hottub.patents
US 12,372,871 B2#3484440 Most CitedActiveUnited States (USPTO)Utility

EUV active films for EUV lithography

0Forward Citations (#3484440 Global)
0.0/yrCitation Velocity (#3484440 Global)
0.00Citation PageRank (#3484440 Global)
26Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

A method of processing a substrate that includes forming over the substrate an extreme ultraviolet (EUV)-active photoresist film including a network of metal oxide terminated with alkoxy groups and patterning the EUV-active photoresist film with EUV lithography.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method of processing a substrate, the method comprising: forming a metal alkoxide by exposing a metal precursor to an alcohol, the metal alkoxide being an intermediate for forming a network of metal oxide, the metal precursor comprising an extreme ultraviolet (EUV) metal and ligands, each of the ligands comprising an alkoxy group, an amine, a carboxylate, or a halogen, the metal precursor not comprising a metal-carbon bond; forming over the substrate an EUV-active photoresist film comprising the network of metal oxide; and patterning the EUV-active photoresist film with EUV lithography.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the metal oxide comprises an alkoxy group comprising a hydrogen at a β position relative to oxygen.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the metal oxide is a tin oxide.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the metal oxide comprises an ethoxide, an iso-propoxide, a tert-butoxide, a cyclohexyl alkoxide, a cyclohexene alkoxide, or a cyclohexadiene alkoxide.

  5. Claim 5Depends on #1

    The method of claim 1, wherein forming the metal alkoxide comprises: before exposing the metal precursor to the alcohol, exposing the substrate to a vapor comprising the metal precursor; and wherein forming the EUV-active photoresist film comprises exposing the metal alkoxide to an oxidant to form metal-oxygen-metal bonds by replacing one or more of the ligands of the metal alkoxide.

  6. Claim 6Depends on #1

    The method of claim 1, wherein forming the EUV-active photoresist film comprises: depositing a layer comprising metal alkoxide over the substrate by exposing the substrate to a vapor comprising the metal alkoxide; and exposing the layer comprising metal alkoxide to an oxidant to form metal-oxygen-metal bonds by replacing one or more ligands of the metal alkoxide.

  7. Claim 7Depends on #6

    The method of claim 6, wherein the oxidant comprises oxygen, ozone, water, air, or hydrogen peroxide.

  8. Claim 8Depends on #6

    The method of claim 6, wherein the vapor and the oxidant are introduced simultaneously into a processing chamber holding the substrate.

Technical Overview & Description

TECHNICAL FIELD The present invention relates generally to extreme ultraviolet (EUV) lithography, and, in particular embodiments, to EUV active films and methods of formation thereof. BACKGROUND Generally, a semiconductor device, such as an integrated circuit (IC) is fabricated by sequentially depositing and patterning layers of dielectric, conductive, and semiconductor materials over a semiconductor substrate to form a network of electronic components and interconnect elements (e.g., transistors, resistors, capacitors, metal lines, contacts, and vias) integrated in a monolithic structure. At each successive technology node, the minimum feature sizes are shrunk to reduce cost by roughly doubling the component packing density. A common patterning method is to use a photolithography process to expose a coating of photoresist over the target layer to a pattern of actinic radiation and then transfer the relief pattern to the target layer or an underlying hard mask layer formed over the target layer. With this technique, the minimum feature size would be limited by the resolution of the optical system. Accordingly, scaling of feature sizes for the 7 nm and 5 nm technology nodes may need 13.5 nm extreme ultraviolet (EUV) lithography. Innovations on EUV photolithographic techniques may be needed to satisfy the cost and quality requirements for patterning at the sub-10 nm node regime. SUMMARY In accordance with an embodiment of the present invention, a method of processing a substrate that includes forming over the substrate an extreme ultraviolet (EUV)-active photoresist film including a network of metal oxide terminated with alkoxy groups and patterning the EUV-active photoresist film with EUV lithography. In accordance with an embodiment of the present invention, a method of processing a substrate in a plasma processing chamber, the method including: exposing the substrate in the plasma processing chamber to a first vapor including a EUV metal precursor; exposing the sub

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (10)

  • Cardineau et al.,
  • “
  • EUV Resists based on Tin-Oxo Clusters
  • ”
  • , Advances in Patterning Materials and Processes XXXI, Proc. of SPIE vol. 9051 90511B-1, downloaded from http://proceedings.spiedigitallibrary.org/ on May 20, 2015, 12 pages.
  • Hinsberg et al.,
  • “
  • A Numberic Model for the Imaging Mechanism of Metal Oxide EUV Resists
  • ”
  • , Inpria Corp., Columbia Hill Techincal Consulting, EUVL Workshop 2018, 21 pages.