hottub.patents
US 12,312,686 B2#3537467 Most CitedActiveUnited States (USPTO)Utility

Method and apparatus for filling gap using atomic layer deposition

0Forward Citations (#3537467 Global)
0.0/yrCitation Velocity (#3537467 Global)
0.00Citation PageRank (#3537467 Global)
12Prior Art Cited
34Claims (4 Indep. · 30 Dep.)
34Drawings / Sheets

Abstract

A method and an apparatus for filling a gap by using an atomic layer deposition (ALD) method are provided. The method includes forming a first reaction inhibition layer by adsorbing a reaction inhibitor onto a side wall of the gap, forming a first precursor layer by adsorbing a first reactant onto the bottom of the gap and the side wall of the gap around the bottom of the gap, and forming a first atomic layer on the bottom of the gap and the side wall of the gap around the bottom of the gap. The reaction inhibitor includes a precursor material that does not react with a second reactant. The first reaction inhibition layer may have a density gradient in which a density of the reaction inhibitor decreases toward a bottom of the gap. The forming the first atomic layer includes adsorbing the second reactant onto the first precursor layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.

Claims (34 — 4 Independent, 30 Dependent)

  1. Claim 1Independent Claim

    A method of filling a gap formed on a substrate using atomic layer deposition (ALD), the method comprising: forming a first reaction inhibition layer by adsorbing a reaction inhibitor onto a side wall of the gap, the reaction inhibitor including a precursor material that does not react with a second reactant, and the first reaction inhibition layer having a density gradient in which a density of the reaction inhibitor decreases toward a bottom of the gap; forming a first precursor layer by adsorbing a first reactant onto the bottom of the gap and the side wall of the gap around the bottom of the gap; and forming a first atomic layer on the bottom of the gap and the side wall of the gap around the bottom of the gap, the forming the first atomic layer including adsorbing the second reactant onto the first precursor layer, wherein the reaction inhibitor includes a center metal and a cyclopentadienyl (Cp) ligand, the center metal and a pentamethyl cyclopentadienyl (Cp*) ligand, Hf(t BuO) 4, Hf(O i Pr) 4, or Hf(O t Bu)(NEtMe) 3.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the density gradient of the first reaction inhibition layer is determined according to a following equation: l = 4 ⁢ w 3 ⁢ (1 + 3 8 ⁢ (P ⁢ t S ⁢ 2 ⁢ π ⁢ ⁢ m ⁢ ⁢ kT) - 1) where indicates a depth (nm) of a location of the side wall of the gap, onto which the reaction inhibitor is adsorbed, w indicates a width (nm) of the gap, P indicates a partial pressure (Pa) of the reaction inhibitor in a reaction chamber, t indicates an exposure time (s) of the reaction inhibitor, m indicates a molecular mass (kg) of the reaction inhibitor, S indicates a saturation dose of about 2.5 × 10 18 molecules*meter, k indicates a Boltzmann factor 1.38 × 10 23 J/K, and T indicates a temperature (K) in the reaction chamber.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the reaction inhibitor is oxidized by O 3 or an O 2 plasma.

  4. Claim 4Depends on #1

    The method of claim 1, further comprising: converting the reaction inhibitor into a material of the first atomic layer via O 3 or O 2 plasma processing.

  5. Claim 5Depends on #1

    The method of claim 1, wherein the reaction inhibitor does not react with H 2 O or O 2.

  6. Claim 6Depends on #1

    The method of claim 1, wherein the reaction inhibitor includes the center metal and the Cp ligand.

  7. Claim 7Depends on #1

    The method of claim 1, wherein the reaction inhibitor includes the center metal and the Cp* ligand.

  8. Claim 8Depends on #1

    The method of claim 1, wherein the reaction inhibitor includes TiCp*(OMe) 3, Ti(CpMe)(O i Pr) 3, Ti(CpMe)(NMe 2) 3, ZrCp(NMe 2) 3 ZrCp 2 Cl 2, Zr(Cp 2 CMe 2)Me 2, Zr(Cp 2 CMe 2)Me(OMe), HfCp(NMe 2) 3, or Hf(CpMe)(NMe 2) 3.

  9. Claim 9Depends on #1

    The method of claim 1, wherein the reaction inhibitor has a same center metal as a metal of the first reactant.

  10. Claim 10Depends on #1

    The method of claim 1, wherein the first reactant includes TiCl 4, Ti(O i Pr) 4, Ti(NMe 2) 4, Ti(NMeEt) 4, Ti(NEt 2) 4, ZrCl 4, Zr(NMe 2) 4, Zr(O t Bu) 4, ZrCp 2 Me 2, Zr(MeCp) 2 (OMe)Me, HfCl 4, Hf(NMe 2) 4, Hf(NEtMe) 4, Hf(NEt 2) 4, HfCp2Me 2, or Hf(MeCp) 2 (OMe)Me.

  11. Claim 11Depends on #1

    The method of claim 1, wherein the second reactant includes H 2 O or O 2.

  12. Claim 12Depends on #1

    The method of claim 1, wherein an average density of the reaction inhibitor increases as a partial pressure of the reaction inhibitor in a reaction chamber increases.

