Methods of producing composite vehicle braking components including aluminum alloys
Abstract
A method of manufacturing a brake rotor or brake drum having a composite structure includes casting an aluminum alloy to form a core of the brake rotor or brake drum, the core defining a core surface, depositing a high entropy alloy or yttrium stabilized zirconia on the core surface to form a thermal barrier layer on the core surface, and depositing an iron-aluminum-silicon-zirconium alloy on the thermal barrier layer to form a wear-resistant layer on the thermal barrier layer, the wear-resistant layer defining a friction surface of the brake rotor or brake drum.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (20 — 3 Independent, 17 Dependent)
- Claim 1Independent Claim
A method of manufacturing a brake rotor or brake drum having a composite structure, the method comprising: casting an aluminum alloy to form a core of the brake rotor or brake drum, the core defining a core surface; depositing a high entropy alloy or yttrium stabilized zirconia on the core surface to form a thermal barrier layer on the core surface; and depositing an iron-aluminum-silicon-zirconium alloy on the thermal barrier layer to form a wear-resistant layer on the thermal barrier layer, the wear-resistant layer defining a friction surface of the brake rotor or brake drum.
- Claim 2Depends on #1
The method of claim 1, wherein depositing the high entropy alloy or yttrium stabilized zirconia includes performing atom layer deposition to deposit the high entropy alloy or yttrium stabilized zirconia on the core surface.
- Claim 3Depends on #2
The method of claim 2, wherein: the atom layer deposition includes a first half-cycle and a second half-cycle; the first half-cycle includes a precursor dosing stage and a purge stage; and the second half-cycle includes a co-reactant exposure stage and a purge stage.
- Claim 4Depends on #3
The method of claim 3, further comprising repeating the first half-cycle and the second half-cycle until a thickness of the thermal barrier layer is greater than or equal to a specified threshold thickness.
- Claim 5Depends on #4
The method of claim 4, wherein the specified threshold thickness is within a range of 35 nanometers to 61 nanometers.
- Claim 6Depends on #4
The method of claim 4, wherein the specified threshold thickness within a range of 61 nanometers to 138 nanometers.
- Claim 7Depends on #2
The method of claim 2, wherein a deposition temperature is less than or equal to 250 degrees Celsius.
- Claim 8Depends on #3
The method of claim 3, wherein the precursor dosing stage includes: applying a tetrakis-(dimethylamido) zirconium (Zr(NMe 2) 4) precursor for zirconia; applying a tris-(methylcyclopentadienyl) yttrium precursor for yttrium; and applying water as an oxidant for each precursor.
- Claim 9Depends on #1
The method of claim 1, wherein depositing the high entropy alloy or yttrium stabilized zirconia includes depositing the high entropy alloy to form the thermal barrier layer on the core surface.
- Claim 10Depends on #1
The method of claim 1, wherein depositing the high entropy alloy or yttrium stabilized zirconia includes depositing the yttrium stabilized zirconia to form the thermal barrier layer on the core surface.
- Claim 11Depends on #1
The method of claim 1, wherein: depositing the yttrium stabilized zirconia includes depositing the yttrium stabilized zirconia in one or more super cycle; and each super cycle includes depositing seven cycles of zirconia and depositing one cycle of yttrium.
- Claim 12Depends on #11
The method of claim 11, wherein a growth rate of the thermal barrier layer is one nanometer per super cycle of deposition.
- Claim 13Depends on #1
The method of claim 1, wherein depositing the iron-aluminum-silicon-zirconium alloy includes depositing the iron-aluminum-silicon-zirconium alloy on the thermal barrier layer using a directed energy deposition process.
- Claim 14Depends on #1
The method of claim 1, wherein casting the aluminum alloy includes casting an aluminum-silicon alloy to form the core of the brake rotor or brake drum.
