Aluminum alloy precision plates

0Forward Citations (#2714968 Global)
0.0/yrCitation Velocity (#2714968 Global)
0.00Citation PageRank (#2714968 Global)
15Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

The present invention relates to plates with a thickness of between 8 and 50 mm and made from aluminum alloy with a composition, as % by weight, Si: 0.7-1.3; Mg: 0.6-1.2; Mn: 0.65-1.0; Fe: 0.05-0.35; at least one element selected from Cr: 0.1-0.3 and Zr: 0.06-0.15; Ti < 0.15; Cu < 0.4; Zn < 0.1; other elements < 0.05 each and < 0.15 in total, the remainder aluminum, and the method for manufacturing same. The plates according to the invention are particularly useful as precision plates, in particular for producing elements of machines, for example assembly or inspection equipment. The plates according to the invention have improved dimensional stability in particular during the machining steps, while having sufficient static mechanical properties, and excellent suitability for anodizing.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method for manufacturing an aluminum alloy plate with a final thickness of between 20 and 30 mm, wherein a) a rolling ingot is cast from aluminum alloy with the composition, as % by weight, Si: 0.7-1.3; Mg: 0.6-1.2; Mn: 0.85-1.0; Fe: 0.05-0.35; at least one element selected from Cr: 0.1-0.3 and Zr: 0.06-0.15; Ti < 0.15; Cu < 0.04; Zn < 0.1; other elements < 0.05 each and < 0.15 in total, remainder aluminum, b) said rolling ingot is homogenized, c) said rolling ingot is rolled at a temperature of at least 340 ° C. and no more than 420 ° C. to obtain a plate, d) optionally heat treatment and/or cold rolling of the plate thus obtained is carried out, e) a solution heat treatment of the plate, optionally heat treated and/or cold rolled is carried out, and said plate is quenched, f) said plate thus solution heat treated and quenched is stress relieved by controlled stretching with a permanent elongation of 1 to 5%, g) aging of the plate thus stretched is carried out, h) optionally said pl

  2. Claim 2Depends on #1

    The method according to claim 1, wherein the Cr content is between 0.15 and 0.25% by weight and the Zr content is less than 0.05% by weight.

  3. Claim 3Depends on #1

    The method according to claim 1, wherein the Fe content is between 0.08 and 0.15% by weight.

  4. Claim 4Depends on #1

    The method according to claim 1, wherein the homogenizing temperature is between 515 ° C. and 545 ° C.

  5. Claim 5Depends on #1

    The method according to claim 1, wherein the hot-rolling temperature is maintained at at least 350 ° C. and the maximum rolling mill draft of passes during hot rolling is less than 50%.

  6. Claim 6Depends on #1

    The method according to claim 1, wherein the hot-rolling temperature is maintained at at least 350 ° C. and the maximum rolling mill draft of passes during hot rolling is less than 50%.

  7. Claim 7Depends on #1

    The method according to claim 1, wherein exit temperature of the hot rolling is no more than 410 ° C.

  8. Claim 8Independent Claim

    A plate with a final thickness of between 20 and 30 mm made from aluminum alloy with a composition, as % by weight, Si: 0.7-1.3; Mg: 0.6-1.2; Mn: 0.85-1.0; Fe: 0.05-0.35; at least one element selected from Cr: 0.1-0.3 and Zr: 0.06-0.15; Ti < 0.15; Cu < 0.04; Zn < 0.1; other elements < 0.05 each and < 0.15 in total, remainder aluminum, obtained by: a) a rolling ingot is cast from the aluminum alloy with the composition b) said rolling ingot is homogenized, c) said rolling ingot is rolled at a temperature of at least 340 ° C. and no more than 420 ° C. to obtain a plate, d) optionally heat treatment and/or cold rolling of the plate thus obtained is carried out, e) a solution heat treatment of the plate, optionally heat treated and/or cold rolled is carried out, and said plate is quenched, f) said plate thus solution heat treated and quenched is stress relieved by controlled stretching with a permanent elongation of 1 to 5%, g) aging of the plate thus stretched is carried out, h) optionall

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application is the National Stage entry of International Application No. PCT/FR2020/051704, filed 29 Sep. 2020, which claims priority to French Application No. 1911024, filed 4 Oct. 2019. BACKGROUND Field The invention relates to plates made from aluminum alloy in the 6xxx series, in particular intended to be used as precision slabs. Description of Related Art Excellent dimensional stability is very important for applications using precision plates, the thickness of which is typically between 8 and 150 mm. This type of product is typically used for producing machine elements, in particular as reference sheets for assembly or inspection equipment. For these applications, it is particularly important to reduce as far as possible any deformation of the plate during machining thereof, which makes it possible to avoid additional operations of premachining or final retouching. The patent application EP2263811 relates to rolled products the surface of which is machined having a flatness of 0.2 mm or less. According to one embodiment of this patent application, the alloy contains 0.3 to 1.5% by mass Mg, 0.2 to 1.6% by mass Si, and in addition one or more elements selected from the group consisting of 0.8% by mass or less Fe, 1.0% by mass or less Cu, 0.6% by mass or less Mn, 0.5% by mass or less Cr, 0.4% by mass or less Zn, and 0.1% by mass or less Ti, the remainder being Al and unavoidable impurities. The patent application WO2014/060660 relates to a vacuum-chamber element obtained by machining and surface treating a plate with a thickness of at least 10 mm made from aluminum alloy with a composition, as % by weight, Si: 0.4-0.7; Mg: 0.4-0.7; Ti 0.01- < 0.15, Fe < 0.25; Cu < 0.04; Mn < 0.4; Cr 0.01- < 0.1; Zn < 0.04; other elements < 0.05 each and < 0.15 in total, the remainder aluminum. The patent application WO2018/162823 relates to a vacuum-chamber element obtained by machining and surface treating a plate with a thickness of

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (15)

PatentTitleYearCitations

Non-Patent Literature (2)

  • Tanner et al., Modelling stress reduction techniques of cold compression and stretching in wrought aluminum alloy products, Elsevier, Finite Elements in Analysis and Design 39 (2003) 369-386. (Year: 2003).
  • PCT International Search Report for PCT/FR2020/051704, mailed Jan. 21, 2021, 4 pages.