Resource utilization-oriented treatment method for spent electroless nickel plating bath

0Forward Citations (#3456311 Global)
0.0/yrCitation Velocity (#3456311 Global)
0.00Citation PageRank (#3456311 Global)
6Prior Art Cited
8Claims (1 Indep. · 7 Dep.)
0Drawings / Sheets

Abstract

The present disclosure relates to the field of resource utilization-oriented treatment technologies for wastewater, and more particularly, to a resource utilization-oriented treatment method for a spent electroless nickel plating bath. The method includes oxidation de-complexation, synchronous precipitation of nickel and phosphorus, secondary precipitation of nickel, and resource utilization of sodium salt. In the present disclosure, in a reaction process, no sludge is generated to avoid secondary pollution to the environment. Further, the present disclosure has the advantages of short flow and less chemical use, greatly reducing treatment costs. In this way, this method is a low-cost and clean resource utilization-oriented treatment method capable of achieving resource utilization-oriented recovery of nickel, phosphorus, sodium, sulfate radical, or chlorine in the spent electroless nickel plating bath.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.

Claims (8 — 1 Independent, 7 Dependent)

  1. Claim 1Independent Claim

    A resource utilization-oriented treatment method for a spent electroless nickel plating bath, comprising the following steps: at step S1, oxidation de-complexation: adjusting the pH of the spent electroless nickel plating bath and adding hydrogen peroxide and then stirring to uniformity, and then moving to an oxidation tower for aeration for performing oxidation reaction of 2 to 5 h to obtain an acid reaction solution, wherein the oxidation tower is internally filled with a non-homogeneous Fenton catalyst; at step S2, synchronous precipitation of nickel and phosphorus: adjusting the pH of the acid reaction solution and adding a precipitant, performing heating, aging, and filtering to obtain a first filtrate and a nickel phosphate product; at step S3, secondary precipitation of nickel: adding a sodium hydroxide solution to the first filtrate to adjust pH to be greater than 10, and performing heating, aging, and filtering to obtain a second filtrate and a nickel hydroxide product; at ste

  2. Claim 2Depends on #1

    The resource utilization-oriented treatment method of claim 1, wherein, in step S1, the pH of the spent electroless nickel plating bath is adjusted to 5 to 6, and a substance for adjusting the pH of the spent electroless nickel plating bath is an acid solution or a sodium hydroxide solution; when cathode ions in the spent electroless nickel plating bath are H 2 PO 2 −, HPO 3 2 −, PO 4 3 −, SO 4 2 −, the acid solution is sulfuric acid; when the cathode ions in the spent electroless nickel plating bath are H 2 PO 2 −, HPO 3 2 −, PO 4 3 −, Cl −, the acid solution is hydrochloric acid.

  3. Claim 3Depends on #1

    The resource utilization-oriented treatment method of claim 1, wherein, in step S1, the non-homogeneous Fenton catalyst includes a carrier and a catalytic component, wherein the carrier is a porous composite material and the catalytic component is a precious metal, a rare earth metal oxide, and a transition metal oxide.

  4. Claim 4Depends on #1

    The resource utilization-oriented treatment method of claim 1, wherein, in step S2, the pH of the acid reaction solution is adjusted to 0.7 to 8, a mass concentration of the precipitant is 15% to 30%, and the precipitant is used in such an amount that a total phosphorus concentration in the first filtrate is lower than 0.5 mg/L.

  5. Claim 5Depends on #1

    The resource utilization-oriented treatment method of claim 1, wherein, when cathode ions in the spent electroless nickel plating bath are H 2 PO 2 −, HPO 3 2 −, PO 4 3 − and SO 4 2 −, the precipitant is a nickel sulfate solution; when the cathode ions in the spent electroless nickel plating bath are H 2 PO 2 −, HPO 3 2 −, PO 4 3 − and Cl −, the precipitant is a nickel chloride solution.

  6. Claim 6Depends on #1

    The resource utilization-oriented treatment method of claim 1, wherein, in step S2, the heating temperature is 70 ° C. and the aging time is 0.5 hour to 1 hour.

  7. Claim 7Depends on #1

    The resource utilization-oriented treatment method of claim 1, wherein, in step S3, the heating temperature is 70 ° C. and the aging time is 1 hour to 2 hours.

  8. Claim 8Depends on #1

    The resource utilization-oriented treatment method of claim 1, wherein, in step S4, when cathode ions in the spent electroless nickel plating bath are H 2 PO 2 −, HPO 3 2 −, PO 4 3 −, SO 4 2 −, the acidity adjusting solution is sulfuric acid, and the conductivity is adjusted to 70 to 110 mS/cm; when the cathode ions in the spent electroless nickel plating bath are H 2 PO 2 −, HPO 3 2 −, PO 4 3 −, Cl −, the acidity adjusting solution is hydrochloric acid, and the conductivity is adjusted to 120 to 200 mS/cm.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATION This Application is a national stage application of PCT/CN2020/141208. This application claims priority from PCT Application No. PCT/CN2020/141208, filed Dec. 30, 2020, the content of which is incorporated herein in the entirety by reference. TECHNICAL FIELD The present disclosure relates to the field of resource utilization-oriented treatment technologies, and more particularly to a resource utilization-oriented treatment method for a spent electroless nickel plating bath. BACKGROUND Electroless nickel plating has become a major surface treatment technology due to the advantages of its plating layer in the aspects such as uniformity, corrosion resistance, and wear resistance and is widely applied in the fields such as electronic products, aerospace, and machine manufacturing. During an electroless nickel plating process, as a redox reaction proceeds continuously, the accumulation of by-products such as phosphite will lead to aging of the plating bath, forming a large amount of spent electroless nickel plating bath. The main ingredients in the spent electroless nickel plating bath are Na + , H 2 PO 2 − , HPO 3 2 − , PO 4 3 − , SO 4 2 − (or Cl − ), free Ni 2+ , complex nickel, and organic substance. At present, in the industry, much research is focused on the recovery of nickel resources and removal of total phosphorus, and COD pollution factors and few comprehensive disposal solutions are proposed. The nickel resource recovery method includes a catalytic reduction method and an electrolysis method. In the catalytic reduction method, a reductant and an aid, for example, sodium borohydride, sodium hypophosphite, or the like are added. However, this process increases the concentration of the spent bath and complicates the property of the spent bath, which increases processing difficulty and, subsequently, costs. The electrolysis method can directly recover the elementary substance nickel, but the spent bath contains less nickel an

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (6)

PatentTitleYearCitations

Non-Patent Literature (2)

  • International Search Report of PCT/CN2020/141208.
  • Written Opinion of PCT/CN2020/141208.