Silicon precursor compounds and method for forming silicon-containing films
Abstract
Provided are certain silicon precursor compounds which are useful in the formation of silicon-containing films in the manufacture of semiconductor devices, and more specifically to compositions and methods for forming such silicon-containing films, such as films comprising silicon dioxide or silicon nitride.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A method for forming a silicon-containing film on the surface of a microelectronic device, which comprises introducing at least one compound of Formula (I): wherein each R 1 is independently chosen from hydrogen or C 1 -C 4 alkyl, and each R 2 is independently chosen from chloro, bromo, iodo, hydrogen, or C 1 -C 4 alkyl, provided that no fewer than two of R 2 is chosen from chloro, bromo, or iodo, to said surface in a reaction chamber, under atomic layer deposition conditions at a temperature of greater than 600 ° C., the atomic layer deposition conditions are non-plasma conditions, the silicon-containing film is free of halides, the silicon-containing film is a silicon nitride film with about 9% to about 13% carbon with a silicon to nitrogen ratio of about 1:1, and wherein the compound of Formula (I) has a purity of greater than 98%.
- Claim 2Depends on #1
The method of claim 1, wherein the atomic layer deposition conditions are at a temperature of greater than 600 ° C. to about 900 ° C.
- Claim 3Depends on #1
The method of claim 1, wherein the atomic layer deposition conditions are at a temperature of about 625 ° C. to about 725 ° C.
- Claim 4Depends on #1
The method of claim 1, wherein the silicon-containing film has a thickness of from about 100 Å to about 1000 Å.
- Claim 5Depends on #1
The method of claim 1, wherein the silicon-containing film has a thickness of from about 200 Å to about 500 Å.
- Claim 6Depends on #1
The method of claim 1, wherein the surface is chosen from silicon dioxide, silicon nitride, aluminum oxide, aluminum nitride, aluminum, tungsten, copper, cobalt, molybdenum, ruthenium, a silicon wafer, or combinations thereof.
- Claim 7Depends on #1
The method of claim 1, wherein the compound of Formula (I) has the formula:
- Claim 8Independent Claim
A method for forming a silicon-containing film on the surface of a microelectronic device, which comprises introducing at least one compound of Formula (I): wherein each R 1 is independently chosen from hydrogen or C 1 -C 4 alkyl, and each R 2 is independently chosen from chloro, bromo, iodo, hydrogen, or C 1 -C 4 alkyl, provided that no fewer than two of R 2 is chosen from chloro, bromo, or iodo, to said surface in a reaction chamber, under thermal atomic layer deposition conditions at a temperature of greater than 400 ° C., wherein the thermal atomic layer deposition conditions are non-plasma conditions, the silicon-containing film is free of halides, the silicon-containing film is a silicon nitride film with about 9% to about 13% carbon and a silicon to nitrogen ratio of about 1:1, and wherein the compound of Formula (I) has a purity of greater than 98%.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit under the provisions of 35 U.S.C. § 119 of U.S. Provisional Patent Application No. 63/042,769, filed Jun. 23, 2020, and U.S. Provisional Patent Application No. 63/081,711, filed Sep. 22, 2020, the entirety of which are incorporated herein by reference. FIELD OF THE INVENTION In general, the invention relates to methods and precursors for the deposition of silicon-containing films onto microelectronic device surfaces. BACKGROUND OF THE INVENTION In semiconductor manufacturing, thin (e.g., < 1000 nanometers thickness) passive layers of chemically inert dielectric materials, such as silicon nitride (Si 3 N 4 ), silicon oxynitride (SiO x N y ), silicon carbide (SiC), silicon carbon nitride (SiCN) and silicon carbo oxide (SiCO) and/or silicon dioxide (SiO 2 ) are widely employed in microelectronic device structures, to function as structural elements of the multi-layered device such as sidewall spacer elements, diffusion masks, oxidation barriers, trench isolation coatings, inter-metallic dielectric materials, passivation layers, insulators and etch-stop layers. Deposition of silicon-containing films by chemical vapor deposition techniques is a highly attractive methodology for forming such films. CVD processes involving low deposition temperatures are particularly desired, e.g., temperatures less than about 450 ° C., but require the availability of suitable silicon precursor compounds for such purpose. In some cases, higher deposition temperatures can be considered, when the thermal budget of the integrated circuit will allow. In these cases, temperatures > 450 ° C. might be utilized to achieve the desired dielectric film. Accordingly, a need exists for precursors for the formation of silicon-containing films which can be utilized at such higher temperatures. In particular, there is a need for liquid silicon precursors with good thermal stability, high volatility, and reactivity with a substrate
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (16)
| Patent | Title | Year | Citations |
|---|