Method and device for stabilizing precursor fibers or films for producing carbon fibers or films
Abstract
A process for stabilizing precursor fibers for the production of carbon fibers is disclosed. The process comprises the following steps: continuously introducing, passing and removing said precursor fibers into, through and from a process chamber; establishing a predetermined process gas atmosphere different in composition from ambient air in said at least one process chamber, said process gas atmosphere containing at least one of a reactive component and a catalyst having a predetermined partial pressure; while said precursor fibers are in said process chamber, heating the precursor fibers to at least a first temperature and maintaining said first temperature for a predetermined period of time.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.
Claims (21 — 1 Independent, 20 Dependent)
- Claim 1Independent Claim
A method for stabilizing precursor fibers for the production of carbon fibers, comprising the steps of: continuously introducing, passing and removing the precursor fibers into, through and from a process chamber; setting a predetermined process gas atmosphere different in composition from ambient air in said process chamber, said process gas atmosphere being below atmospheric pressure and containing air and/or pure oxygen as a reactive component and/or catalyst, the air and/or pure oxygen having a predetermined partial pressure; while the precursor fibers are in the process chamber, heating the precursor fibers to at least a first temperature and maintaining the first temperature for a predetermined period of time, wherein the method is free from steps in which magnetic fields are applied to the precursor fibers in the process chamber.
- Claim 2Depends on #1
The method according to claim 1, wherein the pressure in the process chamber is at least 90% of ambient pressure.
- Claim 3Depends on #1
The method according to claim 1, further comprising heating the precursor fibers to at least a second temperature while the precursor fibers are in the process chamber, the second temperature being higher than the first temperature, and maintaining the temperature for a predetermined period of time.
- Claim 4Depends on #3
The method according to claim 3, wherein the precursor fibers are heated from the first temperature to that of the second temperature via at least one further intermediate temperature, wherein the temperature difference between temporally successive stages is at least 5 ° C., and wherein precursor fibers are held at the at least one intermediate temperature for a predetermined period of time.
- Claim 5Depends on #1
The method according to claim 1, wherein the second temperature is higher than the first temperature by at least 30 ° C.
- Claim 6Depends on #1
The method according to claim 1, wherein the precursor fibers are kept at the first temperature, the second temperature and at least one optional intermediate temperature for at least 10 min each.
- Claim 7Depends on #1
The method according to claim 1, wherein the precursor fibers comprise polyacrylonitrile fibers and the first temperature is in the range 220 to 320 ° C. and the second temperature is in the range 280 to 400 ° C.
- Claim 8Depends on #7
The method according to claim 7, wherein the first temperature is in the range 260 to 320 ° C. and the second temperature is in the range 300 to 380 ° C.
- Claim 9Depends on #1
The method according to claim 1, wherein the precursor fibers comprise polyacrylonitrile fibers and the process gas atmosphere has as reactive component oxygen with a partial pressure of from 5 to 60 mbar.
- Claim 10Depends on #1
The method according to claim 1, wherein the precursor fibers are based on cellulose and/or lignin and the first temperature is in the range 200-240 ° C. and the second temperature is in the range 240-300 ° C.
- Claim 11Depends on #1
The method according to claim 1, wherein the precursor fibers comprise cellulose and the process gas atmosphere is an acidic atmosphere promoting dehydration of cellulose.
- Claim 12Depends on #11
The method according to claim 11, wherein the acidic, sulfur- or boron-containing component in the process gas is controlled via the partial pressure to control dehydration.
- Claim 13Depends on #11
The method according to claim 11, wherein the acid, sulfur or boron containing component in the process gas is controlled by the partial pressure to control the activation.
- Claim 14Depends on #1
The method according to claim 1, wherein the precursor fibers comprise cellulose and/or lignin and the process gas atmosphere comprises sulfur-containing compounds.
- Claim 15Depends on #1
The method according to claim 1, wherein the precursor fibers comprise polyacrylonitrile and/or cellulose and/or lignin and the process gas atmosphere comprises boron-containing compounds.
- Claim 16Depends on #1
The method according to claim 1, wherein the precursor fibers comprise lignin and a latent curing agent and the process gas atmosphere is an acidic atmosphere that activates the latent curing agent in the lignin.
- Claim 17Depends on #1
The method according to claim 1, wherein the precursor fibers are lignin processed in a curing atmosphere of formaldehyde.
- Claim 18Depends on #1
The method according to claim 1, wherein the precursor fibers are kept under defined tension during the process.
- Claim 19Depends on #1
The method according to claim 1, wherein the gas atmosphere is exchanged continuously or intermittently during the stabilization process.
- Claim 20Depends on #1
The method according to claim 1, wherein the precursor fibers are passed through a plurality of substantially parallel process chambers, each adjacent process chamber being connected at one end via a deflection unit in such a way that the fibers remain in the process gas atmosphere.
- Claim 21Depends on #1
The method according to claim 1, wherein the process gas atmosphere comprises a mixture including inert gas in addition to the air and/or pure oxygen, the mixture being selected to produce the predetermined partial pressure of the air and/or pure oxygen in the process gas atmosphere.
Technical Overview & Description
RELATED APPLICATIONS The present invention is a U.S. National Stage under 35 USC 371 patent application, claiming priority to Serial No. PCT/EP2019/077438, filed on 10 Oct. 2019; which claims priority from 10 2018 217 354.0, filed 10 Oct. 2018, the entirety of both of which are incorporated herein by reference. TECHNICAL FIELD It is known to produce carbon fibers or carbon sheets or films from different precursor materials. Since the processes are essentially the same for both fibers and sheets, only the fibers will be explained in more detail below. Carbon fibers are technically produced in several process steps. The starting material is usually polyacrylonitrile, in short PAN, but other precursors, in particular lignin, cellulose and polyethylene, are also considered as alternatives for the carbon fiber production. BACKGROUND The first step in the process is to form the starting materials into so-called precursor fibers. These precursor fibers are subsequently converted into carbon fibers in two further process steps in separate sections. The first step is called stabilization while the second is called carbonization. While carbonization usually takes place at high temperatures above 1300 ° C., stabilization, which leads to stabilization or crosslinking of the precursor fibers, takes place at much lower temperatures, usually in the range of 200 ° C. to 300 ° C. This step is necessary to change the molecular structures of the precursor fibers in such a way that the fibers can withstand the thermal stress during carbonization. Stabilization is usually carried out in a forced-air oven with separately heatable zones, in which the precursor fibers are heated to temperatures between 200 ° C. and 300 ° C. and react with the oxygen in the air at atmospheric pressure. The stabilization process produces gaseous reaction products, such as carbon dioxide, hydrocyanic acid, carbon monoxide and ammonia, which have to be removed and disposed of in a controlled manner. This resul
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (7)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (3)
- English Translation of JP2010-242248 https://www.j-platpat.inpit.go.jp/p0200 (Year: 2010).
- Structure and properties of oxidatively stabilized viscose rayon fibers impregnated with boric acid and phosphoric acid prior to carbonization and activation steps, Oct. 27, 2013, Vo. 48, p. 2009-2021). https://link.springer.com/article/10.1007/s10853-012-6970-5 (Year: 2012).
- PCT International Search Report for corresponding International Application Serial No. PCT/EP2019/077438, mailed Nov. 15, 2019, pp. 1-2.