Patents
US 12,371,375 B2#97027811 Most CitedActiveUnited States (USPTO)Utility

Cement slurries, cured cement and methods of making and use of these

0Forward Citations (#97027811 Global)
0.0/yrCitation Velocity (#97027811 Global)
0.56Citation PageRank (#97027811 Global)
34Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Cement slurries, cured cements, and methods of making cured cement and methods of using cement slurries are provided. The cement slurries have, among other attributes, improved expanding capabilities and may be used, for instance, in the oil and gas drilling industry. The cement slurry comprises water, a cement precursor material, and an expanding agent. The expanding agent comprising at least a poly(acrylic acid)-metal oxide nanocomposite, where the metal oxide comprises MgO, CaO, or both, and the poly(acrylic acid) comprises a t-butyl terminal group, an isobornyl terminal group, or both.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing a poly(acrylic acid) block copolymer-metal oxide nanocomposite comprising: synthesizing a poly(acrylic acid) block copolymer comprising a t-butyl terminal group, an isobornyl terminal group, or both via reversible addition-fragmentation chain transfer (RAFT) polymerization; and grafting the poly(acrylic acid) onto MgO nanocomposites, CaO nanocomposites, or both, thereby forming the poly(acrylic acid)-metal oxide nanocomposite.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising producing a cement slurry by mixing water, a cement precursor material, and an expanding agent comprising at least the poly(acrylic acid)-metal oxide nanocomposite.

  3. Claim 3Depends on #2

    The method of claim 2 , in which the cement slurry further comprises from 15 to 100 mol. % acid catalyst relative to combined moles of the t-butyl te

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (34)

PatentTitleYearCitations
US 4,569,393 ACO2 -Induced in-situ gelation of polymeric viscosifiers for permeability contrast correction198661
EP 0,212,671 A2Method for emplacement of a gelatinous foam in gas flooding enhanced recovery—16
US 6,875,729 B2Sealing composition200518
US 7,081,295 B2Method of manufacturing a polymethylmethacrylate core shell nanocomposite optical plastic article200613
US 2006167147 A1Metal-containing composite materials—97
US 2007072979 A1Dispersing agents in nanocomposites—22
US 2007160826 A1Polymer composite with silane coated nanoparticles—14
US 7,353,876 B2Self-degrading cement compositions and methods of using self-degrading cement compositions in subterranean formations200813
US 2009082230 A1Well Treatment Fluids Containing Nanoparticles and Methods of Using Same—36
US 2011257289 A1Ab diblock copolymers and applications for their use—20
US 8,053,397 B2Using nanoparticles for water flow control in subterranean formations201123
US 2012067581 A1Mechanism for treating subteranean formations with embedded additives—56
US 2012191214 A1Hydraulic Cement-Based Implant Material and Use Thereof—14
US 8,273,173 B2Nano-additive for hydrocarbon well cementing operations20123
CN 103,497,272 APolymer emulsion and preparation method thereof—17
WO 2014/011603 A1Block copolymers and their composites with inorganic nanoparticles, and methods of making and using same—9
US 8,710,152 B2Block polymers and their process of preparation20143
CN 103,819,111 AApplication of nanometer magnesium oxide in cement base material as expanding agent—14
CN 103,819,702 APreparation method of L-polylactide-modified MgO nano-rod composite material—6
US 8,822,386 B2Nanofluids and methods of use for drilling and completion fluids201470
US 2014374095 A1Nanoparticle slurries and methods—39
US 9,475,922 B2Nanoparticles with multiple attached polymer assemblies and use thereof in polymer composites20169
US 9,611,175 B2Surface-modified calcium oxide20175
WO 2017/137789 A1Release of expansion agents for well cementing—21
WO 2017/137791 A1Ph sensitive encapsulated expansion agent for well cementing—5
US 9,765,252 B2Sealant compositions and methods utilizing nano-particles20176
WO 2017/174208 A1Slurry comprising an encapsulated expansion agent for well cementing—7
WO 2017/218720 A1In situ formed inorganic solids in fracture networks—3
US 9,951,266 B2Expanded wellbore servicing materials and methods of making and using same20186
US 2018298272 A1Polymeric and elastomeric proppant placement in hydraulic fracture network—7

Non-Patent Literature (5)

  • Beavers et al. “Lactic acid-magnesium oxide nanocrystal interactions: how nanoparticle size and shape affect chemistry and template oligomerization” New J. Chem., 2009, 33, 1951-1959, 9 pgs.
  • First Examination Report issued in corresponding Saudi Arabian Application 523440715, pp. 1-7, dated Apr. 17, 2025.
  • Inui et al. “Pressure-Sensitive Adhesion System Using Acrylate Block Copolymers in Response to Photoirradiation and Postbaking as the Dual External Stimuli for On-Demand Dismantling” ACS Appl. Mater. Interfaces 2012, 4, 2124-2132, 9 pgs.
  • Jong et al. “New insights into the hydrolytic degradation of poly(lactic acid): participation of the alcohol terminus” Polymer 42 (2001) 2795-2802, 8 pgs.
  • Ma et al. “Nanocomposites of poly(L-lactide) and surface modified magnesia nanoparticles: Fabrication, mechanical property and biodegradability” Journal of Physics and Chemistry of Solids 72 (2011) 111-116, 6 pgs.