Method for enriching niobium and titanium in a mineral containing iron, niobium and titanium and a use of a nickel-containing substance
Abstract
A method for enriching niobium and titanium in a mineral containing iron, niobium, and titanium, includes: reacting raw materials comprising 1 part by weight of a mineral containing iron, niobium, and titanium, 0.1-0.8 part by weight of a nickel-containing substance and 0.2-1 part by weight of carbon at 800-1500 ° C. to obtain a nickel-iron alloy and a niobium-titanium rich slag, where an amount of the mineral containing iron, niobium, and titanium is counted in terms of iron element, and an amount of the nickel-containing substance is counted in terms of nickel element. The nickel-containing substance is one or more selected from the group consisting of oxides of nickel and nickel minerals.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.
Claims (10 — 2 Independent, 8 Dependent)
- Claim 1Independent Claim
A method for enriching niobium and titanium in a mineral containing iron, niobium, and titanium, comprising: reacting raw materials comprising 1 part by weight of the mineral containing iron, niobium, and titanium, 0.1-0.8 part by weight of a nickel-containing substance, and 0.2-1 part by weight of carbon at 800-1500 ° C. to obtain a nickel-iron alloy and a niobium-titanium rich slag, where an amount of the mineral containing iron, niobium, and titanium is counted in terms of iron element, and an amount of the nickel-containing substance is counted in terms of nickel element; wherein the nickel-containing substance is one or more selected from the group consisting of oxides of nickel and nickel minerals.
- Claim 2Depends on #1
The method according to claim 1, wherein the reacting is performed for 20-50 h.
- Claim 3Depends on #1
The method according to claim 1, wherein the raw materials consist of 1 part by weight of the mineral containing iron, niobium, and titanium, 0.2-0.6 part by weight of the nickel-containing substance, and 0.4-0.7 part by weight of the carbon; and wherein the amount of the mineral containing iron, niobium, and titanium is counted in terms of iron element, and the amount of the nickel-containing substance is counted in terms of nickel element.
- Claim 4Depends on #1
The method according to claim 1, wherein the mineral containing iron, niobium, and titanium comprises 5-70 wt % of Fe 2 O 3, 0.8-4 wt % of FeO, 0.1-1.5 wt % of P 2 O 5, 0.5-20 wt % of Nb 2 O 5, and 0.5-20 wt % of TiO 2.
- Claim 5Depends on #1
The method according to claim 1, wherein the carbon is semi-coke.
- Claim 6Depends on #1
The method according to claim 1, wherein the carbon contains 6-15 wt % of ash, 10-22 wt % of volatile matter, and 60-85 wt % of fixed carbon; and the carbon has a particle size of less than or equal to 20 mm.
- Claim 7Depends on #1
The method according to claim 1, wherein the nickel-containing substance comprises nickel oxide.
- Claim 8Depends on #1
The method according to claim 1, wherein the reacting is carried out in a reaction device; the reaction device contains the raw materials; the raw materials in the reaction device are divided into an upper layer raw material, a middle layer raw material, and a lower layer raw material; the upper layer and lower layer raw materials are carbon, and the middle layer raw material comprises a mixture of the mineral containing iron, niobium, and titanium and the nickel-containing substance.
- Claim 9Depends on #1
The method according to claim 1, wherein niobium has a yield of more than 99 wt %, titanium has a yield of more than or equal to 99 wt %, an enrichment ratio of niobium is more than 1.5, and an enrichment ratio of titanium is more than 1.5.
- Claim 10Independent Claim
A method of using a nickel-containing substance to enrich niobium and titanium from a mineral containing iron, niobium, and titanium, comprising: reacting raw materials comprising 1 part by weight of the mineral containing iron, niobium, and titanium, 0.1-0.8 part by weight of the nickel-containing substance, and 0.2-1 part by weight of carbon at 800-1500 ° C. to obtain a nickel-iron alloy and a niobium-titanium rich slag, where an amount of the mineral containing iron, niobium, and titanium is counted in terms of iron element, and an amount of the nickel-containing substance is counted in terms of nickel element; wherein the nickel-containing substance is one or more selected from the group consisting of oxides of nickel and nickel minerals.
Technical Overview & Description
TECHNICAL FIELD OF THE DISCLOSURE The present disclosure relates to a method for enriching niobium and titanium in a mineral containing iron, niobium and titanium and a use of a nickel-containing substance. BACKGROUND OF THE DISCLOSURE Niobium is an important strategic resource in China. Although China has rich niobium resources, ranking the second place in the world, just after Brazil, China has not realized comprehensive utilization of the valuable element, because these niobium resources have low grade and fine dissemination size. At present, all niobium used in China is almost imported. The niobium resources in China are mainly distributed in Baiyenebo of Baotou, Taimei and Limu of Guangxi, Yichun of Jiangxi and Keketuohai of Xinjiang. Among these places, Baiyenebo has the largest niobium resource reserves, accounting for 95% of China's niobium resource reserves. Its prospective reserves reach 6.6 million tons, and its industrial reserves are 1.57 million tons. Generally, a mineral containing niobium and titanium has about 35-60 wt % iron-containing oxide, about 0.5-4 wt % niobium oxide, about 0.5-4 wt % titanium dioxide, and about 0.1-1.5 wt % phosphorus oxide. The mineral containing niobium and titanium has a low niobium grade and high phosphorus content, so it is expensive to be directly smelt into niobium-titanium-iron alloy, while phosphorus and other impurities may easily enter into the alloy, resulting in the alloy with low quality. CN103993162A discloses a method for removing iron and phosphorus from niobium-iron concentrate with a high content of phosphorus, comprising the following steps: adding niobium-iron concentrate and semi-coke in a silicon carbide reaction tank; placing the reaction tank in a high temperature furnace and keeping it at a temperature of 850-1050 ° C. for 40-60 hours, so as to transfer the niobium-iron concentrate into iron-containing concentrate lumps through the solid state reduction; cooling down to 200-300 ° C. in the furnace;
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (10)
Non-Patent Literature (2)
- International Search Report issued in International Application No. PCT /CN2022/090887 dated Aug. 2, 2022 (3 pages).
- Written Opinion issued in International Application No. PCT /CN2022/090887 dated Aug. 2, 2022 (4 pages).