hottub.patents
US 12,351,509 B2#3503330 Most CitedActiveUnited States (USPTO)Utility

Window and method of manufacturing the same

0Forward Citations (#3503330 Global)
0.0/yrCitation Velocity (#3503330 Global)
0.00Citation PageRank (#3503330 Global)
38Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

A window including glass configured to protect an electronic panel from an external impact and a manufacturing method therefor include a base substrate having a front surface and a rear surface; and a bezel layer disposed on the rear surface of the base substrate, wherein the front surface of the base substrate has a roughness ranging from 0.2 nm to 3 nm, and at least a portion of the base substrate may be bent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 38 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method of manufacturing a window comprising the operations of: providing an initial window which comprises glass and comprises a lithium oxide and phosphorus oxide (P 2 O 5); and washing the initial window to manufacture the window, wherein the operation of washing comprises: an acid washing operation of providing the initial window into an acidic environment; and a base washing operation of providing the initial window, which has been subjected to the acid washing operation, into a basic environment, and wherein a roughness of the window ranges from 0.2 nm to 3 nm, and wherein the surface roughness of the window is lower than a roughness of the provided initial window.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the acidic environment has a pH of 2 or lower.

  3. Claim 3Depends on #2

    The method of claim 2, wherein the acidic environment comprises an acidic solution including at least one of nitric acid (HNO 3), sulfuric acid (H 2 SO 4), or hydrochloric acid (HCl).

  4. Claim 4Depends on #3

    The method of claim 3, wherein the acid washing operation is performed for about 5 minutes to 10 minutes at a temperature of 60 ° C. to 65 ° C.

  5. Claim 5Depends on #1

    The method of claim 1, wherein the basic environment has a pH of 13 or higher.

  6. Claim 6Depends on #5

    The method of claim 5, wherein the basic environment comprises a basic solution including at least one of sodium hydroxide (NaOH) or potassium hydroxide (KOH).

  7. Claim 7Depends on #1

    The method of claim 1, wherein the window, which has been subjected to the acid washing operation, comprises: a first layer which includes an alkali metal and silicon that has a predetermined silicon content ratio with respect to the alkali metal; and a second layer which is formed on a surface of the first layer and has a higher silicon content ratio than the first layer.

  8. Claim 8Depends on #7

    The method of claim 7, wherein the second layer is formed at a portion of the initial window, from which the alkali metal is eluted out during the acid washing operation.

Technical Overview & Description

CROSS REFERENCE TO RELATED APPLICATION This application is a National Stage Entry of International Application No. PCT/KR2019/004927, filed on Apr. 23, 2019, and claims priority from and the benefit of Korean Patent Application No. 10-2019-0003422, filed on Jan. 10, 2019, which is hereby incorporated by reference for all purposes as if fully set forth herein. BACKGROUND Field Embodiments of the invention relate generally to a window and a method of manufacturing the same, and, more specifically, to a window including glass and a method of manufacturing the same. Discussion of the Background Electronic devices include windows, housing units, and electronic elements. The electronic elements may include various elements such as display elements, touch elements, or detection elements which are activated in response to electrical signals. The windows protect the electronic elements and provide users with active areas. Accordingly, the users provide inputs to the electronic elements through the windows or receive information generated in the electronic elements. Also, the electronic elements may be stably protected from external impact by the windows. Recently, in response to the trend toward slimmer electronic devices, the windows have also been desired to be lightweight and thin, and in order to compensate for resultant structural vulnerability, a variety of methods for strengthening the windows have been researched. The above information disclosed in this Background section is only for understanding of the background of the inventive concepts, and, therefore, it may contain information that does not constitute prior art. SUMMARY The purpose of the present invention is to provide a chemically strengthened window and a method of manufacturing the same. Additional features of the inventive concepts will be set forth in the description which follows, and in part will be apparent from the description, or may be learned by practice of the inventive concepts. A window accordi

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (38)

PatentTitleYearCitations

Non-Patent Literature (3)

  • WO-2013067954-A1 Machine Translation by Clarivate Analytics Retrieved Mar. 5, 2024. (Year: 2024).
  • International Search Report dated Oct. 10, 2019 in International Application No. PCT/KR2019/004927.
  • Extended European Search Report dated Sep. 8, 2022, issued in European Patent Application No. 19909556.3.