hottub.patents
US 12,330,122 B2#3522196 Most CitedActiveUnited States (USPTO)Utility

Preparation method for chelating membrane for purifying wet electronic chemicals

0Forward Citations (#3522196 Global)
0.0/yrCitation Velocity (#3522196 Global)
0.00Citation PageRank (#3522196 Global)
10Prior Art Cited
8Claims (1 Indep. · 7 Dep.)
0Drawings / Sheets

Abstract

Disclosed in the present disclosure is a preparation method for a chelating membrane for purifying wet electronic chemicals, including the following steps: performing hydrophilic treatment on a porous PTFE membrane to obtain a hydrophilic base membrane; sequentially cleaning a chelating resin with a hydrochloric acid solution, a sodium hydroxide solution and deionized water, and then drying; grinding and sieving the cleaned and dried chelating resin to obtain a powder; mixing the powder with polyisobutylene and a polyhexafluoroethylene emulsion, and performing vacuum defoaming to form a membrane coating solution; coating the hydrophilic base membrane with the membrane coating solution to prepare a chelating membrane; and sequentially washing the chelating membrane with a hydrochloric acid solution, a sodium hydroxide solution and pure water until the chelating membrane is neutral, and then drying and storing the chelating membrane.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (8 — 1 Independent, 7 Dependent)

  1. Claim 1Independent Claim

    A preparation method for a chelating membrane for purifying wet electronic chemicals, comprising the following steps: performing hydrophilic treatment on a porous PTFE membrane to obtain a hydrophilic base membrane; sequentially cleaning a chelating resin with a hydrochloric acid solution, a sodium hydroxide solution and deionized water, and then drying, wherein the chelating resin is an iminodiacetic acid chelating resin; grinding and sieving the cleaned and dried chelating resin to obtain a powder; mixing the powder with the polyisobutylene and the polyhexafluoroethylene emulsion at 150-200 ° C. for 4-8 h, and carrying out vacuum defoaming for 3-6 h to form the membrane coating solution; and a mass ratio of the powder to the polyisobutylene to the polyhexafluoroethylene emulsion is (60-75):(5-10):(15-35); and coating the hydrophilic base membrane with the membrane coating solution to prepare a chelating membrane.

  2. Claim 2Depends on #1

    The preparation method for a chelating membrane according to claim 1, further comprising the following steps: sequentially washing the chelating membrane with a hydrochloric acid solution, a sodium hydroxide solution and pure water until the chelating membrane is neutral, and then drying and storing the chelating membrane.

  3. Claim 3Depends on #1

    The preparation method for a chelating membrane according to claim 1, wherein the step of performing hydrophilic treatment on a porous PTFE membrane to obtain a hydrophilic base membrane specifically comprises the following steps: adding the porous PTFE membrane to ethanol for soaking for 0.5-2 h, and then drying in air for 5-30 min; adding nitric acid to a 2-10 wt % potassium permanganate aqueous solution for dissolution at room temperature for 0.5-2 h to obtain a mixed solution; placing the treated PTFE membrane in the mixed solution, and performing heating in a water bath at 50-90 ° C. for 1-3 h; and after the heating is completed, placing the membrane in ultrapure water for ultrasonic washing for 0.1-0.5 h, and then drying in an oven at 40-60 ° C. for 1-2 h to obtain the hydrophilic base membrane.

  4. Claim 4Depends on #3

    The preparation method for a chelating membrane according to claim 3, wherein a volume ratio of the nitric acid to the potassium permanganate aqueous solution is 1:(20-30).

  5. Claim 5Depends on #1

    The preparation method for a chelating membrane according to claim 1, wherein the steps of sequentially cleaning a chelating resin with a hydrochloric acid solution, a sodium hydroxide solution and deionized water, and then drying specifically comprise: sequentially cleaning the chelating resin with the hydrochloric acid solution, the sodium hydroxide solution and the deionized water, and then drying in an oven at 80-90 ° C. for 1-2 h.

  6. Claim 6Depends on #1

    The preparation method for a chelating membrane according to claim 1, wherein the powder is 1,000-3,000 mesh.

  7. Claim 7Depends on #1

    The preparation method for a chelating membrane according to claim 1, wherein the step of coating the hydrophilic base membrane with the membrane coating solution to prepare a chelating membrane specifically comprises: coating the hydrophilic base membrane with the membrane coating solution at a temperature of 150-200 ° C. to prepare the chelating membrane.

  8. Claim 8Depends on #2

    The preparation method for a chelating membrane according to claim 2, wherein the steps of sequentially washing the chelating membrane with a hydrochloric acid solution, a sodium hydroxide solution and pure water until the chelating membrane is neutral, and then drying and storing the chelating membrane specifically comprise: sequentially washing the chelating membrane with the hydrochloric acid solution, the sodium hydroxide solution and the pure water until the chelating membrane is neutral, then drying the chelating membrane in an oven at 80-90 ° C. for 1-2 h, and storing the chelating membrane for later use; and the pure water is electronic-grade ultrapure water and is at a grade of equal to or greater than E1.1.

Technical Overview & Description

This application is the National Stage Application of PCT/CN2023/108034, filed on Jul. 19, 2023, which claims priority to Chinse Patent Application No. 202210751020.7, filed on Jun. 28, 2022, which is incorporated by reference for all purposes as if fully set forth herein. TECHNICAL FIELD The present disclosure relates to the technical field of chelating membranes, and in particular, to a preparation method for a chelating membrane for purifying wet electronic chemicals. BACKGROUND Ultra-clean and high-purity reagents are one of key basic chemical materials in a production process of an ultra-large scale integrated circuit (IC) and are mainly used for cleaning and corrosion of chips as well as cleaning of silicon wafers (wafers), and the purity and cleanliness of the reagents have an extremely important impact on the yield, electrical performance and reliability of the integrated circuit. When the wafers are polluted by metal ions, great harm will be caused to semiconductor components. For example, Fe, Cu, Na and other metals will lead to the production of OISF, thereby increasing a leakage current during binding of a p-n junction and shortening the life of few carriers. The ultra-clean and high-purity reagents have the characteristics of many varieties, large consumption, high technical requirements, a short shelf life, strong corrosion and the like. In China, the ultra-clean and high-purity reagents have been developed and produced since the 1970s. Until now, solid particle impurities in the ultra-clean and high-purity reagents have been controlled, but contents of metal ions in the ultra-clean and high-purity reagents need to be controlled by traditional methods such as distillation and rectification, and these methods have not only a low removal rate of metal ions but also high energy consumption. SUMMARY In view of the disadvantages of the prior art, the present disclosure provides a preparation method for a chelating membrane for purifying wet electronic chemi

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (5)

  • Zhang Zhi-hui et al.,
  • “
  • Adsorption Behaviors of Ni2+ in the DTPA-MA/PVDF Blended Membrane
  • ”