hottub.patents
US 12,269,059 B2#3575346 Most CitedActiveUnited States (USPTO)Utility

Silicone compositions and methods related thereto

0Forward Citations (#3575346 Global)
0.0/yrCitation Velocity (#3575346 Global)
0.00Citation PageRank (#3575346 Global)
20Prior Art Cited
21Claims (1 Indep. · 20 Dep.)
6Drawings / Sheets

Abstract

A composition is described herein that includes a polysiloxane, a silicon based crosslinker, a reinforcement filler, a vulcanization catalyst, and a repair-enabling filler. Methods of using such a composition are also described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 0.

Claims (21 — 1 Independent, 20 Dependent)

  1. Claim 1Independent Claim

    A composition comprising: a) 100 parts by weight of a polysiloxane; b) from 2 to 40 parts by weight of a silicon based crosslinker; c) from 5 to 26 parts by weight of a reinforcing filler; d) from 0.01 to 5 parts by weight of a vulcanization catalyst; e) from 60 to 130 parts by weight of a repair-enabling filler, wherein the repair-enabling filler comprises particles having an average particle size from about 100 nm to 250 μ m; and f) a solvent, wherein the repair-enabling filler is present from about 60 to about 130 parts by weight with respect to the polysiloxane, such that a cured coating from the composition maintains flexibility to the extent that it is able to elongate a minimum of 40% without being permanently damaged, wherein the cured coating from the composition having the flexibility to the extent that it is able to elongate a minimum of 40% without being permanently damaged is sandable as determined following the procedure in ASTM D-3322 section 6.17.

  2. Claim 2Depends on #1

    The composition of claim 1, wherein the polysiloxane is a hydroxyl endblocked polydiorganosiloxane having a viscosity from 1000 to 250,000 cP at 25 ° C. and having one or more different organic radicals selected from the group consisting of methyl, ethyl, phenyl, and 3,3,3-trifluoropropyl.

  3. Claim 3Depends on #1

    The composition of claim 1, wherein the silicon based crosslinker is an alkoxysilicon compound.

  4. Claim 4Depends on #1

    The composition of claim 1, wherein the silicon based crosslinker is an acetoxysilicon compound.

  5. Claim 5Depends on #1

    The composition of claim 1, wherein the silicon based crosslinker is a ketoximosilicon compound.

  6. Claim 6Depends on #1

    The composition of claim 1, wherein the polysiloxane is a fluorosilicone.

  7. Claim 7Depends on #1

    The composition of claim 1, wherein the polysiloxane is a phenylsilicone.

  8. Claim 8Depends on #1

    The composition of claim 1, wherein the polysiloxane is a methylsilicone.

  9. Claim 9Depends on #1

    The composition of claim 1, wherein the vulcanization catalyst is a metal salt of carboxylic acids.

  10. Claim 10Depends on #1

    The composition of claim 1, wherein the repair-enabling filler comprises one or more materials selected from the group consisting of quartz, titania, and fused silica, or a combination thereof.

  11. Claim 11Depends on #1

    The composition of claim 1, wherein the repair-enabling filler is homogenously dispersed in the composition.

  12. Claim 12Depends on #1

    The composition of claim 1, wherein the composition further comprises one or more additives selected from the group consisting of a colorant, an electrically conductive material, a thermally conductive material, an UV absorber, an adhesion promoter, or a matting agent, or a combination thereof.

  13. Claim 13Depends on #1

    The composition of claim 1, wherein the composition is a film having a thickness from about 5 μ m to about 1300 μ m.

  14. Claim 14Depends on #1

    The composition of claim 1, wherein: a) the polysiloxane is a linear polysiloxane with 100 mol % of the backbone consisting of trifluoropropylmethylsiloxy units; b) the silicon based crosslinker is a mixture of ethyltriacetoxysilane and methyltriacetoxysilane; c) the reinforcing filler is fumed silica; d) the vulcanization catalyst is dibutyltin diacetate; and e) the repair-enabling filler is crushed quartz.

  15. Claim 15Depends on #1

    The composition of claim 1, wherein: a) the polysiloxane is a linear polysiloxane with the back bone consisting of a mixture dimethylsiloxy and diphenylsiloxy; b) the silicon based crosslinker is methyltris(methylethylketoximo) silane; c) the reinforcing filler is fumed silica; d) the vulcanization catalyst is dibutyltin diacetate; and e) the repair-enabling filler is crushed quartz.

  16. Claim 16Depends on #1

    A method comprising the steps of: a) removing a portion of an area of a cured coating that is present on a substrate, thereby exposing a portion of an area of the substrate that corresponds to the area of the removed portion of the cured coating, which exposed portion of the substrate borders cured coating that was not removed; b) smoothing the cured coating that borders the exposed area of the substrate; c) applying the composition of claim 1 to the exposed area of the substrate; d) curing the applied composition from step c); and e) removing any excess of the cured applied composition, thereby repairing the cured coating on the substrate.

