Molten electrolyte dual-phase membranes for intermediate temperature fuel cells
Abstract
In one aspect of an inventive concept, a fuel cell system includes a cathode and an anode, a porous ceramic support positioned between the cathode and anode, and a molten electrolyte mixture in pores of the ceramic support. In another aspect of an inventive concept, a method for producing energy includes directing a gas stream through a cathode, where an inner side of the cathode is adjacent to a dual phase membrane including a ceramic support infiltrated with a molten electrolyte mixture, sweeping an outer side of the anode with water, where an inner side of the anode is adjacent to the dual phase membrane, and collecting energy from the anode. The dual phase membrane is sandwiched between the cathode and an anode.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 0.
Claims (23 — 3 Independent, 20 Dependent)
- Claim 1Independent Claim
A fuel cell system, comprising: a cathode and an anode; a porous ceramic support positioned between the cathode and anode, wherein the ceramic support is comprised of zirconia stabilized with yttria; a molten electrolyte mixture in pores of the ceramic support; and a water flow system on an outer side of the anode, wherein the outer side of the anode is opposite an inner side of the anode, wherein the inner side of the anode is adjacent to the ceramic support, wherein the water flow system is configured to sweep steam across the outer side of the anode.
- Claim 2Depends on #1
A fuel cell system as recited in claim 1, wherein the fuel cell system is operable to generate electricity up to a temperature of 600 degrees Celsius.
- Claim 3Depends on #1
A fuel cell system as recited in claim 1, wherein the fuel cell system is operable to generate electricity at temperatures in a range of about 150 degrees Celsius to about 400 degrees Celsius.
- Claim 4Depends on #1
A fuel cell system as recited in claim 1, wherein the molten electrolyte mixture includes a molten hydroxide mixture, wherein the molten hydroxide mixture includes an alkaline hydroxide having a melting point below 200 degrees Celsius.
- Claim 5Depends on #4
A fuel cell system as recited in claim 4, wherein the ceramic support with the molten hydroxide mixture therein is a hydroxide ceramic dual phase membrane.
- Claim 6Depends on #4
A fuel cell system as recited in claim 4, wherein the molten hydroxide mixture includes at least one cation selected from the group consisting of: lithium, sodium, potassium, cesium, and rubidium.
- Claim 7Depends on #1
A fuel cell system as recited in claim 1, wherein the cathode and the anode are porous.
- Claim 8Depends on #1
A fuel cell system as recited in claim 1, wherein the cathode is configured to be a catalyst for an oxide reduction reaction, wherein the anode is configured to be a catalyst for a hydrogen oxidation reaction.
- Claim 9Depends on #1
A fuel cell system as recited in claim 1, wherein a material of the cathode and a material of the anode include the same material.
- Claim 10Depends on #1
A fuel cell system as recited in claim 1, wherein a material of the cathode and a material of the anode include different materials.
- Claim 11Depends on #1
A fuel cell system as recited in claim 1, wherein the cathode and/or anode include at least one metal selected from the group consisting of: platinum group metals, nickel, copper, cobalt, mixed metal oxides, nickel cobalt alloys, and a combination thereof.
- Claim 12Depends on #1
A fuel cell system as recited in claim 1, wherein the cathode and/or anode includes an electrode material selected from the group consisting of: metal mesh, carbon material, metal particles, and a combination thereof.
- Claim 13Depends on #1
A fuel cell system as recited in claim 1, wherein the molten electrolyte mixture is configured to generate ionic conductivity greater than 0.50 siemens per centimeter at temperatures greater than 150 degrees Celsius.
- Claim 14Depends on #1
A fuel cell system as recited in claim 1, comprising a triple phase boundary region, wherein the triple phase boundary region includes an association of the cathode and/or anode, the molten electrolyte mixture, and a gas.
- Claim 15Depends on #14
A fuel cell system as recited in claim 14, wherein the gas is selected from the group consisting of: hydrogen gas, oxygen gas, and air.
- Claim 16Depends on #1
A fuel cell system as recited in claim 1, wherein the ceramic support has physical characteristics of formation by an additive manufacturing technique.
- Claim 17Depends on #1
A fuel system as recited in claim 1, wherein the porous ceramic support comprises pores having an average diameter sufficient to retain liquid by capillary action.
