Abstract

A composition comprising the following components a)-c): a) an alpha composition comprising a multimodal ethylene/alpha-olefin interpolymer, and wherein the alpha composition comprises the following properties: i) an Mz/Mn ≥ 8.0, ii) a density from 0.855 to 0.890 g/cc, iii) a V100 (100 ° C.) ≤ 2,000 Pa · s, iv) a V1.0 (100 ° C.) ≥ 15,000 Pa · s, v) a Mn ≥ 16,000 g/mol; b) a peroxide; and c) a silane coupling agent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 38 · Forward citations: 0.

Claims (8 — 1 Independent, 7 Dependent)

  1. Claim 1Independent Claim

    A composition comprising the following components a)-c): a) an alpha composition comprising a multimodal ethylene/alpha-olefin interpolymer, and wherein the alpha composition comprises the following properties: i) an Mz/Mn ≥ 8.0, ii) a density from 0.855 to 0.890 g/cc, iii) a V100 (100 ° C.) ≤ 2,000 Pa · s, iv) a V1.0 (100 ° C.) ≥ 15,000 Pa · s, v) a Mn ≥ 16,000 g/mol; b) a peroxide; and c) a silane coupling agent.

  2. Claim 2Depends on #1

    The composition of claim 1, wherein the alpha composition has an I2 ≥ 1.0 g/10 min.

  3. Claim 3Depends on #1

    The composition of claim 1, wherein the alpha composition has an I2 ≤ 30 g/10 min.

  4. Claim 4Depends on #1

    The composition of claim 1, wherein the alpha composition has an I10/I2 ≥ 6.0.

  5. Claim 5Depends on #1

    The composition of any one of the previous claim 1, wherein the alpha composition has an I10/I2 ≤ 40.0.

  6. Claim 6Depends on #1

    The composition of any one of the previous claim 1, wherein, the alpha composition has a molecular weight distribution MWD ≥ 3.00.

  7. Claim 7Depends on #1

    The composition of claim 1, wherein, for the multimodal interpolymer, a [Mn (highest 20% mass fraction) /Mn (lowest 20% mass fraction)] ≥ 16.0.

  8. Claim 8Depends on #1

    The composition of claim 1, wherein, for the multimodal interpolymer, a [Mn (highest 20% mass fraction) /Mn (lowest 20% mass fraction] ≤ 100.0.

Technical Overview & Description

BACKGROUND OF THE INVENTION Materials designed for photovoltaic encapsulants must satisfy many requirements. In order to prevent movement of electrical components and wiring, within a photovoltaic module, polymeric encapsulating materials must not flow significantly at temperatures up to 85 ° C. One way to accomplish this, is to use a semicrystalline polymer with a melting point above this temperature. However, other encapsulating material requirements, such as high optical clarity and low modulus, are optimized with low-crystallinity polymers. To balance these requirements, typically a low-crystallinity polymer, such as an ethylene-vinyl acetate copolymer (EVA) or a polyolefin elastomer (POE), such as an ENGAGE Polyolefin Elastomer, is used in conjunction with a peroxide-based reactive curing formulation. The low crystallinity polymer provides high clarity and low modulus, while the curing formulation facilitates a crosslinking reaction, which causes the polymer to form a network, providing mechanical stability at high temperatures. This crosslinking reaction takes place during module lamination, typically conducted at 150 ° C. If a peroxide curing formulation is used, the film extrusion process must be conducted at a low temperature, in order to prevent the peroxide from decomposing and initiating the crosslinking reaction in the extruder. Heat generated during extrusion is related to the rate of extrusion and the polymer viscosity; high viscosity and high extrusion rates generate more heat. Therefore, to extrude a “ peroxide-curing ” encapsulant film, a low viscosity resin, extruded at low rates, is preferred. However, low extrusion rates are economically disadvantageous, and low viscosity is typically achieved via the use of a low molecular weight resin. Low molecular weight resins cannot be crosslinked efficiently, and require a higher loading of the peroxide curing formulation, or longer times in the module lamination process, in order to reach the necessary l

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (38)

Non-Patent Literature (1)

  • PCT/CN2019/128576, International Search Report and Written Opinion with a mailing date of Aug. 31, 2020.