hottub.patents
US 12,374,562 B2#3482943 Most CitedActiveUnited States (USPTO)Utility

Wafer shape control for W2W bonding

0Forward Citations (#3482943 Global)
0.0/yrCitation Velocity (#3482943 Global)
0.00Citation PageRank (#3482943 Global)
27Prior Art Cited
20Claims (2 Indep. · 18 Dep.)
11Drawings / Sheets

Abstract

A method, for bonding a first wafer to a second wafer, includes generating a first modification map based on wafer shape data of the first wafer and the second wafer. The first modification map defines adjustments to internal stresses of the first wafer. A first wafer shape of the first wafer is modified by forming a first stressor film on the first wafer based on the first modification map. The first wafer is aligned with the second wafer after the modifying. The first wafer is bonded to the second wafer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 0.

Claims (20 — 2 Independent, 18 Dependent)

  1. Claim 1Independent Claim

    A method for bonding a first wafer to a second wafer, the method comprising: generating a first modification map, which defines adjustments to internal stresses of the first wafer, based on wafer shape data of the first wafer and the second wafer; modifying a first wafer shape of the first wafer by forming a first stressor film on the first wafer based on the first modification map; aligning the first wafer with the second wafer after the modifying; and bonding the first wafer to the second wafer.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the modifying the first wafer shape of the first wafer further comprises modifying the first stressor film based on the first modification map.

  3. Claim 3Depends on #2

    The method of claim 2, wherein the modifying the first stressor film comprises exposing the first stressor film to a pattern of electromagnetic radiation based on the first modification map.

  4. Claim 4Depends on #3

    The method of claim 3, further comprising developing a photoresist layer of the first stressor film to form a relief pattern.

  5. Claim 5Depends on #4

    The method of claim 4, further comprising etching a shape control layer of the first stressor film using the relief pattern as an etching mask.

  6. Claim 6Depends on #3

    The method of claim 3, wherein the first stressor film is exposed to the pattern of electromagnetic radiation by direct-write.

  7. Claim 7Depends on #2

    The method of claim 2, wherein the modifying the first stressor film comprises applying heat to the first stressor film.

  8. Claim 8Depends on #7

    The method of claim 7, wherein the heat is applied to the first stressor film using a heat array with heat zones having independent temperature control.

  9. Claim 9Depends on #8

    The method of claim 8, further comprising flowing a respective current through each resistor of the heat array so that each resistor generates a respective amount of heat.

  10. Claim 10Depends on #7

    The method of claim 7, wherein the heat is applied to the first stressor film using a laser system that is configured to heat at least one of the first wafer or a wafer chuck that is configured to hold the first wafer.

  11. Claim 11Depends on #2

    The method of claim 2, wherein the modifying the first stressor film comprises implanting ions into the first stressor film.

  12. Claim 12Depends on #1

    The method of claim 1, further comprising keeping the first stressor film unmodified between the forming the first stressor film and the aligning the first wafer with the second wafer.

  13. Claim 13Depends on #11

    The method of claim 11, wherein the forming the first stressor film comprises forming the first stressor film as a blanket film.

  14. Claim 14Depends on #1

    The method of claim 1, wherein: the first wafer has a front side working surface and a backside surface opposite the front side working surface, and the first stressor film is formed on the backside of the first wafer.

  15. Claim 15Depends on #1

    The method of claim 1, further comprising: generating a second modification map, which defines adjustments to internal stresses of the second wafer, based on the wafer shape data of the first wafer and the second wafer; and modifying a second wafer shape of the second wafer by forming a second stressor film on the second wafer based on the second modification map.

  16. Claim 16Depends on #15

    The method of claim 15, wherein the modifying the second wafer shape of the second wafer further comprises modifying the second stressor film based on the second modification map.

  17. Claim 17Depends on #1

    The method of claim 1, further comprising measuring the wafer shape data of the first wafer and the second wafer using one or more metrology tools.

  18. Claim 18Depends on #17

    The method of claim 17, wherein the measuring the wafer shape data comprises measuring relative z-height values of the first wafer and the second wafer by bow measurement.

  19. Claim 19Depends on #1

    The method of claim 1, wherein the first modification map is generated based on historic data in addition to the wafer shape data of the first wafer and the second wafer, the historic data including overlay information of historic wafers.

  20. Claim 20Independent Claim

    A method for bonding a first wafer to a second wafer, the method comprising: receiving wafer shape data of the first wafer and the second wafer from one or more metrology tools; generating a first modification map and a second modification map based on the wafer shape data of the first wafer and the second wafer, wherein the first modification map defines adjustments to internal stresses of the first wafer, and the second modification map defines adjustments to internal stresses of the second wafer; modifying a first wafer shape of the first wafer by forming a first stressor film on the first wafer based on the first modification map; modifying a second wafer shape of the second wafer by forming a second stressor film on the second wafer based on the second modification map; aligning the first wafer with the second wafer after the modifying the first wafer shape and after the modifying the second wafer shape; and bonding the first wafer to the second wafer.

Technical Overview & Description

INCORPORATION BY REFERENCE This present disclosure claims the benefit of U.S. Provisional Application Nos. 63/328,825 and 63/328,823 filed on Apr. 8, 2022, each of which is incorporated herein by reference in its entirety. FIELD OF THE INVENTION This disclosure relates generally to semiconductor fabrication and particularly to wafer overlay control. BACKGROUND Semiconductor fabrication involves multiple varied steps and processes. One typical fabrication process is known as photolithography (also called microlithography). Photolithography uses radiation, such as ultraviolet or visible light, to generate fine patterns in a semiconductor device design. Many types of semiconductor devices, such as diodes, transistors, and integrated circuits, can be constructed using semiconductor fabrication techniques including photolithography, etching, film deposition, surface cleaning, metallization, and so forth. Exposure systems (also called exposure tools) are used to implement photolithographic techniques. An exposure system typically includes an illumination system, a reticle (also called a photomask) or spatial light modulator (SLM) for creating a circuit pattern, a projection system, and a wafer alignment stage for aligning a photosensitive resist-covered semiconductor wafer. The illumination system illuminates a region of the reticle or SLM with a (preferably) rectangular slot illumination field. The projection system projects an image of the illuminated region of the reticle pattern onto the wafer. For accurate projection, it is important to expose a pattern of light on a wafer that is relatively flat or planar, preferably having less than 10 microns of height deviation. SUMMARY The present disclosure relates to a method for bonding wafers together. According to a first aspect of the disclosure, a method, for bonding a first wafer to a second wafer, is provided. The method includes generating a first modification map based on wafer shape data of the first wafer and the se

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (27)

PatentTitleYearCitations

Non-Patent Literature (3)

  • International Search Report
  • &
  • Written Opinion issued Jun. 19, 2023 in PCT/US2023/013553, 9 pages.