hottub.patents
US 12,378,622 B2#3479304 Most CitedActiveUnited States (USPTO)Utility

High-strength steel bar and production method thereof

0Forward Citations (#3479304 Global)
0.0/yrCitation Velocity (#3479304 Global)
0.00Citation PageRank (#3479304 Global)
4Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

Disclosed are a high-strength steel bar and a production method therefor. The high-strength steel bar comprises, by mass percentage, the following chemical components: C: 0.15-0.32%, Si+Mn: 0.5-1.9%, Mn+Cr+Mo+Ni: 1.1-2.1%, V: 0.02-0.8%, at least one of Nb, Ti and Al: 0.01-0.3%, and the balance of Fe and inevitable impurities; wherein Mn=(2.5-3.5)Si, and a carbon equivalent satisfies Ceq=C+Mn/6+(Cr+Mo+V)/5+(Cu+Ni)/15 ≤ 0.56%.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A high-strength steel bar, comprising, by mass percentage, the following chemical components: C: 0.15-0.32%, Si+Mn: 0.5-1.9%, Mn+Cr+Mo+Ni: 1.1-2.1%, V: 0.02-0.8%, at least one of Nb, Ti and Al: 0.01-0.3%, and a balance of Fe and inevitable impurities; wherein Mn=(2.5-3.5)Si, and a carbon equivalent satisfies Ceq=C+Mn/6+(Cr+Mo+V)/5+(Cu+Ni)/15 ≤ 0.56%; a microstructure of the high-strength steel bar comprises ferrite, pearlite, bainite and a precipitated phase; the ferrite has a volume percentage of 5-35% and a size of 2-15 μ m, the pearlite has a volume percentage of 30-70%, the bainite has a volume percentage of 5-35% and a size of 5-25 μ m; the high-strength steel bar has a yield strength ≥ 600 MPa, a yield ratio ≤ 0.78, an elongation after fracture ≥ 25%, and an uniform elongation ≥ 15%.

  2. Claim 2Depends on #1

    The high-strength steel bar according to claim 1, comprising, by mass percentage, the following chemical components: C: 0.15-0.29%, Si+Mn: 0.5-1.8%, Mn+Cr+Mo+Ni: 1.1-2.0%, V: 0.05-0.8%, at least one of Nb, Ti and Al: 0.01-0.3% and the balance of Fe and inevitable impurities; wherein Mn=(2.5-3.5)Si, and the carbon equivalent satisfies Ceq=C+Mn/6+(Cr+Mo+V)/5+(Cu+Ni)/15 ≤ 0.54%.

  3. Claim 3Depends on #1

    The high-strength steel bar according to claim 1, comprising, by mass percentage, the following chemical components: C: 0.15-0.32%, Si+Mn: 0.5-1.6%, Cr: 0.3-0.6%, Mn+Cr+Mo+Ni: 1.3-2.0%, V: 0.02-0.8%, at least one of Nb, Ti and Al: 0.01-0.3% and the balance of Fe and inevitable impurities; wherein Mn=(2.5-3.5)Si, and the carbon equivalent satisfies Ceq=C+Mn/6+(Cr+Mo+V)/5+(Cu+Ni)/15 ≤ 0.56%.

  4. Claim 4Depends on #1

    The high-strength steel bar according to claim 1, comprising, by mass percentage, the following chemical components: C: 0.15-0.32%, Si+Mn: 0.5-1.9%, Mn+Cr+Mo+Ni: 1.3-2.1%, V: 0.02-0.8%, B: 0.0008-0.002%, at least one of Nb, Ti and Al: 0.01-0.3% and the balance of Fe and inevitable impurities; wherein Mn=(2.5-3.5)Si, and the carbon equivalent satisfies Ceq=C+Mn/6+(Cr+Mo+V)/5+(Cu+Ni)/15 ≤ 0.56%.

  5. Claim 5Depends on #4

    The high-strength steel bar according to claim 4, comprising, by mass percentage, the following chemical components: C: 0.15-0.32%, Si+Mn: 0.5-1.9%, Mn+Cr+Mo+Ni: 1.1-2.1%, V: 0.02-0.8%, B: 0.0008-0.002%, at least one of Nb and Al: 0.01-0.3%, Ti: 0.01-0.1% and the balance of Fe and inevitable impurities; wherein Ti/N ≥ 1.5, Mn=(2.5-3.5)Si, and the carbon equivalent satisfies Ceq=C+Mn/6+(Cr+Mo+V)/5+(Cu+Ni)/15 ≤ 0.56%.

  6. Claim 6Depends on #1

    The high-strength steel bar according to claim 1, wherein the cross-sectional diameter of the high-strength steel bar is 14-18 mm, the content of C is 0.15-0.3% by mass percentage, and the carbon equivalent Ceq is 0.40-0.52%; or the cross-sectional diameter of the high-strength steel bar is 20-22 mm, the content of C is 0.15-0.3% by mass percentage, and the carbon equivalent Ceq is 0.52-0.54%.

  7. Claim 7Depends on #1

    The high-strength steel bar according to claim 1, wherein the precipitated phase has a size ≤ 100 nm and a volume content ≥ 2*10 5 /mm 3.

  8. Claim 8Depends on #1

    The high-strength steel bar according to claim 1, wherein the ferrite has a volume percentage of 8-30% and a size of 3-12 μ m, the pearlite has a volume percentage of 35-65%, the bainite has a volume percentage of 8-35% and a size of 6-22 μ m, and the precipitated phase has a size ≤ 80 nm and a volume content ≥ 5*10 5 /mm 3.

Technical Overview & Description

The present application is a 35 U.S.C. § 371 National Phase conversion of International (PCT) Patent Application No. PCT/CN2019/096977, filed on Jul. 22, 2019, which claims priority to Chinese Patent Application No. 201910434471.6, filed on May 23, 2019 and tiled “ HIGH-STRENGTH STEEL BAR AND PRODUCTION METHOD THEREOF ” , which is incorporated herein by reference in its entirety. The PCT International Patent Application was filed and published in Chinese. TECHNICAL FIELD The present invention belongs to the technical field of steel and iron materials, and relates to a high-strength steel bar and a production method thereof. BACKGROUND During use of low-level steel bars (including ordinary steel bars), not only is consumption of steel materials increased, consumption of resources and energy is caused, burdens on the environment are increased, but also due to an obvious yield platform and low strength, large plastic deformation is caused in a yield stage when the tensile force is not increased, and thus the safety of a building is seriously affected. Since related requirements of safety levels of major protection projects and other structures are constantly improved, low-level steel bars are unable to fully meet the requirements, and thus high-strength steel bars (such as large deformation resistant steel bars) are produced as required. SUMMARY An objective of the present invention is to provide a high-strength steel bar and a production method thereof, and the steel bar has high strength and no obvious yield platform. To fulfill said objective of the present invention, the present invention provides a high-strength steel bar comprising, by mass percentage, the following chemical components: C: 0.15-0.32%, Si+Mn: 0.5-1.9%, Mn+Cr+Mo+Ni: 1.1-2.1%, V: 0.02-0.8%, at least one of Nb, Ti and Al: 0.01-0.3%, and the balance of Fe and inevitable impurities; wherein Mn=(2.5-3.5)Si, and a carbon equivalent satisfies Ceq=C+Mn/6+(Cr+Mo+V)/5+(Cu+Ni)/15 ≤ 0.56%. As an improvement of

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (4)

PatentTitleYearCitations

Non-Patent Literature (1)

  • CN-104451410-A Translation (Year: 2015).