hottub.patents
US 12,371,781 B2#3485411 Most CitedActiveUnited States (USPTO)Utility

In situ protective coating of chamber components for semiconductor processing

0Forward Citations (#3485411 Global)
0.0/yrCitation Velocity (#3485411 Global)
0.00Citation PageRank (#3485411 Global)
80Prior Art Cited
8Claims (1 Indep. · 7 Dep.)
0Drawings / Sheets

Abstract

An in situ protective coating is deposited on surfaces of chamber components of a reaction chamber at high temperatures. The in situ protective coating may be deposited at a temperature greater than about 200 ° C. to provide a high quality coating that is resistant to certain types of halogen chemistries, such as fluorine-based species, chlorine-based species, bromine-based species, or iodine-based species. Subsequent coatings or layers may be deposited on the in situ protective coating having different etch selectivities than the underlying in situ protective coating. The in situ protective coating may be deposited throughout the reaction chamber to deposit on surfaces of the chamber components, including on chamber walls.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 80 · Forward citations: 0.

Claims (8 — 1 Independent, 7 Dependent)

  1. Claim 1Independent Claim

    A method comprising: introducing a first reactant in a gas phase into a reaction chamber to adsorb onto surfaces of a plurality of chamber components, wherein the plurality of chamber components are part of the reaction chamber; introducing a second reactant in a gas phase into the reaction chamber; controlling a radio-frequency (RF) signal supplied to the reaction chamber to cause a portion of a plasma glow discharge of the second reactant to form in areas outside an area between an upper electrode and a lower electrode, wherein the first reactant and the second reactant react to deposit a first protective coating on the surfaces of the plurality of chamber components without a wafer present in the reaction chamber; and depositing a second protective coating on a surface of the wafer in the reaction chamber and on the first protective coating in the reaction chamber, wherein the second protective coating is etched at a substantially greater etch rate than the first protective coating

  2. Claim 2Depends on #1

    The method of claim 1, wherein a phase difference between a first phase of the RF signal supplied to the upper electrode and a second phase of the RF signal supplied to the lower electrode is between about 180 degrees out-of-phase and 0 degrees out-of-phase.

  3. Claim 3Depends on #2

    The method of claim 2, wherein the phase difference is about 0 degrees out-of-phase.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the each of the first and second protective coating includes an oxide, a nitride, a carbide, or combinations thereof.

  5. Claim 5Depends on #4

    The method of claim 4, wherein the each of the first and second protective coating includes silicon oxide (SiO 2), aluminum oxide (Al 2 O 3), zirconium oxide (ZrO 2), hafnium oxide (HfO 2), tin oxide (SnO 2), or silicon nitride (Si 3 N 4).

  6. Claim 6Depends on #1

    The method of claim 1, wherein one or more materials of the plurality of chamber components include aluminum (Al).

  7. Claim 7Depends on #1

    The method of claim 1, wherein the plurality of chamber components include at least chamber walls of the reaction chamber.

  8. Claim 8Depends on #1

    The method of claim 1, further comprising: etching the second protective coating on the surface of the wafer and on the first protective coating, wherein the second protective coating is etched at a substantially greater rate than the first protective coating so as to substantially preserve the first protective coating during etching.

Technical Overview & Description

INCORPORATION BY REFERENCE A PCT Request Form is filed concurrently with this specification as part of the present application. Each application that the present application claims benefit of or priority to as identified in the concurrently filed PCT Request Form is incorporated by reference herein in its entirety and for all purposes. BACKGROUND As the semiconductor and other industries advance, device dimensions are becoming increasingly smaller. These progressively smaller features require deposition procedures that are highly uniform, and the presence of film impurities or other non-uniformities can often lead to the failure of a semiconductor device. The background provided herein is for the purposes of generally presenting the context of the disclosure. Work of the presently named inventors, to the extent that it is described in this background, as well as aspects of the description that may not otherwise qualify as prior art at the time of filing, are neither expressly nor impliedly admitted as prior art against the present disclosure. SUMMARY Provided herein is a method of depositing a protective coating in a reaction chamber. The method includes introducing a first reactant in a gas phase into a reaction chamber to adsorb onto surfaces of a plurality of chamber components, where the plurality of chamber components are part of the reaction chamber, and introducing a second reactant in a gas phase into the reaction chamber, where the first reactant and the second reactant react to deposit a protective coating on the surfaces of the plurality of chamber components at a temperature greater than about 200 ° C. In some implementations, the first reactant reacts with the second reactant in a plasma-enhanced atomic layer deposition (PEALD) process. In some implementations, the method further includes controlling a radio-frequency (RF) signal supplied to the reaction chamber to cause a substantial portion of a plasma glow discharge of the second reactant to form in

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (10)

  • Office Action dated Dec. 10, 2015 issued in U.S. Appl. No. 14/089,653.
  • Office Action dated May 13, 2016 issued in U.S. Appl. No. 14/089,653.
  • Final Office Action dated Oct. 28, 2016 issued in U.S. Appl. No. 14/089,653.
  • Notice of Allowance dated Jan. 23, 2017 issued in U.S. Appl. No. 14/089,653.
  • Notice of Allowance dated Jun. 1, 2017 issued in U.S. Appl. No. 14/089,653.
  • Office Action dated Mar. 14, 2018 issued in U.S. Appl. No. 15/650,731.
  • Final Office Action dated Aug. 16, 2018 issued in U.S. Appl. No. 15/650,731.
  • Office Action, dated Aug. 17, 2015, issued in U.S. Appl. No. 14/158,536.
  • Notice of Allowance, dated Jan. 11, 2016, issued in U.S. Appl. No. 14/158,536.
  • Office Action, dated Nov. 18, 2016, issued in U.S. Appl. No. 14/712,167.