  13. Claim 13Depends on #1

    The method of claim 1, wherein the adsorbing the reaction inhibitor is repeatedly performed for a plurality of cycles, and an average density of the reaction inhibitor increases as a number of cycles increases.

  14. Claim 14Depends on #1

    The method of claim 1, further comprising: forming a first filling layer by repeatedly performing the forming the first precursor layer and the forming the first atomic layer for a plurality of cycles, wherein the first filling layer and the first reactant include a same metal.

  15. Claim 15Depends on #14

    The method of claim 14, wherein the density of the reaction inhibitor decreases toward the bottom of the gap so that the first filling layer is formed in a bottom-up direction from the bottom of the gap.

  16. Claim 16Depends on #15

    The method of claim 15, wherein the first filling layer is formed to have a shape varying according to an average density of the reaction inhibitor.

  17. Claim 17Depends on #16

    The method of claim 16, wherein the first filling layer has the shape in which the first filling layer is formed a bottom-up direction from the bottom of the gap.

  18. Claim 18Depends on #16

    The method of claim 16, wherein the first filling layer has the shape in which the first filling layer is formed from the bottom of the gap and the side wall of the gap around the bottom of the gap.

  19. Claim 19Depends on #16

    The method of claim 16, wherein a gap filling process time is adjusted according to the shape in which the first filling layer is formed.

  20. Claim 20Depends on #14

    The method of claim 14, further comprising: forming a second reaction inhibition layer on the side wall of the gap after the forming the first filling layer; forming a second precursor layer on an upper surface of the first filling layer and the side wall of the gap around the upper surface of the first filling layer; and forming a second atomic layer on the upper surface of the first filling layer and the side wall of the gap around the upper surface of the first filling layer.

  21. Claim 21Depends on #20

    The method of claim 20, further comprising: forming a second filling layer in a bottom-up direction from the upper surface of the first filling layer, by repeatedly performing the forming the second precursor layer and the forming the second atomic layer for a plurality of cycles.

  22. Claim 22Independent Claim

    A method of filling a gap formed on a structure using atomic layer deposition (ALD), the structure defining the gap and including a first reaction inhibition layer including a reaction inhibitor adsorbed onto a side wall of the gap, the method comprising: forming a first precursor layer by adsorbing a first reactant onto a first exposed region of the gap, the first exposed region of the gap including a bottom of the gap and first portions of the side wall of the gap around the bottom of the gap, the first reaction inhibition layer defining the first exposed region of the gap based on the first reaction inhibition layer having a density gradient in which a density of the reaction inhibitor decreases toward the bottom of the gap such that the first reaction inhibition layer exposes the first portions of the side wall of the gap and the bottom of the gap, the reaction inhibitor including a precursor material; and forming a first atomic layer on the first exposed region of the gap by adsorbing a second reactant onto the first precursor layer, the second reactant being a material that does not react with the precursor material in the reaction inhibitor, wherein the reaction inhibitor includes a center metal and a cyclopentadienyl (Cp) ligand, the center metal and a pentamethyl cyclopentadienyl (Cp*) ligand, Hf(t BuO) 4, Hf(O i Pr) 4, or Hf(O t Bu) (NEtMe) 3.

  23. Claim 23Depends on #22

    The method of claim 22, wherein the reaction inhibitor is oxidized by O 3 or an O 2 plasma.

  24. Claim 24Depends on #22

    The method of claim 22, further comprising: removing the reaction inhibitor by converting the reaction inhibitor into a material of the first atomic layer via O 3 or O 2 plasma processing.

  25. Claim 25Depends on #22

    The method of claim 22, wherein the reaction inhibitor includes a center metal and an organic ligand.

  26. Claim 26Depends on #22

    The method of claim 22, wherein the second reactant includes H 2 O or O 2.

  27. Claim 27Depends on #1

    The method of claim 1, wherein the reaction inhibitor includes Hf(t BuO) 4, Hf(O i Pr) 4, or Hf(O t Bu)(NEtMe) 3.

  28. Claim 28Depends on #22

    The method of claim 22, wherein the reaction inhibitor includes Hf(t BuO) 4, Hf(O i Pr) 4, or Hf(O t Bu)(NEtMe) 3.

  29. Claim 29Independent Claim

    A method of filling a gap formed on a substrate using atomic layer deposition (ALD), the method comprising: forming a first reaction inhibition layer by adsorbing a reaction inhibitor onto a side wall of the gap, the reaction inhibitor including a precursor material that does not react with a second reactant, and the first reaction inhibition layer having a density gradient in which a density of the reaction inhibitor decreases toward a bottom of the gap; forming a first precursor layer by adsorbing a first reactant onto the bottom of the gap and the side wall of the gap around the bottom of the gap; and forming a first atomic layer on the bottom of the gap and the side wall of the gap around the bottom of the gap, the forming the first atomic layer including adsorbing the second reactant onto the first precursor layer, wherein the reaction inhibitor includes a center metal and a cyclopentadienyl (Cp) ligand, the center metal and a pentamethyl cyclopentadienyl (Cp*) ligand, Hf(t BuO) 4, Hf(O i Pr) 4, or Hf(O t Bu)(NEtMe) 3, the first reactant includes TiCl 4, Ti (OiPr) 4, Ti(NMe 2) 4, Ti(NMeEt) 4, Ti(NEt 2) 4, ZrCl 4, Zr(NMe 2) 4, Zr(O t Bu) 4, ZrCp 2 Me 2, Zr(MeCp) 2 (OMe)Me, HfCl 4, Hf(NMe 2) 4, Hf(NEtMe) 4, Hf(NEt 2) 4, HfCp2Me 2, or Hf(MeCp) 2 (OMe)Me, and the second reactant includes H 2 O or O 2.

