Doubly oriented electrical steel sheet and manufacturing method therefor

0Forward Citations (#3467307 Global)
0.0/yrCitation Velocity (#3467307 Global)
0.00Citation PageRank (#3467307 Global)
28Prior Art Cited
10Claims (1 Indep. · 9 Dep.)
2Drawings / Sheets

Abstract

A double oriented electrical steel sheet according to an embodiment of the present invention includes: in wt %, Si at 2.0 to 4.0 wt %, Al at 0.01 to 0.04 wt %, S at 0.0004 to 0.002 at %, Mn at 0.05 to 0.3 wt %, N at 0.008 wt % or less (excluding 0 wt %), C at 0.005 wt % or less (excluding 0 wt %), P at 0.005 to 0.15 wt %, Ca at 0.0001 to 0.005 wt %, Mg at 0.0001 to 0.005 wt %, and the balance including Fe and other impurities unavoidably added thereto.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.

Claims (10 — 1 Independent, 9 Dependent)

  1. Claim 1Independent Claim

    A double oriented electrical steel sheet, including: in wt %, Si at 2.0 to 4.0 wt %, Al at 0.01 to 0.04 wt %, S at 0.0004 to 0.002 wt %, Mn at 0.05 to 0.3 wt %, N at 0.008 wt % or less (excluding 0 wt %), C at 0.005 wt % or less (excluding 0 wt %), P at 0.005 to 0.15 wt %, Ca at 0.00010 to 0.005 wt %, Mg at 0.00010 to 0.005 wt %, and the balance including Fe and other impurities unavoidably added thereto, wherein an area fraction of a grain with an orientation within 15 ° is 60 to 99% from {100} < 001 >, wherein the double oriented electrical steel sheet satisfies Formula 1: [Ca]+[Mg] ≥ [S] [Formula 1] (in Formula 1, [Ca], [Mg], and [S] represent contents (wt %) of Ca, Mg, and S, respectively).

  2. Claim 2Depends on #1

    The double oriented electrical steel sheet of claim 1, further comprising one or more of Sb at 0.001 to 0.1 wt % and Sn at 0.001 to 0.1 wt %.

  3. Claim 3Depends on #1

    The double oriented electrical steel sheet of claim 1, further comprising one or more of Ti at 0.01 wt % or less, Mo at 0.01 wt % or less, Bi at 0.01 wt % or less, Pb at 0.01 wt % or less, Mg at 0.01 wt % or less, As at 0.01 wt % or less, Be at 0.01 wt % or less, and Sr at 0.01 wt % or less.

  4. Claim 4Depends on #1

    The double oriented electrical steel sheet of claim 1, wherein an average grain size is 20 times or more a thickness of the steel sheet.

  5. Claim 5Depends on #1

    The double oriented electrical steel sheet of claim 1, wherein the steel sheet comprises an oxide layer formed from a surface of a substrate forming the steel sheet in a direction inside the substrate and an insulating layer formed on the surface of the substrate.

  6. Claim 6Depends on #5

    The double oriented electrical steel sheet of claim 5, wherein a thickness of the oxide layer is 5 μ m or less.

  7. Claim 7Depends on #5

    The double oriented electrical steel sheet of claim 5, wherein a thickness of the insulating layer is 0.2 to 8 μ m.

  8. Claim 8Depends on #5

    The double oriented electrical steel sheet of claim 5, further comprising a forsterite layer interposed between the surface of the substrate and the insulating layer.

  9. Claim 9Depends on #1

    The double oriented electrical steel sheet of claim 1, wherein Br in a rolling direction and Br in a transverse direction are equal to or larger than 1.63 T, Br in a circumferential direction is equal to or larger than 1.56 T, and the Br is calculated by Formula 2: Br=7.87/(7.87 − 0.065 × [Si] − 0.1105 × [Al]) × B8 [Formula 2] (in Formula 2, [Si] and [Al] are contents (wt %) of Si and Al, respectively, and B8 is intensity (Tesla) of a magnetic field induced at 800 A/m).

  10. Claim 10Depends on #1

    The double oriented electrical steel sheet of claim 1, wherein a Br value measured after annealing the steel sheet at a temperature of 750 ° C. to 880 ° C. for 1 to 2 hours is equal to or larger than 1.65 T, and the Br is calculated by Formula 2: Br=7.87/(7.87 − 0.065 × [Si] − 0.1105 × [Al]) × B8 [Formula 2] (in Formula 2, [Si] and [Al] are contents (wt %) of Si and Al, respectively, and B8 is intensity (Tesla) of a magnetic field induced at 800 A/m).

Technical Overview & Description

CROSS-REFERENCE OF RELATED APPLICATIONS This application is the U.S. National Phase under 35 U.S.C. § 371 of International Patent Application No. PCT/KR2019/012471, filed on Sep. 25, 2019, which in turn claims the benefit of Korean Application No. 10-2018-0115267, filed on Sep. 27, 2018, the entire disclosures of which applications are incorporated by reference herein. TECHNICAL FIELD An embodiment of the present invention relates to a double oriented electrical steel sheet and a manufacturing method thereof. Specifically, an embodiment of the present invention relates to a double oriented electrical steel sheet and a manufacturing method thereof that may have very excellent magnetism in a rolling direction and a transverse direction by appropriately controlling contents of Mg and Ca in an alloy composition to increase a fraction of grains having an orientation of {110} < 001 > . BACKGROUND ART A method for increasing magnetic flux density of an electrical steel sheet is improving texture of a steel and arranging an axis of < 100 > in a magnetization direction is known to be the most efficient. In addition, an additional method in use is reducing an alloy amount of the steel to increase a fraction for Fe to occupy the steel, and allowing a saturated magnetic flux to approach that of pure iron to thus increase the magnetic flux density. An oriented electrical steel sheet among them uses an orientation of {110} < 001 > that is referred to as a Goss orientation, and it is conventionally obtained through a process of manufacturing a slab, and hot rolling, hot-rolled steel sheet annealing, cold rolling, decarburization during first recrystallization, nitriding, and secondary high-temperature annealing. However, this has excellent magnetism in the rolling direction (RD) and very poor magnetism in the transverse direction (TD), so it is only usable for a transformer of which the magnetization direction is set to be the rolling direction. Therefore, it is required to manufa

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (3)

  • Written Opinion and International Search Report dated Jan. 14, 2020 issued in International Patent Application No. PCT/KR2019/012471 (with partial English translation).
  • Japanese Office Action dated Apr. 26, 2022 issued in Japanese Patent Application No. 2021-517630.
  • Extended European Search Report dated Oct. 27, 2021 issued in European Patent Application No. 19866768.5.