Modified deodorant urea-formaldehyde (UF) resin and use thereof, as well as particleboard and preparation method thereof
Abstract
The present disclosure provides a modified deodorant urea-formaldehyde (UF) resin and use thereof, as well as a particleboard and a preparation method thereof, and relates to the technical field of wood-based panels. Raw materials for preparing the modified deodorant UF resin provided by the present disclosure include: melamine-modified UF resin (MUF), aluminum ammonium sulfate dodecahydrate, wax, and water. Raw materials for preparing the MUF include: urea, formaldehyde, and melamine. When the modified deodorant UF resin provided by the present disclosure is used to prepare wood-based panels, the aluminum ammonium sulfate dodecahydrate losses 12 crystal water during hot pressing to form a metastable structure NH 4 Al(SO 4 ) 2 , in which NH 4 + can react with the formaldehyde to reduce formaldehyde emission, and NH 4 + and Al 3 + can absorb hydroxyl groups of organic substances to form hydrogen bonds to reduce odor of the wood-based panels.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A preparation method of a particleboard, the particleboard comprising a first surface layer, a core layer, and a second surface layer which are formed in sequence, wherein raw materials for preparing the first surface layer and the second surface layer both comprise fine shavings or particles and a modified deodorant urea-formaldehyde (UF) resin; and raw materials for preparing the core layer comprise coarse shavings or particles and the modified deodorant UF resin, and the preparation method comprising the following steps: (1) mixing the coarse shavings with the modified deodorant UF resin to obtain a coarse material for the core layer; (2) mixing the fine shavings with the modified deodorant UF resin to obtain a fine material for the two surface layers; and (3) laying the fine material for the first surface layer, the coarse material for the core layer, and the fine material for the second surface layer in sequence, and conducting hot pressing to obtain the particleboard, wherein the
- Claim 2Depends on #1
The preparation method according to claim 1, wherein the modified deodorant UF resin in the first surface layer and the second surface layer has a dosage of 20-100 kg/m 3 independently.
- Claim 3Depends on #1
The preparation method according to claim 1, wherein the fine shavings of the first surface layer and the second surface layer have a length of 0.08-5 mm independently, a width of 0.08-1.5 mm independently, a thickness of 0.08-1.5 mm independently, and a moisture content less than or equal to 14% independently.
- Claim 4Depends on #1
The preparation method according to claim 1, wherein the modified deodorant UF resin in the core layer has a dosage of 20-90 kg/m 3.
- Claim 5Depends on #1
The preparation method according to claim 1, wherein the coarse shavings have a length of 0.08-60 mm, a width of 0.08-3.5 mm, a thickness of 0.08-3.5 mm, and a moisture content less than or equal to 10%.
- Claim 6Depends on #1
The preparation method according to claim 1, wherein the hot pressing is conducted at 170-250 ° C. under 0-5 MPa with a hot pressing factor of 1-5 s/mm.
- Claim 7Depends on #1
The preparation method according to claim 1, wherein the hot pressing is continuous hot pressing, and the continuous hot pressing comprises conducting a first zone hot pressing, a second zone hot pressing, a third zone hot pressing, a fourth zone hot pressing, and a fifth zone hot pressing in sequence; the first zone hot pressing is conducted at 220-240 ° C. under 0-5 MPa with a hot pressing factor of 0-0.86 s/mm; the second zone hot pressing is conducted at 230-250 ° C. under 0-4 MPa with a hot pressing factor of 0-0.86 s/mm; the third zone hot pressing is conducted at 215-235 ° C. under 0-3 MPa with a hot pressing factor of 0-0.86 s/mm; the fourth zone hot pressing is conducted at 200-220 ° C. under 0-2 MPa with a hot pressing factor of 0-0.86 s/mm; the fifth zone hot pressing is conducted at 170-190 ° C. under 0-1.5 MPa with a hot pressing factor of 0-0.86 s/mm; and the first zone hot pressing, the second zone hot pressing, the third zone hot pressing, the fourth zone hot pressing,
- Claim 8Depends on #2
The preparation method according to claim 2, wherein the fine shavings of the first surface layer and the second surface layer have a length of 0.08-5 mm independently, a width of 0.08-1.5 mm independently, a thickness of 0.08-1.5 mm independently, and a moisture content less than or equal to 14% independently.
Technical Overview & Description
CROSS REFERENCE TO RELATED APPLICATION This patent application claims the benefit and priority of Chinese Patent Application No. 202210280123.X, filed on Mar. 21, 2022, the disclosure of which is incorporated by reference herein in its entirety as part of the present application. TECHNICAL FIELD The present disclosure relates to the technical field of wood-based panels, and in particular, to a modified deodorant urea-formaldehyde (UF) resin and use thereof, as well as a particleboard and a preparation method thereof. BACKGROUND ART A particleboard is a wood-based panel that is bonded together under the action of heat and pressure after crushed aggregates made of wood or other lignocellulosic materials are applied with an adhesive or resin. It is mainly used in furniture manufacturing, construction industry, and train and automobile carriage manufacturing. A UF resin is a commonly used particleboard adhesive. However, the particleboard prepared from the UF resin will release certain amount of irritating formaldehyde and odor, which will have certain negative impact on the environment and human body. SUMMARY In view of this, the objective of the present disclosure is to provide a modified deodorant UF resin and use thereof, as well as a particleboard and a preparation method thereof. The particleboard prepared from the modified deodorant UF resin provided by the present disclosure has a low formaldehyde emission and little odor or smell. To achieve the above objective of the present disclosure, the present disclosure provides the following technical solutions: The present disclosure provides a modified deodorant UF resin. Raw materials for preparing the modified deodorant UF resin include: melamine-modified UF resin (MUF), aluminum ammonium sulfate dodecahydrate, wax, and water. The MUF includes 45-49% of urea, 48-52% of formaldehyde, and 1-7% of melamine by mass percentage. The aluminum ammonium sulfate dodecahydrate accounts for 1-7% of the mass of the MUF. The wax
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.