- Claim 18Depends on #1
A fuel system as recited in claim 1, wherein the porous ceramic support comprises pores having an average diameter in a range of 50 nanometers to about 10 microns.
- Claim 19Depends on #1
A fuel system as recited in claim 1, wherein the porous ceramic support comprises pores having an average diameter in a range of 50 nm to about 500 nm.
- Claim 20Depends on #1
A fuel cell system as recited in claim 1, wherein the porous ceramic support comprises pores configured to retain liquid by capillary action during exposure of the support to temperatures at about 400 degrees Celsius for greater than 100 hours.
- Claim 21Independent Claim
A fuel cell system, comprising: a cathode and an anode; a porous ceramic support positioned between the cathode and anode; a molten electrolyte mixture in pores of the ceramic support; a power source for applying a voltage differential across the cathode and the anode; and a water flow system on an outer side of the anode, wherein the outer side of the anode is opposite an inner side of the anode, wherein the inner side of the anode is adjacent to the ceramic support, wherein the water flow system is configured to sweep steam across the outer side of the anode, wherein the fuel cell system is configured to synthesize ammonia from water and nitrogen gas.
- Claim 22Independent Claim
A fuel cell system, comprising: a cathode and an anode; a porous ceramic support positioned between the cathode and anode; a molten electrolyte mixture in pores of the ceramic support; and a water flow system on an outer side of the anode, wherein the outer side of the anode is opposite an inner side of the anode, wherein the inner side of the anode is adjacent to the ceramic support, wherein the water flow system is configured to sweep steam across the outer side of the anode.
- Claim 23Depends on #22
A method for producing energy from the fuel cell system of claim 22, the method comprising: directing a gas stream through the cathode; sweeping an outer side of the anode with water; and collecting energy from the anode.
Technical Overview & Description
The United States Government has rights in this invention pursuant to Contract No. DE-AC52-07NA27344 between the United States Department of Energy and Lawrence Livermore National Security, LLC for the operation of Lawrence Livermore National Laboratory. FIELD OF THE INVENTION The present invention relates to anion exchange fuel cells, and more particularly, this invention relates to molten hydroxide dual-phase membranes for carbonate management and energy production using intermediate temperature fuel cells. BACKGROUND A typical fuel cell has an ion conductive membrane that is impermeable to gas. In addition, fuel cells, having two electrodes that are separated by the membrane, transport ions from one electrode to the other and consume hydrogen and oxygen to produce water, heat, and electricity. The membrane composition (e.g. proton exchange membrane (PEM), anion exchange membrane (AEM), dual phase membrane, etc.) of the fuel cell determines the species that are transported across the membrane (PEM moves protons, AEM moves anions such as typically hydroxide ions OH − ), the kind of catalysts used, the temperature range of operation, etc. Alkaline Fuel Cells (AFCs) were one of the first fuel cell technologies developed and in conventional applications use a membrane that includes a solution of aqueous potassium hydroxide (KOH) as the electrolyte supported in porous medium, such as asbestos. Early uses of the AFC systems by NASA generated electricity at nearly 70% efficiency using aqueous solution of KOH. AFC systems have evolved to include a hydroxide conducting polymer membrane, namely anion exchange membrane (AEM), to replace the aqueous hydroxide solution; however, these systems are costly and operate at a low hydroxide conductivity. Moreover, conventional AEM fuel cells having dense and gas impermeable membrane saturated with aqueous alkaline hydroxide solution have several challenges. Conventional AEM fuel cells tend to rely on a feed of pure oxygen rather than
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (13)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (10)
- Ganley,
- “
- An intermediate-temperature direct ammonia fuel cell with a molten alkaline hydroxide electrolyte
- ”
- , Journal of Power Sources, vol. 178, Issue 1, Mar. 15, 2008, pp. 44-47 (Year: 2008).
- Datasheets for Zircar products (Year: NA) (Year: NA).
- Deleebeeck, L., Hansen, K.K. Hybrid direct carbon fuel cells and their reaction mechanisms
- —
- a review. J Solid State Electrochem 18, 861-882 (2014). https://doi.org/10.1007/s10008-013-2258-1 (Year: 2013).