  17. Claim 17Depends on #16

    The method of claim 16, wherein removing the portion of the area of the cured coating removes a defect in the cured coating.

  18. Claim 18Depends on #17

    The method of claim 17, wherein the defect comprises a delamination, a tear, a scuff, a void in the cured coating, bubbling, or a score in the cured coating.

  19. Claim 19Depends on #16

    The method of claim 16, wherein the cured coating has a thickness from about 5 μ m to about 1300 μ m.

  20. Claim 20Depends on #16

    The method of claim 16, wherein removing the portion of the area of the cured coating and smoothing the cured coating that borders the exposed area of the substrate comprises sanding.

  21. Claim 21Depends on #16

    The method of claim 16, wherein the substrate is selected from the group consisting of a metal substrate, a plastic substrate, and a silicone substrate, or a combination thereof.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of U.S. Provisional Application No. 62/926,368 filed Oct. 25, 2019, which is incorporated herein by reference in its entirety. FIELD OF INVENTION This disclosure relates to a composition that is suitable to be repaired when in the form of a coating, and methods for making, repairing, and using such a coating composition. BACKGROUND A coating is defined as a layer of material that is intended to protect a substrate underneath from the external environment. Thus, the coating protects the substrate from UV exposure, chemical exposure, physical impact, and temperature swings among other environmental events. The coatings are useful in a broad range of applications, such as coatings used in aerospace and defense industries (e.g. terrestrial and extra-terrestrial vehicles) to impart protective and functional properties. At times the coatings can get damaged, such as a scuff, gouge, or small removal of material. It is desirable to repair the damaged coatings. This is most commonly done by sanding and reapplying a coating to a uniform thickness and homogeneity while preserving the desired properties. There is a need for compositions that can be used as repairable coatings. There is also a need for methods related to the compositions that can be used as repairable coatings. Such a composition and methods related thereto are disclosed herein. SUMMARY OF THE INVENTION Disclosed herein is a composition comprising: a) 100 parts by weight of a polysiloxane; b) from 2 to 40 parts by weight of a silicon based crosslinker; c) from 1 to 40 parts by weight of a reinforcing filler; d) from 0.01 to 5 parts by weight of a vulcanization catalyst; and e) from 30 to 130 parts by weight of a repair-enabling filler. Also disclosed herein is a method comprising the steps of: a) removing an area of a cured coating that is present on a substrate, thereby exposing the substrate; b) smoothing the cured coating that borders

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 4,034,140 AHeat-curable silicone elastomers having unprimed adhesion197727
US 4,102,852 ASelf-extinguishing room temperature vulcanizable silicone rubber compositions197818
US 4,405,425 AFlame-retardant polysiloxane elastomers198322
US 5,789,084 ALiquid silicone rubber coating composition1998102
US 5,928,778 ADecorative material having abrasion resistance199970
US 6,171,704 B1Coating for aerospace aluminum parts200135
US 6,316,119 B1Multi-component composite coating composition and coated substrate200147
US 6,699,586 B2Organosilicon nano/microhybrid or microhybrid system composition for scratch and abrasion resistant coatings200443
US 6,830,816 B2Highly filled, pasty, composition containing silicoorganic nanohybrid and/or microhybrid capsules for scratch-resistant and/or abrasion-resistant coatings200438
US 7,250,467 B2Room-temperature-curable organopolysiloxane composition20078
US 7,588,797 B2Field repairable high temperature smooth wear coating200911
US 9,512,342 B1Moisture cured polymer and recycled glass roof coating, caulk/sealant and patching compound membranes201617
US 9,546,300 B2Coating composition for coated substrates and methods of making the same20172
US 10,604,660 B2Wear resistant coating, article, and method20202
KR 20060099332 AManufacturing method of high- capacity non-zero dispersion shifted fiber—0
KR 20150140345 AEmbossed polymer sheet—7
CN 105,754,477 APaint protective coating and preparation method thereof—3
CN 107,779,015 BPhotovoltaic backboard repairing paint, repairing method using same and application20200

Non-Patent Literature (4)

  • International Search Report and Written Opinion for PCT Application No. PCT/US2020/056994, filed Oct. 23, 2020, mailed on Jan. 25, 2021 (8 pages).
  • International Preliminary Report on Patentability was issued on Apr. 26, 2022 by the International Searching Authority for International Application No. PCT/US2020/056994 filed on Oct. 23, 2020 and published as WO2021/081287 (Applicant
  • —
  • Nusil Technology) (5 pages).