hottub.patents
US 12,401,044 B2#3459162 Most CitedActiveUnited States (USPTO)Utility

Current collectors comprising metallised films

0Forward Citations (#3459162 Global)
0.0/yrCitation Velocity (#3459162 Global)
0.00Citation PageRank (#3459162 Global)
16Prior Art Cited
29Claims (2 Indep. · 27 Dep.)
2Drawings / Sheets

Abstract

A current collector comprising a biaxially oriented polymeric substrate layer and a first metal layer on a side of the polymeric substrate layer, wherein the polymeric substrate layer exhibits positive thermal expansion in air at 200 ° C. in each of the transverse direction (TD) and machine direction (MD). The polymeric substrate layer has a thickness of no more than 12 pm and the first metal layer has a thickness of no more than 1000 nm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 0.

Claims (29 — 2 Independent, 27 Dependent)

  1. Claim 1Independent Claim

    A current collector comprising a biaxially oriented polyester substrate layer, a first metal layer on a side of the polyester substrate layer, and a second metal layer, wherein the first metal layer and the second metal layer are on opposing sides of the polyester substrate layer, wherein the polyester substrate layer exhibits positive thermal expansion in air at 200 ° C. in each of the transverse direction (TD) and machine direction (MD), wherein the polyester substrate layer has a thickness of no more than 12 μ m, wherein the first metal layer has a thickness of no more than 1000 nm, and wherein the second metal layer independently has a thickness of no more than 1000 nm.

  2. Claim 2Depends on #1

    The current collector according to claim 1, wherein the thickness of the polyester substrate layer is from 1.0 μ m to 12.0 μ m, preferably from 2.0 to 8.0 μ m, preferably from 4.0 to 8.0 μ m, preferably from 4.0 to 6.0 μ m.

  3. Claim 3Depends on #1

    The current collector according to claim 1, wherein the polyester is polyethylene terephthalate or polyethylene naphthalate.

  4. Claim 4Depends on #1

    The current collector according to claim 1, wherein the polyester substrate layer exhibits thermal expansion in air at 200 ° C. of from greater than 0% to no more than 3.0%, preferably from 0.1% to 2.0%, preferably from 0.2% to 1.5%, in each of the transverse direction (TD) and in the machine direction (MD).

  5. Claim 5Depends on #1

    The current collector according to claim 1, wherein the polyester substrate layer exhibits a positive coefficient of linear thermal expansion (CLTE) over the range of 32 ° C. to 200 ° C., preferably of less than 20 × 10 − 5 / ° C., preferably of less than 17 × 10 − 5 / ° C., preferably of less than 10 × 10 − 5 / ° C., preferably of less than 9 × 10 − 5 / ° C., preferably of less than 8.5 × 10 − 5 / ° C. in each of the transverse direction (TD) and machine direction (MD).

  6. Claim 6Depends on #1

    The current collector according to claim 1, wherein the thickness of the first metal layer and the second metal layer is each independently from 50 nm to 1000 nm, preferably from 100 nm to 1000 nm, preferably from 100 nm to 800 nm, preferably from 150 nm to 700 nm.

  7. Claim 7Depends on #1

    The current collector according to claim 1, wherein the first metal layer and the second metal layer each independently exhibits isotropic thermal expansion in air at 200 ° C. of from greater than 0% to no more than 1.0%, wherein isotropic thermal expansion means that the layers expand by the same amount in orthogonal directions, preferably from 0.25% to 0.75%, preferably from 0.3% to 0.5%, preferably wherein the first metal layer and the second metal layer exhibit the same thermal expansion at 200 ° C. as each other.

  8. Claim 8Depends on #1

    The current collector according to claim 1, wherein the first metal layer and the second metal layer each independently exhibit a positive coefficient of linear thermal expansion (CLTE) in air at 100 ° C. of from 10 × 10 − 6 / ° C. to 30 × 10 − 6 / ° C., preferably from 12 × 10 − 6 / ° C. to 18 × 10 − 6 / ° C.

  9. Claim 9Depends on #1

    The current collector according to claim 1, wherein the first metal layer and the second metal layer each independently comprise at least one of aluminium, copper, nickel, titanium, silver, nickel-copper alloy, or aluminium-zirconium alloy, and preferably wherein the first and second metal layers are selected from the same material.

  10. Claim 10Depends on #1

    The current collector according to claim 1, wherein the first and second metal layers are both either aluminium or copper.

  11. Claim 11Depends on #1

    The current collector according to claim 1, wherein the adhesion strength between a metal layer and the polyester substrate layer is least 600 g/25 mm, preferably at least about 700 g/25 mm, preferably at least about 800 g/25 mm.

