US 12,409,643 B2#3451354 Most CitedActiveUnited States (USPTO)Utility

Articles having inorganic substrates and polymer film layers

0Forward Citations (#3451354 Global)
0.0/yrCitation Velocity (#3451354 Global)
0.00Citation PageRank (#3451354 Global)
18Prior Art Cited
25Claims (2 Indep. · 23 Dep.)
2Drawings / Sheets

Abstract

In a first aspect, an article includes an inorganic substrate and a polymer film layer. The inorganic substrate includes a material including a ceramic, a glass, a glass-ceramic or a mixture thereof. The material includes a metal cation selected from the group consisting of silicon, aluminum, titanium, zirconium, tantalum, niobium and mixtures thereof and oxygen. The polymer film layer includes a polymer including an imide group. From an interface where the inorganic substrate contacts the polymer film layer, a line-profile of a CNO − signal from negative secondary ion mass spectroscopy decreases as it moves away from the interface and into the bulk of the polymer film layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 0.

Claims (25 — 2 Independent, 23 Dependent)

  1. Claim 1Independent Claim

    An article comprising: an inorganic substrate comprising a material comprising a ceramic, a glass, a glass-ceramic or a mixture thereof, wherein the material comprises: a metal cation selected from the group consisting of silicon, aluminum, titanium, zirconium, tantalum, niobium and mixtures thereof; and oxygen; a polymer film layer comprising a polymer comprising an imide group, wherein, from an interface where the inorganic substrate contacts the polymer film layer, a line-profile of a CNO − signal from negative secondary ion mass spectroscopy decreases as it moves away from the interface and into the bulk of the polymer film layer; and a hard coat layer adhered to the polymer film layer on a side opposite the inorganic substrate, wherein the hard coat layer is formed from a curable resin coating composition.

  2. Claim 2Depends on #1

    The article of claim 1, wherein the polymer comprising an imide group is selected from the group consisting of polyimides, poly(amide-imides), poly(ether-imides), poly(ester-imides), copolymers comprising amide, ester or ether groups, and mixtures thereof.

  3. Claim 3Depends on #2

    The article of claim 2, wherein the polyimide is derived from a dianhydride, a fluorinated aromatic diamine and an aliphatic diamine.

  4. Claim 4Depends on #3

    The article of claim 3, wherein the dianhydride comprises an alicyclic dianhydride.

  5. Claim 5Depends on #1

    The article of claim 1, wherein the inorganic substrate comprises glass.

  6. Claim 6Depends on #1

    The article of claim 1, wherein the metal cation comprises silicon.

  7. Claim 7Depends on #1

    The article of claim 1, wherein a Mode I Interlaminar Fracture Toughness (G Ic) between the inorganic substrate and the polymer film layer is 9 J/m 2 or more.

  8. Claim 8Depends on #1

    The article of claim 1, wherein the polymer film layer has a T g of 300 ° C. or less.

  9. Claim 9Depends on #1

    The article of claim 1, wherein the article has a b* of 1.25 or less and a yellowness index of 2.25 or less when measured using the procedure described by ASTM E313 at a thickness of 25 μ m.

  10. Claim 10Depends on #1

    The article of claim 1, wherein the article has a haze of 15% or less and an L* of 93 or more when measured at a thickness of 25 μ m.

  11. Claim 11Depends on #1

    An impact-resistant article comprising the article of claim 1.

  12. Claim 12Depends on #1

    A penetration-resistant article comprising the article of claim 1.

  13. Claim 13Depends on #1

    A sound-reducing article comprising the article of claim 1.

  14. Claim 14Independent Claim

    An article comprising: an inorganic substrate comprising a material comprising a ceramic, a glass, a glass-ceramic or a mixture thereof, wherein the material comprises: a metal cation selected from the group consisting of silicon, aluminum, titanium, zirconium, tantalum, niobium and mixtures thereof; and oxygen; a polymer film layer comprising a polymer comprising an imide group, wherein, a Mode I Interlaminar Fracture Toughness (G Ic) between the polymer film layer and the inorganic substrate layer is 9 J/m 2 or more; and a hard coat layer adhered to the polymer film layer on a side opposite the inorganic substrate, wherein the hard coat layer is formed from a curable resin coating composition.

