Method for etching lithium niobate and method for forming lithium niobate pattern using the same
Abstract
The present invention relates to a method for etching lithium niobate, the method including a process of etching lithium niobate using a mask pattern as a physical dry etching method using Ar plasma produced in a chamber through Ar gas, wherein in the process of etching lithium niobate, a process pressure of the chamber is maintained at 1 mTorr to 20 mTorr, and a method for forming a lithium niobate pattern using the same.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.
Claims (14 — 2 Independent, 12 Dependent)
- Claim 1Independent Claim
A method for etching lithium niobate, the method comprising: a process of etching lithium niobate using a mask pattern, as a physical dry etching method using Ar plasma produced in a chamber through Ar gas, wherein in the process of etching lithium niobate, a process pressure of the chamber is maintained at 1 mTorr to 20 mTorr, and a process of forming a mask pattern on the lithium niobate, wherein the forming of the mask pattern comprises: a process of forming an adhesive film on the lithium niobate; a process of spin-coating an HSQ resist on the adhesive film; a process of forming a conductive layer by spin-coating a conductive layer solution on the HSQ resist: a process of patterning the conductive layer and the HSQ resist; and a process of developing the conductive layer and the HSQ resist.
- Claim 2Depends on #1
The method of claim 1, wherein the process of etching lithium niobate is performed using ICP etching equipment, and in this case, an ICP power is 300 W to 1000 W, and a bias power is 50 W to 300 W.
- Claim 3Depends on #1
The method of claim 1, wherein the process of etching lithium niobate is performed using magnetron plasma etching equipment, and in this case, an electromagnetic intensity is 10 Gauss to 70 Gauss, and a bias power is 50 W to 300 W.
- Claim 4Depends on #1
The method of claim 1, wherein the forming of the mask pattern further comprises: a process of treating the surface of the adhesive film with O 2 plasma after the process of forming the adhesive film; and a process of heating the HSQ resist using a hot plate at 80 ° C. to 200 ° C. after the process of spin-coating the HSQ resist.
- Claim 5Depends on #1
The method of claim 1, wherein the adhesive film is formed as a silicon dioxide film (SiO 2) using a plasma-enhanced chemical vapor deposition (PECVD) method.
- Claim 6Depends on #1
The method of claim 1, further comprising a process of stabilizing the chamber by performing a multiple Ar purge process prior to the process of etching lithium niobate.
- Claim 7Depends on #6
The method of claim 6, wherein the multiple Ar purge process comprises: a process of operating a vacuum pump under atmospheric pressure conditions, and then injecting Ar gas until the chamber internal pressure becomes 100 Torr, and then repeatedly performing an Ar purge process of operating the vacuum pump at least three times; and a process of injecting Ar gas up to the process pressure.
- Claim 8Depends on #1
A method for forming a lithium niobate pattern, the method comprising: a process of forming a lithium niobate pattern using the method according to claim 1; and a cleaning process of removing a redeposited layer in which byproducts generated in the process of forming the lithium niobate pattern are redeposited on the lithium niobate pattern.
- Claim 9Depends on #8
The method of claim 8, wherein the cleaning process is performed using a KOH aqueous solution.
- Claim 10Depends on #8
The method of claim 8, further comprising a process of restoring the transparency of the lithium niobate, which is changed by damage caused during the process of etching lithium niobate, by performing a heat treatment process after the process of forming the lithium niobate pattern.
- Claim 11Depends on #10
The method of claim 10, wherein the heat treatment process is performed at 500 ° C. to 900 ° C. in an O 2 flow gas environment.
- Claim 12Independent Claim
A method for etching lithium niobate, the method comprising: a process of etching lithium niobate using a mask pattern, as a physical dry etching method using Ar plasma produced in a chamber through a mixed gas in which Ar gas and O 2 gas are mixed at a volume ratio of 1:0.5 to 1:2, wherein in the process of etching lithium niobate, a process pressure of the chamber is maintained at 1 mTorr to less than 20 mTorr, and a process of forming a mask pattern on the lithium niobate, wherein the forming of the mask pattern comprises: a process of forming an adhesive film on the lithium niobate; a process of spin-coating an HSQ resist on the adhesive film; a process of forming a conductive layer by spin-coating a conductive layer solution on the HSQ resist; a process of patterning the conductive layer and the HSQ resist; and a process of developing the conductive layer and the HSQ resist.
- Claim 13Depends on #12
The method of claim 12, wherein the forming of the mask pattern further comprises: a process of treating the surface of the adhesive film with O 2 plasma after the process of forming the adhesive film; and a process of heating the HSQ resist using a hot plate at 80 ° C. to 200 ° C. after the process of spin-coating the HSQ resist.
- Claim 14Depends on #12
The method of claim 12, wherein the adhesive film is formed as a silicon dioxide film (SiO 2) using a plasma-enhanced chemical vapor deposition (PECVD) method.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit under 35 USC 119(a) of Korean Patent Application Nos. 10-2022-0036633 filed on Mar. 24, 2022, and 10-2022-0042690 filed on Apr. 6, 2022, in the Korean Intellectual Property Office, the entire disclosures of which are incorporated herein by reference for all purposes. BACKGROUND 1. Field of the Invention The present invention relates to a method for etching lithium niobate (LiNbO 3 ) and a method for forming a lithium niobate pattern using the same, and more particularly, to a method for etching lithium niobate at a low bias voltage through physical dry etching of large-area lithium niobate and a method for forming a high-quality lithium niobate pattern using the same. 2. Discussion of Related Art Lithium niobate (LiNbO 3 ) materials exhibit physically or chemically stable characteristics in a real environment and have low optical loss characteristics in a wide band. Further, lithium niobate materials have the potential to be applied to various functional devices due to an electro-optical effect, piezoelectric effect, acousto-optical effect, and the like. Due to these advantages, interest in lithium niobate is increasing, and recently, with the development of a technique of preparing a lithium niobate thin film, there is an opportunity to manufacture various optical functional devices with high integration through a patterning and etching technique. Various chemical or physical etching techniques have been tried as etching techniques for etching lithium niobate. In particular, since a radioactive ion etching (RIE) etching technique, which can be applied to a large area, enables easy process condition control, can perform anisotropic etching, and is used to manufacture highly integrated devices, has high productivity, precision, and reproducibility, efforts have been made to apply the RIE etching technique to a technique of etching a lithium niobate thin film. The lithium niobate etching metho
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (11)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (10)
- Korean Office Action issued on Jul. 2, 2024, in counterpart Korean Patent Application No. 10-2022-0042690 (1 pages in English, 7 pages in Korean).
- Arizmendi et al.
- “
- Defects induced in pure and doped LiNbO3 by irradiation and thermal reduction
- ”
- vol. 17 No. 3, 1984 (pp. 515-529).
- Ren et al.
- “
- Etching characteristics of LiNbO3 in reactive ion etching and inductively coupled plasma
- ”