A negative electrode material of this application includes silicon-based particles, where the silicon-based particles include: a silicon oxide SiO x , where x is 0.5 to 1.6; and a carbon layer, where the carbon layer covers at least a portion of a surface of the silicon oxide SiO x . In a Raman spectrum, a ratio of a height I 1350 of the silicon-based particles at a peak of 1350 cm − 1 to a height I 1580 at a peak of 1580 cm − 1 satisfies 0 < I 1350 /I 1580 < 5, and a ratio of a height I 510 at a peak of 510 cm − 1 to the height I 1350 at the peak of 1350 cm − 1 satisfies 0 < I 510 /I 1350 < 12. A lithium ion battery prepared from the negative electrode active material has improved first efficiency, cycling performance, and rate performance.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 0.
Claims (18 — 2 Independent, 16 Dependent)
- Claim 1Independent Claim
A negative electrode material, wherein the negative electrode material comprises silicon-based particles, and the silicon-based particles comprise: a silicon oxide SiO x, wherein x is 0.5 to 1.6; and a carbon layer, wherein the carbon layer covers at least a portion of a surface of the silicon oxide SiO x; wherein in a Raman spectrum, a ratio of a height I 1350 of the silicon-based particles at a peak of 1350 cm − 1 to a height I 1580 at a peak of 1580 cm − 1 is 0 < I 1350 /I 1580 < 5; and a ratio of a height I 510 at a peak of 510 cm − 1 to the height I 1350 at the peak of 1350 cm − 1 is 2.3 < I 510 /I 1350 < 12.
- Claim 2Depends on #1
The negative electrode material according to claim 1, wherein the silicon oxide SiO x comprises SiO, SiO 2, nano-Si grains, or any combination thereof.
- Claim 3Depends on #1
The negative electrode material according to claim 1, wherein a specific surface area of the silicon-based particles is 2.5 m 2 /g to 15 m 2 /g.
- Claim 4Depends on #1
The negative electrode material according to claim 1, wherein a thickness of the carbon layer is 3 nm to 40 nm.
- Claim 5Depends on #1
The negative electrode material according to claim 1, wherein an average particle size of the silicon-based particles is 500 nm to 30 μ m.
- Claim 6Independent Claim
A negative electrode, wherein the negative electrode comprises a current collector and a coating on the current collector, and the coating comprises silicon-based particles; wherein the silicon-based particles comprise: a silicon oxide SiO x, wherein x is 0.5 to 1.5; wherein the silicon-based particles further comprise a carbon layer, wherein the carbon layer covers at least a portion of a surface of the silicon oxide SiO x; and wherein in a Raman spectrum, a ratio of a height I 510 at a peak of 510 cm − 1 to the height I 1350 at the peak of 1350 cm − 1 is 2.3 < I 510 /I 1350 < 12.
- Claim 7Depends on #6
The negative electrode according to claim 6, wherein in the Raman spectrum, a ratio of a height I 1350 of the silicon-based particles at a peak of 1350 cm − 1 to a height I 1580 at a peak of 1580 cm − 1 is 0 < I 1350 /I 1580 < 5.
- Claim 8Depends on #6
The negative electrode according to claim 6, wherein the current collector comprises copper, aluminum, nickel, copper alloy, aluminum alloy, nickel alloy, or any combination thereof.
- Claim 9Depends on #6
The negative electrode according to claim 6, wherein an X-ray diffraction pattern of the coating comprises a [004] diffraction pattern and a [110] diffraction pattern, a ratio of a c-axis length C004 of a unit cell length acquired from the [004] diffraction pattern to an a-axis length C110 of a unit cell length acquired from the [110] diffraction pattern, C004/C110, is an orientation index (OI) value of the coating, and the OI value is 7.5 < OI < 18.
- Claim 10Depends on #6
The negative electrode according to claim 6, wherein a specific surface area of the silicon-based particles is 2.5 m 2 /g to 15 m 2 /g.
- Claim 11Depends on #6
The negative electrode according to claim 6, wherein the coating further comprises a binder, wherein the binder comprises polyacrylate, polyimide, polyamide, polyamide imide, polyvinylidene fluoride, styrene butadiene rubber, sodium alginate, polyvinyl alcohol, polytetrafluoroethylene, polyacrylonitrile, sodium carboxymethyl cellulose, potassium carboxymethyl cellulose, or any combination thereof.
- Claim 12Depends on #6
The negative electrode according to claim 6, wherein a peeling strength between the coating and the current collector is greater than or equal to 20 N/m.
