hottub.patents
US 12,378,629 B2#3479297 Most CitedActiveUnited States (USPTO)Utility

Wire rod for ultrahigh-strength steel cord and manufacturing method thereof

0Forward Citations (#3479297 Global)
0.0/yrCitation Velocity (#3479297 Global)
0.00Citation PageRank (#3479297 Global)
10Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

The present invention discloses a wire rod for an ultrahigh-strength steel cord and a manufacturing method thereof. The manufacturing method includes: smelting molten steel where inclusions in sizes ≥ 5 μ m are at a number density ≤ 0.5/mm 2 and sizes of inclusions are ≤ 30 μ m; casting the molten steel into an ingot blank with a center carbon segregation value of 0.92-1.08; cogging the ingot blank into an intermediate blank with a center carbon segregation value of 0.95-1.05; rolling the intermediate blank into a wire rod; and performing temperature control cooling on the wire rod to obtain a wire rod with high purity, high homogeneity and tensile strength ≤ 1,150 MPa. The wire rod may be used for an ultrahigh-strength steel cord with single tensile strength ≥ 3,600 MPa.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A manufacturing method for a wire rod for an ultrahigh-strength steel cord, wherein the wire rod comprises the following chemical components in percentage by mass: 0.78%-0.96% of C, 0.15%-0.30% of Si, 0.30%-0.60% of Mn, ≤ 0.02% of P, ≤ 0.02% of S, ≤ 0.004% of Al, ≤ 0.001% of Ti, ≤ 0.005% of N, ≤ 0.50% of Cr, ≤ 0.05% of Ni, ≤ 0.05% of Cu, ≤ 0.01% of Mo, ≤ 0.10% of Nb, ≤ 0.10% of V, ≤ 0.01% of Sn, ≤ 0.02% of Pb, and the balance of Fe and other inevitable impurities, the manufacturing method sequentially comprising the following steps: a steel smelting stage: smelting molten steel where inclusions in sizes ≥ 5 μ m are at a number density ≤ 0.5/mm 2 and sizes of inclusions are ≤ 30 μ m; a blank casting stage: casting tapped molten steel from the steel smelting stage into an ingot blank with a center carbon segregation value of 0.92-1.08; a cogging stage: cogging the ingot blank into an intermediate blank with a center carbon segregation value of 0.95-1.05, wherein the cogging stage sequent

  2. Claim 2Depends on #1

    The manufacturing method for a wire rod for an ultrahigh-strength steel cord according to claim 1, wherein the steel smelting stage sequentially comprises molten iron desulphurization, furnace primary smelting, external refining and inclusion removal; and in the furnace primary smelting procedure, no other slag formers but a carburant, ferrosilicon and manganese are sequentially added during tapping, and 90% or more of slag on a surface of the tapped molten steel is removed after tapping.

  3. Claim 3Depends on #2

    The manufacturing method for a wire rod for an ultrahigh-strength steel cord according to claim 2, wherein dephosphorization and decarburization are performed using a converter or an electric furnace before tapping in the furnace primary smelting procedure; when dephosphorization and decarburization are performed using the converter, a weight of molten iron is 85%-95% of a total charge weight, dephosphorization is performed at first to obtain semi-steel molten iron containing ≤ 0.03% of P, then decarburization is performed, and the molten steel is controlled to be at a temperature ≥ 1,680 ° C. and contain ≤ 0.015% of P and ≥ 0.2% of C; or when dephosphorization and decarburization are performed using the electric furnace, the weight of the molten iron is 50%-90% of the total charge weight, and after dephosphorization and decarburization, the molten steel is controlled to be at a temperature ≥ 1,650 ° C. and contain ≤ 0.015% of P and ≥ 0.5% of C.

  4. Claim 4Depends on #2

    The manufacturing method for a wire rod for an ultrahigh-strength steel cord according to claim 2, wherein the external refining procedure sequentially comprises: adjusting chemical components and temperature of the molten steel; adding a refining covering agent to a surface of the molten steel according to a proportion of 8-12 kg/t, and melting the refining covering agent in an energized state to make a content of SiO 2 in the inclusions of the molten steel ≥ 40 mass %; and removing the inclusions in the molten steel by soft stirring or vacuum refining.

  5. Claim 5Depends on #4

    The manufacturing method for a wire rod for an ultrahigh-strength steel cord according to claim 4, wherein the step of “ adjusting chemical components and temperature of the molten steel ” and the step of “ adding a refining covering agent to a surface of the molten steel according to a proportion of 8-12 kg/t, and melting the refining covering agent in an energized state to make a content of SiO 2 in the inclusions of the molten steel ≥ 40 mass % ” are performed in a ladle furnace (LF); and after the refining covering agent is added to the surface of the molten steel according to the proportion of 8-12 kg/t, a ladle bottom argon blowing intensity of the LF is controlled to be ≤ 0.005 Nm 3 /(t · min) to make the content of SiO 2 in the inclusions of the molten steel ≥ 40 mass %, a content of CaO ≤ 30 mass % and a content of Al 2 O 3 ≤ 10 mass %.