  15. Claim 15Depends on #14

    The article of claim 14, wherein the polymer comprising an imide group is selected from the group consisting of polyimides, poly(amide-imides), poly(ether-imides), poly(ester-imides), copolymers comprising amide, ester or ether groups, and mixtures thereof.

  16. Claim 16Depends on #15

    The article of claim 15, wherein the polyimide is derived from a dianhydride, a fluorinated aromatic diamine and an aliphatic diamine.

  17. Claim 17Depends on #16

    The article of claim 16, wherein the dianhydride comprises an alicyclic dianhydride.

  18. Claim 18Depends on #14

    The article of claim 14, wherein the inorganic substrate comprises glass.

  19. Claim 19Depends on #14

    The article of claim 14, wherein the metal cation comprises silicon.

  20. Claim 20Depends on #14

    The article of claim 14, wherein the article has a b* of 1.25 or less and a yellowness index of 2.25 or less when measured using the procedure described by ASTM E313 at a thickness of 25 μ m.

  21. Claim 21Depends on #14

    The article of claim 14, wherein the article has a haze of 15% or less and an L* of 93 or more when measured at a thickness of 25 μ m.

  22. Claim 22Depends on #14

    An impact-resistant article comprising the article of claim 14.

  23. Claim 23Depends on #14

    A penetration-resistant article comprising the article of claim 14.

  24. Claim 24Depends on #14

    A sound-reducing article comprising the article of claim 14.

  25. Claim 25Depends on #14

    The article of claim 14, wherein the polymer film layer has a T g of 300 ° C. or less.

Technical Overview & Description

FIELD OF DISCLOSURE The field of this disclosure is articles having inorganic substrates and polymer film layers. BACKGROUND OF THE DISCLOSURE Inorganic (e.g., ceramic and glass) laminated products have long been used for a wide variety of applications, such as armor for buildings, vehicles and personnel, as well as safety glass for transparent applications. Beyond the well-known, every day automotive safety glass used in windshields, laminated glass is used as windows for trains, airplanes, ships, and nearly every other mode of transportation. Safety glass is characterized by high impact and penetration resistance and does not scatter glass shards and debris when shattered. Safety glass typically consists of a sandwich of two glass sheets or panels bonded together with an interlayer of a polymeric film or sheet, which is placed between the two glass sheets. One or both glass sheets may be replaced with optically clear rigid polymeric sheets, such as sheets of polycarbonate materials. Safety glass has further evolved to include multiple layers of glass and polymeric sheets bonded together with interlayers of polymeric films or sheets. The interlayer is typically a relatively thick polymer sheet, which exhibits toughness and bondability to provide adhesion to the glass in the event of a crack or crash. In general, it is desirable that these polymeric interlayers possess a combination of characteristics including very high optical clarity, low haze, high impact resistance, high penetration resistance, excellent ultraviolet light resistance, good long-term thermal stability, excellent adhesion to glass and other rigid polymeric sheets, low ultraviolet light transmittance, low moisture absorption, high moisture resistance, and excellent long term weatherability, among other requirements. A recent trend has been the use of glass-laminated products in the construction of homes and office structures. The use of architectural glass has expanded rapidly over the years as des

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (18)

Non-Patent Literature (10)

  • A.V. Patsis et al.,
  • “
  • Amino Organo Alkoxysilanes in Organic Solvents for Promoting Adhesion of Polyimide Films to Silicon Substrates
  • ”
  • , J Adhesion, 25, 145-157, 1988.
  • Y. Liu et al.,
  • “
  • Chemical cross-linking modification of polyimide membranes for gas separation
  • ”
  • , J Membr Sci 189, pp. 231-239, 2001.