  12. Claim 12Depends on #1

    The current collector according to claim 1 which exhibits a sheet resistance of from 0.01 Ω sq − 1 to 2.0 Ω sq − 1, preferably from 0.02 Ω sq − 1 to 2.0 Ω sq − 1, preferably from 0.02 Ω sq − 1 to 1.5 Ω sq − 1, preferably from 0.05 Ω sq − 1 to 1.0 Ω sq − 1.

  13. Claim 13Depends on #1

    The current collector according to claim 1, wherein the current collector exhibits a breakdown current of no more than about 30 A and/or a breakdown temperature of no more than about 300 ° C.

  14. Claim 14Depends on #1

    The current collector according to claim 1, which further comprises at least one tab which connects the first metal layer and the second metal layer.

  15. Claim 15Depends on #1

    The current collector according to claim 1 wherein the polyester substrate layer comprises channels which extend from the first surface to the second, opposite surface thereof wherein (i) the sides of the channels are at least partially coated with at least one metal, and/or (ii) the channels are at least partially filled with at least one metal.

  16. Claim 16Depends on #1

    A method of manufacturing the current collector of claim 1, wherein the method comprises the steps of: (i) forming the biaxially oriented polyester substrate layer; and (ii) depositing a metal on a first surface of said substrate layer to form the first metal layer; and (iii) depositing on a second surface of said substrate layer a metal to form the second metal layer; such that the layer order is first metal layer/polymeric substrate layer/second metal layer.

  17. Claim 17Depends on #16

    The method according to claim 16, wherein step (i) comprises extruding a layer of molten polyester, subjecting the extrudate to biaxial stretching at a temperature above the glass transition temperature(s) of the polyester, preferably wherein said biaxial stretching is simultaneous biaxial stretching, and preferably stretching is effected so that the dimension of the oriented film is 2 to 5 times its original dimension in each direction of stretching.

  18. Claim 18Depends on #16

    The method according to claim 16, wherein step (i) comprises dimensionally stabilising a biaxially stretched film by annealing under dimensional support at a temperature above the glass transition temperature(s) of the polyester but below the melting temperature (T M) thereof, preferably wherein the annealing temperature is in the range of from about T M − 80 ° C. to about T M − 10 ° C., and preferably in the range of from about 200 to about 245 ° C., preferably in the range of from about 220 to about 240 ° C.

  19. Claim 19Depends on #16

    The method according to claim 16, wherein step (i) comprises subjecting a biaxially stretched film to dimensional relaxation in both the transverse direction and machine direction, and wherein the degree of relaxation is from about 0.5% to about 5.0%.

  20. Claim 20Depends on #19

    The method according to claim 19, wherein step (i) comprises a second relaxation step after the relaxation step wherein the second relaxation step is conducted at a lower temperature than the relaxation step, preferably at least about 5 ° C. lower, and preferably in the range of from about 195 ° C. to about 240 ° C., preferably from about 195 ° C. to about 235 ° C., preferably from about 195 ° C. to about 230 ° C., preferably from about 195 ° C. to about 220 ° C.

  21. Claim 21Depends on #16

    The method according to claim 16, comprising subjecting an exposed surface of the polyester substrate layer to a surface-modifying treatment, wherein said treatment step occurs after step (i) and prior to step (ii), preferably wherein said treatment comprises subjecting the exposed surface of the polyester substrate layer to a plasma treatment, preferably corona discharge.

  22. Claim 22Depends on #16

    The method according to claim 16, wherein step (ii) and/or step (iii) comprises depositing the metal using thermal evaporation deposition, electron beam evaporation deposition or virtual cathode deposition.

  23. Claim 23Independent Claim

    The use of a biaxially oriented polyester film as a substrate in a current collector which further comprises a first metal layer and a second metal layer, wherein said use is for imparting improved adhesion strength and delamination resistance between said substrate and metal layers, and wherein the polyester substrate layer exhibits positive thermal expansion in air at 200 ° C. in each of the transverse direction (TD) and the machine direction (MD), wherein the polyester substrate layer has a thickness of no more than 12 μ m, wherein the first metal layer has a thickness of no more than 1000 nm, and wherein the second metal layer independently has a thickness of no more than 1000 nm.

  24. Claim 24Depends on #1

    A battery comprising an anode material, a cathode material, a separator between the anode material and the cathode material, an anode current collector and a cathode current collector, wherein at least one of the current collectors is a current collector as defined in claim 1.

  25. Claim 25Depends on #24

    The battery according to claim 24, wherein the battery is a lithium-ion battery.