  6. Claim 6Depends on #4

    The manufacturing method for a wire rod for an ultrahigh-strength steel cord according to claim 4, wherein in the step of “ removing the inclusions in the molten steel by soft stirring or vacuum refining ”: when the inclusions in the molten steel are removed by soft stirring, a ladle bottom argon blowing intensity of an LF is controlled to be 0.001 Nm 3 /(t · min)-0.005 Nm 3 (t · min), soft stirring time is ≥ 30 minutes, and then killing treatment is performed for 15-20 minutes; when the inclusions are removed by vacuum refining through an RH vacuum furnace, the molten steel is treated for 15-25 minutes in a high vacuum environment with a vacuum degree ≤ 1.5 mbar in a vacuum chamber of the RH vacuum furnace, and then killing treatment is performed for 10-15 minutes; or when the inclusions are removed by vacuum refining through a vacuum decarburization (VD)/vacuum oxygen decarburization (VOD) furnace, the molten steel is treated for 15-25 minutes in a high vacuum environment with a vacu

  7. Claim 7Depends on #2

    The manufacturing method for a wire rod for an ultrahigh-strength steel cord according to claim 2, wherein in the inclusion removal procedure, tapped molten steel obtained by external refining is transferred to a tundish with an electromagnetic induction heating function, the inclusions in the molten steel are removed under an electromagnetic centrifugal force, and an electromagnetic induction coil is controlled to achieve a voltage of 200-1,500 V, a frequency of 300-800 Hz and a maximum heating rate of 3 ° C./min.

  8. Claim 8Depends on #1

    The manufacturing method for a wire rod for an ultrahigh-strength steel cord according to claim 1, wherein a superheat degree of the tapped molten steel of the steel smelting stage is 15-25 ° C.; and in the blank casting stage, the tapped molten steel of the steel smelting stage is poured into a continuous casting device to be processed into a continuously cast blank, a crystallizer of the continuous casting device has an electromagnetic stirring function so as to electromagnetically stir the poured molten steel, the crystallizer is controlled to achieve a current of 500 A-800 A and a frequency of 1 Hz-5 Hz, an array withdrawal straightener and fan section of the continuous casting device are used for forming the continuously cast blank, and the array withdrawal straightener has a single-roll reduction ≥ 5 mm, a total reduction ≥ 30 mm, the total reduction being controlled to be 10 mm-30 mm during implementation, and a total reduction ratio of 3%-10%.

Technical Overview & Description

CROSS REFERENCE TO RELATED APPLICATIONS The present application is a 35 U.S.C. § 371 National Phase conversion of International (PCT) Patent Application No. PCT/CN2019/111668, filed on Oct. 17, 2019, which claims priority to Chinese Patent Application No. 201910914918.X, filed on Sep. 26, 2019 and tiled “ Wire Rod for Ultrahigh-strength Steel Cord and Manufacturing Method Thereof ” , which is incorporated herein by reference in its entirety. The PCT International Patent Application was filed and published in Chinese. TECHNICAL FIELD The present invention belongs to the technical field of iron and steel smelting, and relates to a wire rod for producing an ultrahigh-strength steel cord and a manufacturing method thereof. BACKGROUND In recent years, domestic automobiles have developed rapidly, and the automobile production and sales of China have ranked first in the world. It has been found that the fuel consumption of an automobile is correspondingly almost halved if the overall weight thereof is halved. For present requirements on environmental protection and energy conservation, lightweight automobile has become a world trend of automobile development nowadays. Steel cord is a main frame work material for meridian lines of automobile tires. The weight of an automobile tire may be reduced by 10% when the strength of the steel cord is improved by a level. Therefore, demands for ultrahigh-strength steel cords are increasing with the development of automobiles to a lightweight direction. At present, wire rods for producing ultrahigh-strength steel cords are all high-strength wire rods. In practice, the strength of a manufactured steel cord is usually ensured by improving the strength of a wire rod so as to meet a requirement for ultrahigh strength of the steel cord. However, these high-strength wire rods have the problems of high drawing fracture rate, relatively high stranding fracture rate, high mold loss, low yield, etc. SUMMARY An objective of the present invention

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (10)

PatentTitleYearCitations

Non-Patent Literature (1)

  • CN106591700A Translation (Year: 2017).