Composition of zinc wire
Abstract
Disclosed is a method for manufacturing a zinc wire. The method comprises melting a zinc ingot at a first temperature of 420° C. to 650° C. to form a molten zinc. Further, the method comprises calibrating a set of impurities in the molten zinc. Furthermore, the method comprises maintaining the molten zinc at a second temperature between 400° C. to 600° C. Subsequently, the method comprises fluxing the molten zinc to remove a non-metallic impurity. Further, the method comprises transferring the molten zinc into a casting mould to form a cast bar. Furthermore, the method comprises continuously feeding the cast bar from the casting mould to a rolling mill to form a rolled zinc wire rod. Finally, the method comprises drawing a zinc wire rod from the rolled zinc wire rod.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A composition of a zinc wire, the composition comprising: zinc as first component with a 99.975% (w/w) concentration; and X as second component, wherein X is one or more of Lead (Pb), Cadmium (Cd), Tin (Sn), Iron (Fe), Aluminum (Al), Copper (Cu), Strontium (Sr), Germanium (Ge), Titanium (Ti), Tantalum (Ta), Arsenic (As), Manganese (Mn), Magnesium (Mg), and Silver (Ag), and wherein a total maximum concentration of the second component is 0.025% (w/w), wherein lead is in 0.0002% (w/w) to 0.0010% (w/w) concentration, copper is in 0.0001% (w/w) to 0.0005% (w/w) concentration, iron is in 0.0005% (w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.