes; second heating stage: heating from 300 ° C. to 480 ° C. at a rate of 5-8 ° C./min and maintaining at this temperature for 15-35 minutes; third heating stage: heating from 480 ° C. to 600-850 ° C. at a rate of 5-8 ° C./min and maintaining at this temperature for 12-20 minutes.
- Claim 4Depends on #3
The process according to claim 3, wherein, during the first heating stage, heating at a rate of 7-10 ° C./min and maintaining the temperature for 30-35 min after heating to 300 ° C.; during the second heating stage, heating at a rate of 6-8 ° C./min, and maintaining the temperature for 20-30 min after heating to 480 ° C.; during the third heating stage, heating at a rate of 5-6 ° C./min, and maintaining the temperature for 15-20 min after heating to 600-850 ° C.
- Claim 5Depends on #1
The process according to claim 1, wherein the sludge biochar is dewatered to a water content of 50-70%.
- Claim 6Depends on #1
The process according to claim 1, wherein iron salts and dewatered sludge are mixed and the resulting mixture settles for a period of time.
- Claim 7Depends on #1
The process according to claim 1, wherein the composite particles further comprise mineral earth and the composite particles are granulated before the passing step.
- Claim 8Depends on #1
The process according to claim 1, wherein said bulk loaded zero-valent iron biochar and sludge biochar composite particles have a biofilm suspended thereon.
- Claim 9Depends on #1
The process according to claim 1, wherein the filled bed or the filter cell of the fixed bed is further mixed with porous filter material.
- Claim 10Depends on #4
The process according to claim 4, wherein, during the first heating stage, heating at a rate of 8 ° C./min, and maintaining the temperature for 30 minutes after heating to 300 ° C.; during the second heating stage, heating at a rate of 6 ° C./min, and maintaining the temperature for 20 minutes after heating to 480 ° C.; during the third heating stage, heating at a rate of 5 ° C./min, and maintaining the temperature for 20 minutes after heating to 600-850 ° C.
- Claim 11Depends on #5
The process according to claim 5, wherein the sludge biochar is dewatered to a water content of 55-65%.
- Claim 12Depends on #7
The process according to claim 7, wherein the mineral earth is bentonite or kaolin.
- Claim 13Depends on #9
The process according to claim 9, wherein the porous filter material has a biofilm suspended thereon.
Technical Overview & Description
TECHNICAL FIELD The present invention relates to the field of environmental recovery, in particular to a treatment and recovery technique of polluted water body and soil. BACKGROUND ART As agricultural and industrial production progresses, large amounts of industrial waste, domestic waste, sewage, etc., are constantly being discharged to the environment, causing pollution of water bodies and soil. Especially water basins, the soil of which suffers contamination due to water pollution. In particular, water and soil pollution in water basins due to multiple pollution sources, such as heavy metals, organics, pesticides, and the like is increasingly common and its recovery issues are increasingly prominent. Nanoscale zero-valent iron has been widely used as an efficient recovery material due to its large specific surface area and surface energy, which can induce special surface effects and quantum effects. However, nanoscale zero-valent iron is extremely prone to oxidation in air to form a passivating layer, thus reducing the activity, and itself is prone to agglomeration, greatly reducing its specific surface area and reactivity, resulting in reduced reducing power, which greatly limits the application of nanoscale zero-valent iron. To this end, researchers tend to improve the removal performance of nanoscale zero-valent iron for heavy metals by utilizing methods of biochar modification. Existing ways of modifying nano scale zero-valent iron with biochar are mainly by impregnating biomass to adsorb iron salts and the like, and then preparing the biochar nanoscale zero-valent iron nickel composite by processes, such as pyrolysis. Even it is further modified by nickel through nickel salts and the like. The obtained biochar nanoscale zero-valent iron nickel composite is a surface-supported composite, whose stability etc. is to be improved. SUMMARY OF THE INVENTION The present inventors have conducted research and found that: for iron-rich straw biomass, after being crushe
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (7)
Non-Patent Literature (3)
- Machine translation of CN106268635A (Year: 2025).
- Machine translation of CN106881350A (Year: 2025).
- Machine translation of CN111732463A (Year: 2025).