- Claim 13Depends on #6
The negative electrode according to claim 6, wherein the coating further comprises graphite particles, wherein a percentage of a quantity of silicon-based particles adjacent to the graphite particles in a total quantity of the silicon-based particles is greater than or equal to 40%; and a distance between the silicon-based particles and the adjacent graphite particles is less than or equal to 500 nm.
- Claim 14Depends on #13
The negative electrode according to claim 13, wherein a weight ratio of the silicon-based particles to the graphite particles is 0.07 to 0.7.
- Claim 15Depends on #13
The negative electrode according to claim 13, wherein a thickness of the carbon layer is 3 nm to 40 nm.
- Claim 16Depends on #13
The negative electrode according to claim 13, wherein an X-ray diffraction pattern of the coating comprises a [004] diffraction pattern and a [110] diffraction pattern, a ratio of a c-axis length C004 of a unit cell length acquired from the [004] diffraction pattern to an a-axis length C110 of a unit cell length acquired from the [110] diffraction pattern, C004/C110, is an orientation index (OI) value of the carbon coating, and the OI value is 7.5 < OI < 18.
- Claim 17Depends on #13
The negative electrode according to claim 13, wherein, in the Raman spectrum, a ratio of a height I 1350 of the silicon-based particles at a peak of 1350 cm − 1 to a height I 1580 at a peak of 1580 cm − 1 is 0 < I 1350 /I 1580 < 5.
- Claim 18Depends on #1
A method of preparing the negative electrode material according to claim 1, wherein the method comprises: heating the silicon oxide SiO x to 200 ° C. to 1500 ° C. in an inert gas atmosphere; injecting a carbon source gas and heating the gas at 200 ° C. to 1500 ° C. for 30 min to 120 min to acquire solids; and pulverizing and sieving the solids.
Technical Overview & Description
CROSS-REFERENCE TO THE RELATED APPLICATIONS This application is a continuation of International Patent Application No. PCT/CN2019/121736 filed on Nov. 28, 2019, the disclosure of which is hereby incorporated by reference in its entirety. TECHNICAL FIELD This application relates to the field of energy storage, and specifically, to a negative electrode material and an electrochemical apparatus and an electronic apparatus containing the negative electrode material, particularly a lithium ion battery. BACKGROUND With popularity of consumer electronic products such as notebook computers, cell phones, tablet computers, portable power sources, and drones, requirements for electrochemical apparatuses therein are becoming increasingly stringent. For example, batteries are required to have a light weight, a high capacity, and a relatively long working life. Lithium ion batteries have dominated the market with their outstanding advantages such as high energy density, high safety, memory-free effect, and long working life. SUMMARY Embodiments of this application provide a negative electrode material and a method for preparing the negative electrode material, in an attempt to resolve at least one problem in the related field to a certain extent. The embodiments of this application further provide a negative electrode, an electrochemical apparatus, and an electronic apparatus that use the negative electrode material. In an embodiment, this application provides a negative electrode material, where the negative electrode material includes silicon-based particles, and the silicon-based particles include: a silicon oxide SiO x , where x is 0.5 to 1.6; and a carbon layer, where the carbon layer covers at least a portion of a surface of the silicon oxide SiO x ; and in a Raman spectrum, a ratio of a height I 1350 of the silicon-based particles at a peak of approximately 1350 cm − 1 to a height I 1580 at a peak of approximately 1580 cm − 1 satisfies approximately 0 < I 1350 /I 1580 < ap
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (29)
Non-Patent Literature (10)
- English translation of CN Publication 107046125, Aug. 2017.
- English translation of KR Publication 100794192, Jan. 2008.
- Extended European Search Report for EP application No. 19953982.6, dated May 2, 2022.
- Notice of Reasons for Refusal, JP application No. 2021-517941, dated May 17, 2022.
- Decision to Grant a Patent, JP application No. 2021-517941, dated Dec. 6, 2022.
- Third Office Action of CN Application No. 201911198111.7, dated Aug. 25, 2021.
- Notification to Grant Patent Right for Invention, CN Application No. 201911198111.7, dated Jan. 5, 2022.
- ISR for International Application PCT-CN2019-121736 mailed Aug. 26, 2020.
- Written Opinion for International Application PCT-CN2019-121736 mailed Aug. 26, 2020.
- First Office Action for Counterpart Application No. CN201911198111.7 mailed Sep. 23, 2020.