Vitreous coating application by induction heating and integration with induction kinetic weld joining
Abstract
Induction heating facilitated coating systems and processes for pipes overcome corrosion and erosion of the pipes at extreme temperatures and pressures in applications including oil and gas downhole tubulars and pipelines as well as processing facilities. Being based on vitreous fused inorganic compounds, the present invention achieves very high corrosion resistance at remarkably modest cost. Attractive economics and immunity to chlorides and moisture permeation at extreme concentrations and temperatures also make it well suited to desalination plants and potable water piping applications. Due to its extreme temperature resistance, it also is very well suited for geothermal wells. Additionally, due to its characteristic smooth durable surface, the present invention is ideally suited for applications involving the opposite of corrosion, namely scaling problems, such as fouling in sewage systems and scale buildup in heavy oil wells.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.
Claims (4 — 1 Independent, 3 Dependent)
- Claim 1Independent Claim
A method of applying a vitreous coating to a metal pipe by a dry process using induction heating and electrostatic sprayers, the method comprising: advancing an induction heating apparatus along an interior surface of a metal pipe, wherein the induction heating apparatus comprises at least one ring-shaped induction coil, a first baffle and second baffle, wherein the first baffle and second baffle at least partially and circumferentially seal off a portion of the interior surface of the metal pipe in proximity to the at least one ring-shaped induction coil, wherein an enclosed processing area is proximate to the at least one ring-shaped induction coil, wherein the enclosed processing area includes at least one electrostatic sprayer; energizing the at least one ring-shaped induction coil to controllably heat the interior surface of the metal pipe in proximity to the enclosed processing area; energizing the least one electrostatic sprayer and electrostatically spraying a dry frit onto the interior surface of the metal pipe; and forming a vitreous coating on the interior surface of the metal pipe from the dry frit by fusing the dry frit onto the interior surface of the metal pipe as the induction heating apparatus advances along the interior surface of the metal pipe.
- Claim 2Depends on #1
The method of claim 1, wherein at least one of the first baffle and the second baffle are porous to gases.
- Claim 3Depends on #1
The method of claim 1, wherein at least one of the first baffle and the second baffle is associated with a fabric seal circumferentially contacting the interior surface of the pipe.
- Claim 4Depends on #1
The method of claim 1, further comprising: quenching the metal pipe with a ring-shaped quench head, wherein the quench head cooperatively advances along the exterior of the metal pipe as the induction heating apparatus advances along the interior surface of the metal pipe.
Technical Overview & Description
RELATED APPLICATIONS This application is a continuation patent application of U.S. Nonprovisional patent application Ser. No. 17/092,199, filed on Nov. 6, 2020, which claims priority to and the benefit of U.S. Provisional Patent Application No. 62/931,259, filed on Nov. 6, 2019, the entire contents of which are hereby incorporated by reference. TECHNICAL FIELD The invention generally relates to applying a corrosion resistant vitreous coating to the inside or outside of a pipe. More particularly the invention relates to applying a vitreous coating to the inside and/or outside of a pipe by induction heating and integration with induction kinetic welding together of more than one pipe where the area of the weld joining the pipes together is coated with the vitreous coating post welding. BACKGROUND According to the National Association of Corrosion Engineers ( “ NACE ” ), the 2018 total estimated annual cost of corrosion in just the oil and gas exploration and production industry within the United States is about $1.4 billion, broken down into $589 million in surface pipeline and facility costs, $463 million in downhole tubing expenses, and another $320 million in capital expenditures related to corrosion. It is widely recognized in the oil and gas industry that effective management of corrosion contributes towards achieving the critical benefits of statutory and corporate compliance with Health, Safety and Environmental Policy, reduction in leaks, increased plant availability, reduction in unplanned maintenance and reduction in deferment costs. The vast majority of these corrosion issues involve steel operating in environments against which it has insufficient natural resistance. Therefore, once corrosion problems of steel have been identified, the routine response is to upgrade steel's corrosion resistance with barrier coatings and/or cathodic protection or by alloying with sufficient chrome, nickel, molybdenum, cobalt, etc., to remain passive in each specific corrosi
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.