Polishing head assembly having recess and cap
Abstract
A polishing head assembly for polishing of semiconductor wafers includes a polishing head and a cap. The polishing head has a recess along a bottom portion. The recess has a recessed surface. The cap is positioned within the recess. The cap includes an annular wall secured to the polishing head and a floor joined to the annular wall at a joint. The floor extends across the annular wall, and the floor has an upper surface and a lower surface. The upper surface is spaced from the recessed surface to form a chamber therebetween. A deformation resistance of a portion of the floor proximate the joint is weakened to allow the portion of the floor proximate the joint to deflect relative to the polishing head by a change of pressure in the chamber.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A polishing head assembly for polishing of semiconductor wafers, the polishing head assembly comprising: a polishing head having a recess along a bottom portion, the recess having a recessed surface; and a cap positioned within the recess, the cap comprising: an annular wall secured to the polishing head, the annular wall comprising a first portion having a first thickness and a second portion extending from the first portion and having a second thickness; and a floor joined to the annular wall at a joint, the floor extending across the annular wall, the floor having an upper surface and a lower surface, the upper surface spaced from the recessed surface to form a chamber therebetween, wherein the first portion of the annular wall is joined to the floor and the first thickness is less than the second thickness to weaken a deformation resistance of a portion of the floor proximate the joint compared to other portions of the floor to allow the portion of the floor proximate the joint to
- Claim 2Depends on #1
The polishing head assembly of claim 1, wherein the first thickness is from about 3 mm to about 5 mm.
- Claim 3Depends on #2
The polishing head assembly of claim 2, wherein the first thickness is about 3 mm.
- Claim 4Depends on #1
The polishing head assembly of claim 1, wherein the floor has a continuous thickness of from about 5 mm to about 6 mm.
- Claim 5Depends on #1
The polishing head assembly of claim 1, wherein: the polishing head has a top portion and holes extending from the top portion through the recessed surface; the annular wall further comprises a shoulder extending from the second portion, the shoulder having apertures corresponding to the holes; and the holes and the corresponding apertures receive fasteners to secure the shoulder of the annular wall to the recessed surface of the polishing head.
- Claim 6Depends on #1
The polishing head assembly of claim 1, wherein the annular wall tapers inwardly toward the joint from the second thickness to the first thickness such that the first thickness of the annular wall is proximate the joint to weaken the deformation resistance of the portion of the floor proximate the joint.
- Claim 7Depends on #6
The polishing head assembly of claim 6, wherein the first thickness of the annular wall proximate the joint is from about 3 mm to about 5 mm.
- Claim 8Depends on #6
The polishing head assembly of claim 6, wherein the first thickness of the annular wall proximate the joint is about 3 mm.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to U.S. Provisional Patent Application No. 63/265,951, filed Dec. 23, 2021, the disclosure of which is hereby incorporated by reference in its entirety. FIELD This disclosure relates generally to polishing of semiconductor wafers and more particularly to a polishing head assembly having a recess and cap. BACKGROUND Semiconductor wafers are commonly used in the production of integrated circuit (IC) chips on which circuitry are printed. The circuitry is first printed in miniaturized form onto surfaces of the wafers. The wafers are then broken into circuit chips. This miniaturized circuitry requires that front and back surfaces of each wafer be extremely flat and parallel to ensure that the circuitry can be properly printed over the entire surface of the wafer. To accomplish this, grinding and polishing processes are commonly used to improve flatness and parallelism of the front and back surfaces of the wafer after the wafer is cut from an ingot. A particularly good finish is required when polishing the wafer in preparation for printing the miniaturized circuits on the wafer by an electron beam-lithographic or photolithographic process (hereinafter “ lithography ” ). The wafer surface on which the miniaturized circuits are to be printed must be flat. Polishing machines typically include a circular or annular polishing pad mounted on a turntable or platen for driven rotation about a vertical axis passing through the center of the pad and a mechanism for holding the wafer and forcing it into the polishing pad. The wafer is typically mounted to the polishing head using for example, liquid surface tension or vacuum/suction. A polishing slurry, typically including chemical polishing agents and abrasive particles, is applied to the pad for greater polishing interaction between the polishing pad and the surface of the wafer. This type of polishing operation is typically referred to as chemical-mechanical
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (33)
| Patent | Title | Year | Citations |
|---|---|---|---|
| GB 1,092,504 A | Process for coagulating and coalescing to form shaped articles | — | 0 |
Non-Patent Literature (1)
- Extended European Search Report issued for Application No. 22216026.9, on May 11, 2023 (9 pages).