hottub.patents
US 12,397,349 B2#3462493 Most CitedActiveUnited States (USPTO)Utility

Angled scanning of laser arrays in additive manufacturing

0Forward Citations (#3462493 Global)
0.0/yrCitation Velocity (#3462493 Global)
0.00Citation PageRank (#3462493 Global)
28Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

Systems and methods for additive manufacturing are described. In some embodiments, a method of controlling the one or more laser energy sources of an additive manufacturing system may be based at least in part on a scan angle and/or desired energy density. Systems and methods for controlling melt pool spacing are also described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method of controlling an energy density in an additive manufacturing process, the method comprising: determining a first desired energy density to be delivered to one or more portions of a build surface; determining a first desired scan angle of one or more laser energy sources; selectively activating the one or more laser energy sources based, at least in part, on the first desired energy density and the first desired scan angle; and translating, while the one or more laser energy sources are activated, the one or more laser energy sources in a first direction relative to the build surface corresponding to the first desired scan angle to form one or more weld tracks on the build surface.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the one or more laser energy sources comprises an array of laser energy sources.

  3. Claim 3Depends on #2

    The method of claim 2, wherein the array of laser energy sources comprises a rectangular, linear, or hexagonal array of laser energy sources.

  4. Claim 4Depends on #1

    The method of claim 1, wherein determining the first desired scan angle of the one or more laser energy sources includes determining the first desired scan angle of the one or more laser energy sources based, at least in part, on the first desired energy density.

  5. Claim 5Depends on #1

    The method of claim 1, further comprising providing the first desired energy density to the one or more portions of the build surface by controlling a translation speed of the one or more laser energy sources as well as a number and intensity of the activated laser energy sources that translate over the one or more portions of the build surface.

  6. Claim 6Depends on #1

    The method of claim 1, wherein a path of travel relative to the build surface of at least a portion of the activated one or more laser energy sources are at least partially overlapped.

  7. Claim 7Depends on #1

    The method of claim 1, wherein determining the first desired scan angle includes determining the first desired scan angle based, at least in part, on a spacing of the one or more laser energy sources.

  8. Claim 8Depends on #1

    The method of claim 1, wherein the one or more laser energy sources are configured to produce one or more laser beam spots on the build surface, the method further comprising adjusting a spacing of the one or more laser beam spots based, at least in part, on the first desired energy density and the first desired scan angle.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of priority under 35 U.S.C. § 119(e) of U.S. Provisional Application Ser. No. 63/037,142, filed Jun. 10, 2020, the disclosure of which is incorporated herein by reference in its entirety. FIELD Disclosed embodiments are related to systems and methods for additive manufacturing. BACKGROUND Powder bed fusion processes are an example of additive manufacturing processes in which a three-dimensional shape is formed by selectively joining material in a layer-by-layer process. In metal powder bed fusion processes, one or more laser beams are scanned over a thin layer of metal powder. If the various laser parameters, such as laser power, laser spot size, and/or laser scanning speed are in a regime in which the delivered energy is sufficient to melt the particles of metal powder, one or more melt pools may be established on a build surface. The laser beams are scanned along predefined trajectories such that solidified melt pool tracks create shapes corresponding to a two-dimensional slice of a three-dimensional printed part. After completion of a layer, the powder surface is indexed by a defined distance, the next layer of powder is spread onto the build surface, and the laser scanning process is repeated. In many applications, the layer thickness and laser power density may be set to provide partial re-melting of an underlying layer and fusion of consecutive layers. The layer indexing and scanning is repeated multiple times until a desired three-dimensional shape is fabricated. SUMMARY In some embodiments, a method of controlling an energy density in an additive manufacturing process includes determining a first desired energy density to be delivered to one or more portions of a build surface, determining a first desired scan angle of one or more laser energy sources, selectively activating the one or more laser energy sources based at least in part on the first desired energy density and the first

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (28)

Non-Patent Literature (2)

  • International Search Report and Written Opinion for International Application No. PCT/US2021/035464, mailed Nov. 26, 2021.
  • Extended European Search Report dated Jun. 11, 2024 in connection with European Application No. 21822731.2.