  26. Claim 26Depends on #24

    The battery according to claim 24, wherein the anode material is coated onto the anode current collector and wherein the anode current collector is a current collector comprising a biaxially oriented polyester substrate layer, a first metal layer on a side of the polyester substrate layer, and a second metal layer, wherein the first metal layer and the second metal layer are on opposing sides of the polyester substrate layer, wherein the polyester substrate layer exhibits positive thermal expansion in air at 200 ° C. in each of the transverse direction (TD) and machine direction (MD), wherein the polyester substrate layer has a thickness of no more than 12 μ m, wherein the first metal layer has a thickness of no more than 1000 nm, and wherein the second metal layer independently has a thickness of no more than 1000 nm.

  27. Claim 27Depends on #24

    The battery according to claim 24, wherein the cathode material is coated onto the cathode current collector and wherein the cathode current collector is a current collector comprising a biaxially oriented polyester substrate layer, a first metal layer on a side of the polyester substrate layer, and a second metal layer, wherein the first metal layer and the second metal layer are on opposing sides of the polyester substrate layer, wherein the polyester substrate layer exhibits positive thermal expansion in air at 200 ° C. in each of the transverse direction (TD) and machine direction (MD), wherein the polyester substrate layer has a thickness of no more than 12 μ m, wherein the first metal layer has a thickness of no more than 1000 nm, and wherein the second metal layer independently has a thickness of no more than 1000 nm.

  28. Claim 28Depends on #24

    Use of a current collector comprising a biaxially oriented polyester substrate layer, a first metal layer on a side of the polyester substrate layer, and a second metal layer, wherein the first metal layer and the second metal layer are on opposing sides of the polyester substrate layer, wherein the polyester substrate layer exhibits positive thermal expansion in air at 200 ° C. in each of the transverse direction (TD) and machine direction (MD), wherein the polyester substrate layer has a thickness of no more than 12 μ m, wherein the first metal layer has a thickness of no more than 1000 nm, and wherein the second metal layer independently has a thickness of no more than 1000 nm in the battery as defined in claim 24.

  29. Claim 29Depends on #1

    A method of manufacturing a battery, the method comprising the steps of (i) preparing or obtaining the current collector of claim 1; (ii) assembling the battery, wherein the battery comprises an anode material, a cathode material, a separator between the anode material and the cathode material, an anode current collector and a cathode current collector, wherein at least one of said current collectors is the current collector obtained from step (i).

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application is a national stage filing under 35 U.S.C. § 371 of International Application No. PCT/GB2022/051215, filed May 13, 2022, which claims the benefit of United Kingdom Application No. GB 2106834.1, filed May 13, 2021, each of which is hereby incorporated herein by reference in its entirety. This invention relates to polymeric films for use in a current collector, to current collectors and other articles made therefrom, and to methods for their manufacture. In particular, the present invention is concerned with current collectors for use in batteries, particularly lithium-ion batteries. Lithium-ion batteries are widely used in the field of rechargeable batteries which is set to continually grow over the foreseeable future due, in part, to the increasing demand for consumer electronics and storage of renewable energy. During battery operation (i.e. during charging and discharging), lithium ions are transferred between the anode material and the cathode material. Commercially available lithium-ion batteries typically contain metal foil current collectors, wherein a metal foil is placed in contact with each of the active solid electrodes. Generally, an aluminium-based foil is used as the cathode current collector and is disposed in contact with the cathode, whereas a copper-based foil is used as the anode current collector and is disposed in contact with the anode. In some arrangements, the cathode material may be coated on the cathode current collector and/or the anode material may be coated on the anode current collector. However, there are problems with such existing metal foil current collectors. Firstly, the metal foil current collectors have a high conductivity which can contribute to an excessive current flow throughout the battery, leading to short-circuiting and over-heating thermal run-away, which can result in fires. Secondly, the metal foil current collectors are relatively thick, dense and heavy (typicall

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (16)

PatentTitleYearCitations

Non-Patent Literature (7)

  • https://amesweb.info/Materials/Linear-Thermal-Expansion-Coefficient-Metals.aspx (Year: 2013).
  • GB2106834.1, Nov. 5, 2021, Search Report under Section 17(5).
  • PCT/GB2022/051215, Oct. 28, 2022, International Search Report and Written Opinion.
  • PCT/GB2022/051215, Mar. 20, 2023, International Preliminary Report on Patentability (Chapter 2).
  • Search Report under Section 17(5) for GB Application No. GB2106834.1 dated Nov. 5, 2021.
  • International Search Report and Written Opinion for International Application No. PCT/GB2022/051215 dated Oct. 28, 2022.