hottub.patents
US 12,424,446 B2#3437974 Most CitedActiveUnited States (USPTO)Utility

Silicon (Si) dry etch for die-to-wafer thinning

0Forward Citations (#3437974 Global)
0.0/yrCitation Velocity (#3437974 Global)
0.00Citation PageRank (#3437974 Global)
5Prior Art Cited
18Claims (2 Indep. · 16 Dep.)
4Drawings / Sheets

Abstract

A method of thinning a die engaged with a substrate is disclosed, utilizing dry etching of a top surface of the die with a plasma comprising fluorine to selectively remove the top surface of the die relative to a top surface of the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.

Claims (18 — 2 Independent, 16 Dependent)

  1. Claim 1Independent Claim

    A method of thinning a die engaged with a substrate, comprising: dry etching a top surface of the die with a plasma comprising fluorine to selectively remove the top surface of the die relative to a top surface of the substrate, wherein the top surface of the die is removed at a rate of greater than or equal to about 1.5 μ m/min.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the plasma comprising fluorine is formed from SF 6, CF 4, C 4 F 8 or a combination thereof, and wherein the top surface of the die is removed at a rate of greater than or equal to about 3 μ m/min.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the die engaged with the substrate is a chip bonded to a wafer, the chip having a thickness of greater than or equal to about 50 μ m prior to the dry etching of the top surface of the die, and the die having a thickness of less than or equal to about 30 μ m after the dry etching of the top surface of the die.

  4. Claim 4Depends on #1

    The method of claim 1, wherein over 50 μ m of a thickness of the die is removed.

  5. Claim 5Depends on #1

    The method of claim 1, wherein the substrate is maintained at a temperature of less than or equal to about 80 ° C. during the dry etching of the top surface.

  6. Claim 6Depends on #1

    The method of claim 1, wherein the substrate further comprises a protective layer disposed over at least a portion of the substrate.

  7. Claim 7Depends on #6

    The method of claim 6, wherein the protective layer comprises SiN, SiCN, oxygen-doped silicon nitride, a metal oxide layer, or a combination thereof.

  8. Claim 8Depends on #6

    The method of claim 6, wherein the protective layer comprises an organic photo resist.

  9. Claim 9Depends on #1

    The method of claim 1, wherein the die is bonded to a dielectric layer disposed on top of the substrate, comprising a metal oxide, SiCN, SiN, or a combination thereof, and wherein the dielectric layer is a protective layer which prevents the plasma comprising fluorine from dry etching a portion of the substrate located below the dielectric layer.

  10. Claim 10Depends on #1

    The method of claim 1, wherein a ratio of a rate at which the top surface of the die is removed relative to a rate at which the top surface of the substrate is removed is greater than or equal to about 100:1.

  11. Claim 11Depends on #1

    The method of claim 1, wherein the die, the substrate, or both comprise a metal pad, and wherein no portion of the metal pad is contacted by the plasma comprising fluorine.

  12. Claim 12Independent Claim

    A method of thinning a chip bonded to a wafer substrate, comprising: dry etching, in a processing chamber, a top surface of the chip with a plasma comprising fluorine formed from SF 6, CF 4, C 4 F 8 or a combination thereof to selectively remove the top surface of the chip relative to a top surface of the wafer substrate; wherein the top surface of the chip is removed at a rate of greater than or equal to about 1.5 μ m/min; wherein the chip comprises silicon; wherein at least a portion of a top surface of the wafer substrate and/or a die side wall comprises a protective layer; wherein at least one metal pad is embedded completely within the chip bonded to the wafer substrate, at least one metal pad is disposed beneath the protective layer, or both; and wherein no metal pad is contacted by the plasma comprising fluorine.

  13. Claim 13Depends on #12

    The method of claim 12, wherein the protective layer comprises SiN, SiCN, oxygen-doped silicon nitride, a metal oxide, or a combination thereof.

  14. Claim 14Depends on #12

    The method of claim 12, wherein the protective layer comprises a photo resist.

  15. Claim 15Depends on #12

    The method of claim 12, wherein the top surface of the chip is removed at a rate of greater than or equal to about 3 μ m/min.

  16. Claim 16Depends on #12

    The method of claim 12, wherein the chip has a thickness of greater than or equal to about 50 μ m prior to the dry etching of the top surface of the chip with the plasma comprising fluorine, and the chip has a thickness of less than or equal to about 30 μ m after the dry etching of the top surface of the chip.

  17. Claim 17Depends on #12

    The method of claim 12, wherein over 50 μ m of a thickness of the chip is removed.

  18. Claim 18Depends on #12

    The method of claim 12, wherein the wafer substrate is maintained at a temperature of less than or equal to about 80 ° C.

Technical Overview & Description

FIELD Embodiments of the present disclosure generally relate to the field of semiconductor manufacturing processes, more particularly, to processes for thinning a die engaged with a substrate. BACKGROUND Current chip-to-wafer bonding is typically limited to the chip or die having a height or thickness of greater than about 30 micrometers ( μ m) due to limitation of thin die handling processes or equipment, which include limitations in die ejection failure causing die breakage, inherent high die stress causing die warpage that results in failing to bond the chip to the wafer, and the like. However, the inventors have observed that relatively thin, e.g., less than 30 μ m, die bonding may be desired for providing improved electrical and thermal properties and reducing form factor. Other improvements include stacking relatively thin dies, such as in dual-stacks of SRAM memory to achieve 3D-integration. However, technical challenges remain to achieve thinned die chip-to-wafer structures. The inventors have observed that utilizing a relatively thin die of less than 30 μ m in chip-to-wafer bonding may be obtained when utilizing a thicker die bonded to the wafer or substrate, which may then be processed to achieve a thin top die. However, the inventors have observed that typical thinning processes such as grinding or chemical mechanical polishing (CMP) undesirably cause issues that lead to yield loss. For example, grinding exposes the die to high temperatures, pressures, and high mechanical shear forces which can cause chipping, cracking, and/or delamination of the die from the substrate. CMP has a relatively low removal rate of less than about 1 μ m per min and high cost. CMP is also limited due to the damage which may occur to the polishing pad that results from the topological aspects of the die. Accordingly, the inventors have provided improved methods for thinning of a die bonded to a substrate. SUMMARY Methods for thinning a die engaged with a substrate are provided h

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • International Search Report for PCT/US2023/085377, detsd Apr. 23, 2024.