hottub.patents
US 12,371,373 B2#3485790 Most CitedActiveUnited States (USPTO)Utility

Fiber cement products and methods for the production thereof

0Forward Citations (#3485790 Global)
0.0/yrCitation Velocity (#3485790 Global)
0.00Citation PageRank (#3485790 Global)
14Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

The present invention relates to fiber cement products comprising an inner core material, which inner core material is covered by at least one outer surface layer, characterized in that: — said inner core material has a density of between about 0.4 and about 0.9 g/cm 3 inclusive, and at least comprises cement and between 1 wt % and 70 wt % (with respect to the total dry weight of said inner core material) of a lightweight filler, and — said at least one outer surface layer has a density of between about 0.9 and about 1.4 g/cm 3 inclusive, and at least comprises fibers and cement.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method for producing a fiber cement product comprising an inner core covered by at least one outer surface layer, wherein said inner core has a density of between about 0.4 and about 0.9 g/cm 3 inclusive, and wherein said at least one outer surface layer has a density of between about 0.9 and about 1.4 g/cm 3 inclusive, wherein said method comprises the steps of: i) providing a first cementitious material comprising cement and between 1 wt % and 70 wt % with respect to a total dry weight of said inner core of a lightweight filler, ii) providing a second fiber cement material comprising fibers and cement, iii) assembling said first cementitious material and said second fiber cement material to obtain a fiber cement product comprising an inner core made of said first cementitious material, which inner core is covered by at least one outer surface layer made of said second fiber cement material, and iv) curing said fiber cement product, wherein in steps (i) and (ii), a fiber cement slur

  2. Claim 2Depends on #1

    The method according to claim 1, wherein said step (i) comprises providing a first cementitious material comprising cement and between 15 wt % and 70 wt % with respect to the total dry weight of said first cementitious material of expanded perlite.

  3. Claim 3Depends on #1

    The method according to claim 1, wherein said fibers in said at least one outer surface layer comprise cellulose fibers.

  4. Claim 4Depends on #1

    The method according to claim 1, wherein said first cementitious material further comprises fibers.

  5. Claim 5Depends on #1

    The method according to claim 1, wherein forming the one or more uncured fiber cement layers according to the flow-on process comprises a fiber distribution step of discharging a fiber cement slurry composition onto a forming surface.

  6. Claim 6Depends on #5

    The method according to claim 5, wherein the forming surface is a felt transport belt.

  7. Claim 7Depends on #6

    The method according to claim 6, wherein said felt transport belt is a felt transport belt of a Hatschek machine.

  8. Claim 8Depends on #5

    The method according to claim 5, wherein said fiber cement slurry composition is discharged by one or more spraying systems and/or one or more spattering devices.

Technical Overview & Description

FIELD OF THE INVENTION The present invention relates to fiber cement products comprising an inner core material, which inner core material is covered by at least one outer surface material. The present invention further relates to methods for the production of these fiber cement products as well as to uses of these fiber cement products in the building industry. BACKGROUND OF THE INVENTION Fiber cement products, essentially consisting of water, cement and fibers, have been used for buildings since the nineteenth century and have a typical density of between about 1.2-1.7 g/cm 3 . The variation in density is achievable by compression and dewatering of the fiber cement slurries used in manufacture and by varying the amount of fibers used. At these densities, the cement based matrix has few voids, which results in lower water absorption which has usually been considered necessary for good durability performance of cement matrices. Typical fiber cement products are thus heavier than timber-based products of equal dimensions and therefore have a reduced workability. Workability encompasses the ease with which the board is handled and installed. Therefore, fiber cement building products are more difficult to cut, machine and nail than timber and timber-based products. In this regard, the density of natural timber sheets typically ranges from about 0.7-0.9 g/cm 3 for dry hardwoods and from about 0.38-0.6 g/cm 3 for dry softwoods. Thus, a density-modified fiber cement material with a density similar to timber may be expected to improve workability and enable lighter, more nailable, easier to cut and easier to machine products to be manufactured. However, this would have to be achieved while retaining the mechanical performance, durability, fire resistant, rot proof and water resistant properties of fiber cement if the density modified fiber cement is to be used in the same range of applications. The prior art describes how low-density additives can be introduced as density

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (14)

PatentTitleYearCitations

Non-Patent Literature (5)

  • Sakota H et al.,
  • “
  • Fiber-Reinforced Cement Articles,
  • ”
  • Chemical Abstracts, Chemical Abstracts Service (C A S), US, vol. 110, No. 9, May 1, 1989 (May 1, 1989), p. 340.