- Claim 15Depends on #1
The method of claim 1, wherein: casting the aluminum alloy includes casting the aluminum alloy to form the core in a shape of a cylindrical body of a brake drum, the cylindrical body defining an inner surface and an outer surface; and depositing the high entropy alloy or yttrium stabilized zirconia includes depositing the high entropy alloy or yttrium stabilized zirconia on the inner surface of the cylindrical body.
- Claim 16Depends on #1
The method of claim 1, wherein: casting the aluminum alloy includes casting the aluminum alloy to form the core in a shape of an annular disc of a brake rotor, the annular disc defining at least one annular surface; and depositing the high entropy alloy or yttrium stabilized zirconia includes depositing the high entropy alloy or yttrium stabilized zirconia on the at least one annular surface of the annular disc.
- Claim 17Independent Claim
A method of manufacturing a composite structure for a vehicle braking component, the method comprising: casting an aluminum alloy to form a vehicle braking component core, the vehicle braking component core defining a core surface; depositing a thermally insulating material directly on the core surface of the vehicle braking component core to form a thermal barrier layer; and depositing an iron-aluminum-silicon-zirconium alloy on the thermal barrier layer to form a wear-resistant layer on the thermal barrier layer, the wear-resistant layer defining a friction surface of the vehicle braking component.
- Claim 18Depends on #17
The method of claim 17, wherein depositing the thermally insulating material includes depositing the thermally insulating material using an atom layer deposition process.
- Claim 19Independent Claim
A vehicle braking component having a composite structure, the vehicle braking component comprising: a vehicle braking component core including an aluminum alloy, the vehicle braking component core defining a core surface; a thermally insulating material on the core surface of the vehicle braking component core, the thermally insulating material defining a thermal barrier layer, a thickness of the thermally insulating material being in a range between 50 and 100 nanometers, and the thermally insulating material including a high entropy alloy or yttrium stabilized zirconia deposited on the core surface at least partially by a process other than atomic layer deposition (ALD); and a wear-resistant layer on the thermal barrier layer, the wear-resistant layer comprising an iron-aluminum-silicon-zirconium alloy, and the wear-resistant layer defining a friction surface of the vehicle braking component.
- Claim 20Depends on #19
The vehicle braking component of claim 19, wherein the process other than atomic layer deposition is a physical vapor deposition process.
Technical Overview & Description
INTRODUCTION The information provided in this section is for the purpose of generally presenting the context of the disclosure. Work of the presently named inventors, to the extent it is described in this section, as well as aspects of the description that may not otherwise qualify as prior art at the time of filing, are neither expressly nor impliedly admitted as prior art against the present disclosure. The present disclosure generally relates to methods of producing composite vehicle braking components including aluminum alloys and, more particularly, to using atomic layer deposition to produce a thermal barrier layer of a composite vehicle braking component. Vehicle braking components may be mounted on a rotatable axle of the vehicle, which may be coupled to a wheel of the vehicle. During baking, a friction surface of the vehicle braking component may contact a brake pad, which engages the friction surface to slow or stop rotation of the vehicle braking component and the wheel. Vehicle braking components such as brake rotors and brake drums are oftentimes made of cast iron, which can withstand the high friction forces and high temperatures generated during braking. SUMMARY A method of manufacturing a brake rotor or brake drum having a composite structure includes casting an aluminum alloy to form a core of the brake rotor or brake drum, the core defining a core surface, depositing a high entropy alloy or yttrium stabilized zirconia on the core surface to form a thermal barrier layer on the core surface, and depositing an iron-aluminum-silicon-zirconium alloy on the thermal barrier layer to form a wear-resistant layer on the thermal barrier layer, the wear-resistant layer defining a friction surface of the brake rotor or brake drum. In other features, depositing the high entropy alloy or yttrium stabilized zirconia includes performing atom layer deposition to deposit the high entropy alloy or yttrium stabilized zirconia on the core surface. In other features, the
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (6)
| Patent | Title | Year | Citations |
|---|