Method of treating a glazed ceramic article
Abstract
A method of treating a glazed ceramic article comprises applying an antimicrobial composition on top of an outermost surface of a glazed ceramic article. The antimicrobial composition comprises an antimicrobial additive. The antimicrobial composition further comprises a carrier medium. The antimicrobial additive is selected from the group consisting of Bi 2 O 3 , ZnO, Ag 2 CO 3 , Ag 2 O, Zn, Bi, Ag, and a combination thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 65 · Forward citations: 0.
Claims (8 — 1 Independent, 7 Dependent)
- Claim 1Independent Claim
A glazed ceramic article having antimicrobial properties made by the process comprising: (a) applying an antimicrobial composition on top of an outermost surface of a glazed ceramic article, wherein the antimicrobial composition comprises an antimicrobial additive, wherein the antimicrobial additive is a combination of 30 to 69 weight % ZnO, 30 to 69 weight % Bi 2 O 3, and 1 to 10 weight % frit containing Ag, and (b) firing the glazed ceramic article having the antimicrobial composition applied thereon thereby form the glazed ceramic article having antimicrobial properties, wherein the application level of the antimicrobial additive on the glazed ceramic article is in a range of 0.5 g/m 2 to 5.0 g/m 2.
- Claim 2Depends on #1
The article of claim 1, wherein the antimicrobial composition further comprises a carrier medium.
- Claim 3Depends on #2
The article of claim 2, wherein the carrier medium is selected from the group consisting of water, polyethylene glycol, and a combination thereof.
- Claim 4Depends on #1
The article of claim 1, wherein the antimicrobial additive is a combination of 33 weight % ZnO, 66 weight % Bi 2 O 3, and 1 weight % frit containing Ag.
- Claim 5Depends on #1
The article of claim 1, wherein the antimicrobial additive is a combination of 66 weight % ZnO, 33 weight % Bi 2 O 3, and 1 weight % frit containing silver.
- Claim 6Depends on #1
The article of claim 1, wherein the antimicrobial additive is present in the antimicrobial composition in a ratio of solids to carrier medium in a range of 1% to 10%.
- Claim 7Depends on #1
The article of claim 1, wherein the application level of the antimicrobial additive on the glazed ceramic article is in a range of 1.0 g/m 2 to 3.0 g/m 2.
- Claim 8Depends on #1
The article of claim 1, wherein the antimicrobial composition is applied in a layer on the outermost surface of the glazed ceramic article.
Technical Overview & Description
FIELD OF THE INVENTION The present invention relates to ceramics, more particularly to a method for treating a glazed ceramic article with an antimicrobial. BACKGROUND OF THE INVENTION It is known to add minerals to a ceramic glaze to produce a glaze with antimicrobial properties. Minerals having an antimicrobial effect are mixed with the glaze prior to application on a ceramic body and then fired to become a permanent part of the ceramic surface. However, adding minerals having an antimicrobial effect to the ceramic glaze often causes defects and alters texture, color, and other properties. Any and all inorganic minerals added to a ceramic glaze prior to tiring will have some effect on the final properties of the glaze. Minerals that will impart antimicrobial effect often negatively impact desired color and texture properties of the glaze. The properties most often affected are color, texture, and slip resistance (i.e. surface roughness). For example, the zinc level in a glaze affects an antimicrobial addition. Zinc fluxes, which causes more melting, in high temperature glazes. There are also interactions with pigments which often affects color. Also, since many antimicrobial additives are expensive minerals, combining these into a relatively thick glaze layer adds significant cost. Furthermore, much of the minerals having an antimicrobial effect are lost in the depth of the glaze where it cannot affect any bacteria on the surface. Thus, there is a need for an alternative method that overcomes the disadvantages associated with known methods. SUMMARY OF THE INVENTION The invention provides a method for surface application of minerals having an antimicrobial effect on glazed ceramics. In an embodiment of the invention, a method of treating a glazed ceramic article with an antimicrobial is provided. The method comprises applying an antimicrobial composition on top of an outermost surface of a glazed ceramic article, wherein the antimicrobial composition comprises an a
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (65)
| Patent | Title | Year | Citations |
|---|---|---|---|
| CN 1,615,698 A | Compound antiseptic agent | — | 2 |
| EP 0,190,504 A2 | Antimicrobial compositions | — | 2 |
Non-Patent Literature (10)
- Ernest M. Levin, Carl R. Robbins and Howard F. Mcmurdie,
- “
- Phase Diagrams for Ceramists
- ”
- , Compiled at the National Bureau of Standards, Copyright 1964 by the American Ceramic Society, pp. 69 and 120, published in Columbus, Ohio.
- ASTM International Designation: C 347-57 (Reapproved 1983),
- “
- Standard Test Method for Reflectance, Reflectivity, and Coefficient of Scatter of White Porcelain Enamels
- ”
- , copyright ASTM International International, Annual Book of Standards, vol. 14.02, published Dec. 1983, pp. 733-735.