hottub.patents
US 12,286,353 B2#3560501 Most CitedActiveUnited States (USPTO)Utility

Process for in-situ functionalization of graphene

0Forward Citations (#3560501 Global)
0.0/yrCitation Velocity (#3560501 Global)
0.00Citation PageRank (#3560501 Global)
80Prior Art Cited
6Structured Claims
0Drawings / Sheets

Abstract

A process for in situ functionalization of graphene including placing a graphitic precursor in an exfoliation cannister with exfoliation media; creating an inert atmosphere in the exfoliation cannister; exfoliating the graphitic precursor to form graphene having carboxyl moieties; and reacting the carboxyl moieties in the exfoliation cannister under conditions, such as a temperature of between 260 and 500 ° C., and in the presence of a substance to chemically reduce or react the carboxyl moieties during the exfoliating to produce hydrophobic graphene. Additionally, a process of molding an article including intermixing a thermoplastic in a molten state with hydrophobic graphene produced by an in situ functionalization process to form a dispersion of the hydrophobic graphene in the thermoplastic; injecting a melt of the dispersion of the hydrophobic graphene in the thermoplastic into a mold having a cavity complementary to the article; and allowing the melt to cool to form the article.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 80 · Forward citations: 0.

Claims (6)

  1. Claim 1Independent Claim

    A process for in situ functionalization of graphene comprising: placing a graphitic precursor in an exfoliation cannister with exfoliation media; creating an inert atmosphere in said exfoliation cannister; exfoliating said graphitic precursor to form graphene having carboxyl moieties; and reacting the carboxyl moieties in said exfoliation cannister under conditions and in the presence of a substance to chemically reduce or react the carboxyl moieties during the exfoliating to produce hydrophobic graphene, wherein the substance is a reagent of N-cyclohexyl-N ′ -(2-morpholinoethyl) carbodiimide (CMC).

  2. Claim 2Depends on #1

    The process of claim 1 wherein said conditions are a temperature of between 26 ° and 500 ° C.

  3. Claim 3Depends on #1

    The process of claim 1 wherein said substance further comprises an alkane, an alkene, an allyl, or a combination thereof, said substance being gaseous or liquid under standard temperature and pressure (STP).

  4. Claim 4Depends on #1

    The process of claim 1 wherein said inert atmosphere is nitrogen, argon, carbon dioxide, ethylene gas, fluorinated gases, phosphorus containing gases, or combinations thereof.

  5. Claim 5Depends on #1

    The process of claim 1 wherein said reacting the carboxyl moieties in said exfoliation cannister yields an intermediate anhydride.

  6. Claim 6Depends on #5

    The process of claim 5 further comprising reacting said intermediate anhydride with a primary amine to form an amide.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application which is a continuation of U.S. patent application Ser. No. 17/613,194, filed Nov. 22, 2021, which is a national stage application, filed under 35 U.S.C. 371, of PCT Application No. PCT/US2020/034535 filed May 26, 2020, which claims priority of U.S. Provisional Patent Application Ser. No. 62/851,774 filed May 23, 2019, which is incorporated herein by reference. TECHNICAL FIELD The present invention generally relates to graphene, and more specifically to a process for producing reduced hydrophilicity of graphene. BACKGROUND During the preparation of graphene, interlayer bonds are sheared and otherwise broken to create labile networks, both in the basal plane and edges of the graphene platelet. A variety of techniques have been developed to chemically modify graphene to add or otherwise react moieties present on graphene platelets. These prior efforts have included efforts to modify electrical properties, water solubility. Friedel-Crafts alkylation, Diels-Alder reactions by reacting hydroxyl groups or unsaturations present on the graphene or graphene oxide platelets. (C. Chua et al., Chem. Soc. Rev. 2014, 43, 291-312; A. Abdolmaleki et al., RSC Adv., 2014, 4, 60052-60057). A common feature of these techniques is that the reactions occur subsequent to synthesis and as a result, add cost and limit throughput of the resulting material. The existing process of ball milling has previously been used to functionalize graphene in situ during milling of a graphitic starting material but has meet with limited success owing to a lack of chemical control over the functional groups that are introduced. (Baek et al, J. Mater. Chem. A. 2014, 2, 8690-8695). Thus, there exists a need for a refined in situ process to remove hydrophilic moieties or react such moieties to otherwise render them less hydrophilic. There also exists a need for the resulting material as a dispersant in hydrophobic matrices. SUMMARY OF THE INVENTION The

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (10)

  • Final Office Action for U.S. Appl. No. 15/285,967, mailed May 16, 2019, 11 pages.
  • Grant Decision for Chinese Application No. 201680070947.7, mailed Jul. 2, 2020, 3 pages.
  • International Search Report and Written Opinion for Application No. PCT/US2016/055873, mailed Dec. 27, 2017, 12 pages.
  • Non-Final Office Action for U.S. Appl. No. 15/285,967, mailed Oct. 30, 2018, 9 pages.
  • Non-Final Office Action for U.S. Appl. No. 17/739,949 mailed Oct. 16, 2024, 9 pages.
  • Notice of Allowance for Korean Application No. 10-2018-7012791 mailed Jul. 31, 2024, 6 pages.
  • Notice of Allowance for U.S. Appl. No. 15/285,967, mailed Sep. 24, 2019, 13 pages.
  • Office Action for Chinese Application No. 201680070947.7, mailed Nov. 4, 2019, 25 pages.
  • Office Action for Korean Application No. KR1020187012791 dated Oct. 26, 2023, 12 pages.
  • Restriction Requirement for U.S. Appl. No. 15/285,967, mailed Jul. 27, 2018, 11 pages.