  30. Claim 30Independent Claim

    A method of filling a gap formed on a substrate using atomic layer deposition (ALD), the method comprising: forming a first reaction inhibition layer by adsorbing a reaction inhibitor onto a side wall of the gap, the reaction inhibitor including a precursor material that does not react with a second reactant, and the first reaction inhibition layer having a density gradient in which a density of the reaction inhibitor decreases toward a bottom of the gap; forming a first precursor layer by adsorbing a first reactant onto the bottom of the gap and the side wall of the gap around the bottom of the gap; forming a first atomic layer on the bottom of the gap and the side wall of the gap around the bottom of the gap, the forming the first atomic layer including adsorbing the second reactant onto the first precursor layer; forming a first filling layer by repeatedly performing the forming the first precursor layer and the forming the first atomic layer for a plurality of cycles; forming a second reaction inhibition layer on the side wall of the gap after the forming the first filling layer; forming a second precursor layer on an upper surface of the first filling layer and the side wall of the gap around the upper surface of the first filling layer; and forming a second atomic layer on the upper surface of the first filling layer and the side wall of the gap around the upper surface of the first filling layer.

  31. Claim 31Depends on #30

    The method of claim 30, further comprising: forming a second filling layer in a bottom-up direction from the upper surface of the first filling layer, by repeatedly performing the forming the second precursor layer and the forming the second atomic layer for a plurality of cycles.

  32. Claim 32Depends on #22

    The method of claim 22, wherein the reaction inhibitor includes the center metal and the Cp ligand.

  33. Claim 33Depends on #22

    The method of claim 22, wherein the reaction inhibitor includes the center metal and the Cp* ligand.

  34. Claim 34Depends on #22

    The method of claim 22, wherein the reaction inhibitor includes TiCp*(OMe) 3, Ti(CpMe)(O t Pr) 3, Ti(CpMe)(NMe 2) 3, ZrCp(NMe 2) 3, ZrCp 2 Cl 2, Zr(Cp 2 CMe 2)Me 2, Zr(Cp 2 CMe 2)Me(OMe), HfCp(NMe 2) 3, or Hf(CpMe)(NMe 2) 3.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATION This application claims the benefit of Korean Patent Application Nos. 10-2020-0075031, filed on Jun. 19, 2020, and 10-2021-0055001, filed on Apr. 28, 2021, in the Korean Intellectual Property Office, the disclosure of which is incorporated herein in its entirety by reference. BACKGROUND 1. Field The disclosure relates to a method and/or an apparatus for filling a gap using atomic layer-deposition (ALD). 2. Description of Related Art As a process of filling a gap, such as a trench, etc., formed on a substrate, atomic layer deposition (ALD) has been used. For ALD, a surface reaction is used. Thus, when a gap is filled by using the ALD, a filling layer may be formed in a uniform thickness on surfaces around the gap so that a formation of voids may be reduced and/or minimized. However, when the gap has a high aspect ratio, a size of an entrance of the gap may become less than a size of an inner portion of the gap. Thus, even when the ALD is used, voids may be formed. SUMMARY One or more embodiments provide a method and/or an apparatus for filling a gap using an atomic layer deposition (ALD). Additional aspects will be set forth in part in the description which follows and, in part, will be apparent from the description, or may be learned by practice of the presented embodiments of the disclosure. According to an embodiment, there is provided a method of filling a gap formed on a substrate by using atomic layer deposition (ALD). The method includes forming a first reaction inhibition layer by adsorbing a reaction inhibitor onto a side wall of the gap, the reaction inhibitor including a precursor material that does not react with a second reactant, and the first reaction inhibition layer having a density gradient in which a density of the reaction inhibitor decreases toward a bottom of the gap; forming a first precursor layer by adsorbing a first reactant onto the bottom of the gap and the side wall of the gap around the bottom of th

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (12)

PatentTitleYearCitations

Non-Patent Literature (10)

  • Extended European Search Report dated Nov. 22, 2021, issued in corresponding European Patent Application No. 21176278.6.
  • Tushar K. Talukdar et al.,
  • “
  • Seamless fill of deep trenches by chemical vapor deposition: Use of a molecular growth inhibitor to eliminate pinch-off
  • ”
  • Journal of Vacuum Science and Technology A, vol. 37, No. 2, 2019, pp. 021509-1-021509-10.
  • Rizwan Khan et al.,
  • ‘
  • Area-selective Atomic Layer Deposition using Si Precursors as Inhibitors
  • ’