Chemical mechanical polishing slurry composition for polishing boron silicon compound, chemical mechanical polishing method and method of fabricating semiconductor device using the same
Abstract
A CMP slurry composition for polishing a boron silicon (B — Si) compound may include a catalyst, an abrasive including a plurality of particles and being configured to polish the boron silicon (B — Si) compound, and a pH adjuster. The CMP slurry composition may further include an oxidizer. The catalyst may have a binary catalyst configuration comprising a first catalyst material and a second catalyst material. The first catalyst material may include Fe, and the second catalyst material may include Cu. The oxidizer may include hydrogen peroxide (H 2 O 2 ). A CMP (chemical mechanical polishing) method for a boron silicon (B — Si) compound may include providing a substrate structure including a thin film formed of the boron silicon (B — Si) compound and performing a CMP process on the thin film. The CMP process is performed by using the CMP slurry composition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A CMP (chemical mechanical polishing) slurry composition for polishing a boron silicon (B — Si) compound, the CMP slurry composition comprising: a catalyst having a binary catalyst configuration that comprises a first catalyst material and a second catalyst material; an abrasive including a plurality of particles and being configured to polish the boron silicon (B — Si) compound; and a pH adjuster, wherein the first catalyst material includes Fe, and the second catalyst material includes Cu.
- Claim 2Depends on #1
The CMP slurry composition of claim 1, further comprising an oxidizer, and wherein the oxidizer includes any one selected from the group consisting of hydrogen peroxide (H 2 O 2), periodic acid, periodate salt, perbromic acid, perbromate salt, perchloric acid, perborate salt, and permanganate.
- Claim 3Depends on #2
The CMP slurry composition of claim 2, wherein a content of the oxidizer is about 1.5 wt % to about 2 wt %.
- Claim 4Depends on #1
The CMP slurry composition of claim 1, wherein the first catalyst material is Fe(NO 3) 3 and the second catalyst material is Cu(NO 3) 2.
- Claim 5Depends on #1
The CMP slurry composition of claim 1, wherein a concentration of the first catalyst material is about 0.05 to about 5.0 mM, and a concentration of the second catalyst material is about 0.05 to about 5.0 mM.
- Claim 6Depends on #1
The CMP slurry composition of claim 1, wherein the abrasive includes metal oxide particles, and surfaces of the metal oxide particles are modified with amine functionalized silane.
- Claim 7Depends on #6
The CMP slurry composition of claim 6, wherein the surfaces of the metal oxide particles are modified with any one of APTES, DAPTMS, and TAPTMS.
- Claim 8Depends on #6
The CMP slurry composition of claim 6, wherein the metal oxide particles are silica particles.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATION The present application claims, under 35 U.S.C. § 119(a), the benefit of Korean application No. 10-2021-0139140, filed on Oct. 19, 2021, which is herein incorporated by reference in its entirety. BACKGROUND 1. Field Embodiments of the present disclosure relates to a CMP slurry composition and a device manufacturing method using the same, and more particularly, to a CMP slurry composition for polishing boron silicon compound, a CMP method using the same, and a semiconductor device manufacturing method using the same. 2. Description of the Related Art In general, patterns constituting a semiconductor device may be formed by sequentially forming an etching target layer and a hard mask pattern on a predetermined underlying layer, and then etching the etching target layer exposed between patterns of the hard mask pattern. As such, when an etching process is performed by using the hard mask pattern serving as the etching mask, it may be desirable to keep the hard mask pattern substantially the same while the etching target layer exposed between the hard mask pattern is etched. However, as a degree of integration of the semiconductor device increases and a line width/scale of the pattern continuously decreases, an aspect ratio of the region to be etched in the etching target layer increases, thereby causing the hard mask pattern to be significantly removed during the etching process. This may be based upon the following reason. That is, as a ratio of the thickness to be etched to the width to be etched (i.e., the aspect ratio) increases, the hard mask pattern formed relatively thin compared to the thickness of the etching target layer may be lost during the etching process. In order to solve this problem, it may be considered to make the thickness of the hard mask pattern thicker, but in this case, the aspect ratio of the hard mask pattern also increases. The hard mask pattern having the increased aspect ratio has a problem that it is
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (12)
| Patent | Title | Year | Citations |
|---|