Thermocompression bonding with passivated copper-based contacting metal
Abstract
Methods and systems for low-force, low-temperature thermocompression bonding. The present application teaches new methods and structures for three-dimensional integrated circuits, in which cold thermocompression bonding is used to provide reliable bonding. To achieve this, reduction and passivation steps are preferably both used to reduce native oxide on the contact metals and to prevent reformation of native oxide, preferably using atmospheric plasma treatments. Preferably the physical compression height of the elements is set to be only enough to reliably achieve at least some compression of each bonding element pair, compensating for any lack of flatness. Preferably the thermocompression bonding is performed well below the melting point. This not only avoids the deformation of lower levels which is induced by reflow techniques, but also provides a steep relation of force versus z-axis travel, so that a drastically-increasing resistance to compression helps to regulate the degree of thermocompression.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.
Claims (11 — 3 Independent, 8 Dependent)
- Claim 1Independent Claim
A method for bonding microelectronic elements, comprising the steps of: a) using plasma-activated radical-enriched gas flow at substantially ambient atmospheric conditions: to reduce native oxides from the surfaces of first copper-based contacting metallizations on a first side of a first element; and to passivate the surfaces of said first copper-based contact metallizations against re-oxidation; b) using plasma-activated radical-enriched gas flow at substantially ambient atmospheric conditions: to reduce native oxides from the surfaces of second copper-based contacting metallizations on a second element; and to passivate the surfaces of said second copper-based contacting metallizations against re-oxidation; c) compressing said first and second copper-based contacting metallizations together, without any conductive liquid phase material, to thereby bond said second element to said first element; d) repeating said step c), using additional elements which have been subjected to step a) to bond copper-based contacting metallizations on the additional elements to copper-based contacting metallizations on an unbonded side of a previously bonded element; and wherein said compressing step compresses said copper-based contacting metallizations by no more than 40% of the initial heights of said copper-based contacting metallizations.
- Claim 2Independent Claim
A method for bonding microelectronic elements, comprising the steps of: a) using plasma-activated radical-enriched gas flow at substantially ambient atmospheric conditions: to reduce native oxides from the surfaces of first copper-based contacting metallizations on a first side of a first element; and to passivate the surfaces of said first copper-based contact metallizations against re-oxidation; b) using plasma-activated radical-enriched gas flow at substantially ambient atmospheric conditions: to reduce native oxides from the surfaces of second copper-based contacting metallizations on a second element; and to passivate the surfaces of said second copper-based contacting metallizations against re-oxidation; c) compressing said first and second copper-based contacting metallizations together, without any conductive liquid phase material, to thereby bond said second element to said first element; d) repeating said step c), using additional elements which have been subjected to step a) to bond copper-based contacting metallizations on the additional elements to copper-based contacting metallizations on an unbonded side of a previously bonded element; wherein said copper-based contacting metallizations are composed of pure copper; and wherein said compressing step compresses said copper-based contacting metallizations by no more than 40% of the initial heights of said copper-based contacting metallizations.
- Claim 3Independent Claim
A method for bonding microelectronic elements, comprising the steps of: a) using plasma-activated radical-enriched gas flow at substantially ambient atmospheric conditions: to reduce native oxides from the surfaces of first copper-based contacting metallizations on a first side of a first element; and to passivate the surfaces of said first copper-based contact metallizations against re-oxidation; b) using plasma-activated radical-enriched gas flow at substantially ambient atmospheric conditions: to reduce native oxides from the surfaces of second copper-based contacting metallizations on a second element; and to passivate the surfaces of said second copper-based contacting metallizations against re-oxidation; c) compressing said first and second copper-based contacting metallizations together, without any conductive liquid phase material, to thereby bond said second element to said first element; d) repeating said step c), using additional elements which have been subjected to step a) to bond copper-based contacting metallizations on the additional elements to copper-based contacting metallizations on an unbonded side of a previously bonded element; wherein said reducing of native oxides is performed in a reduction-only atmosphere; and wherein said compressing step compresses said copper-based contacting metallizations by no more than 40% of the initial heights of said copper-based contacting metallizations.
- Claim 4Depends on #1
The method of claim 1, further comprising bonding an additional element to either the first or the second element, wherein only one side of said additional element has copper-based contacting metallizations.
- Claim 5Depends on #1
The method of claim 1, wherein said compressing step is performed at a temperature of approximately 300 ° C.
- Claim 6Depends on #1
The method of claim 1, wherein said second element has copper-based contacting metallizations both on a first side and also on a second side.
- Claim 7Depends on #1
The method of claim 1, wherein said copper-based contacting metallizations are copper-based contacting metallization bumps.
- Claim 8Depends on #1
The method of claim 1, wherein said copper-based contacting metallizations are copper-based contacting metallization pads.
- Claim 9Depends on #1
The method of claim 1, wherein said copper-based contacting metallizations are copper-based contacting metallization pillars.
- Claim 10Depends on #1
The method of claim 1, wherein said compressing step compresses said copper-based contacting metallizations by no more than 30% of the initial heights of said copper-based contacting metallizations.
- Claim 11Depends on #1
The method of claim 1, further comprising heating said elements during said compressing step.
Technical Overview & Description
CROSS-REFERENCE Priority is claimed from 61/604,162 filed Mar. 4, 2012, which is hereby incorporated by reference. The present application is a continuation-in-part of Ser. No. 12/837,751 filed Jul. 16, 2010, which is hereby incorporated by reference. BACKGROUND The present application relates to 3D interconnect bonding of multiple chips, and more particularly to reliable 3D interconnect bonding of multiple chips without solder reflow. Note that the points discussed below may reflect the hindsight gained from the disclosed inventions, and are not necessarily admitted to be prior art. Metallic contact flip-chip interconnect bonding techniques are currently under development in the semiconductor integration and packaging industry to enable vertical stacking of multiple dice with high density interconnects between each subsequent die in the vertical stack. This is referred to in the semiconductor industry as “ 3D Packaging ” or “ 3DIC ” . Conventional “ flip-chip ” reflow solder bonding techniques are currently being used to align and then fuse solder connections between facing chips by melting solder bumps to form an electrical and mechanical connection between the chips. This has been accomplished in commercial production for many years in the mounting of single chips to circuit boards and in the bonding of two facing chips to each other. The present application teaches that a problem arises, however, when a third or subsequent chip is to be added vertically or horizontally to an already reflowed chip assembly. When the additional solder connections are reflowed (melted), the original solder connections are also melted, leaving the whole stack susceptible to loss of original alignment, parallelism, and contact. This problem is compounded further if multiple stacked-chip groups are to be assembled, one at a time, onto a single substrate. In this case, each previous stack is also subjected to the same de-stabilizing effects of re-melting the previously-made solder conn
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (12)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (5)
- Chen et al. ,
- “
- Wafer-level bonding/stacking technology for 3D integration
- ”
- , Microelectronics Reliability, vol. 50, p. 481-488, 2009 (Year: 2009).