Polypyrrole-graphene/polyurethane antifouling coating as well as preparation method and application thereof
Abstract
A polypyrrole-graphene/polyurethane antifouling coating as well as a preparation method and an application thereof are provided. The polypyrrole-graphene/polyurethane antifouling coating includes component A and component B, wherein the component A mainly includes the following raw materials in parts by weight: 500 parts of group-hydrolyzable polyurethane prepolymer, 25-50 parts of bentonite, 25-50 parts of titanium dioxide, 60-120 parts of zinc oxide, 15-30 parts of talcum powder, and 15-30 parts of polypyrrole-graphene nanofiller; and the component B mainly includes the following raw materials in parts by weight: 5-7 parts of leveling agent, 5-7 parts of defoamer, 6-15 parts of chain extender, 10-25 parts of silane coupling agent, and 1-2 parts of catalyst. The two-component polyurethane coating of the present invention has relatively good adhesion, collision resistance and cracking resistance, and the antifouling property and the antifouling durability can be improved.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 0.
Claims (14 — 2 Independent, 12 Dependent)
- Claim 1Independent Claim
A polypyrrole-graphene/polyurethane antifouling coating, comprising a first component and a second component, wherein the first component comprises the following raw materials in parts by weight: 500 parts of a group-hydrolyzable polyurethane prepolymer, 25 parts-50 parts of bentonite, 25 parts-50 parts of titanium dioxide, 60 parts-120 parts of zinc oxide, 15 parts-30 parts of a talcum powder, and 15 parts-30 parts of a polypyrrole-graphene nanofiller, wherein the group-hydrolyzable polyurethane prepolymer is grafted with pyridine-triphenylborane; and the second component comprises the following raw materials in parts by weight: 5 parts-7 parts of a leveling agent, 5 parts-7 parts of a defoamer, 6 parts-15 parts of a chain extender, 10 parts-25 parts of a silane coupling agent, and 1 part-2 parts of a catalyst.
- Claim 2Depends on #1
The polypyrrole-graphene/polyurethane antifouling coating of claim 1, wherein the group-hydrolyzable polyurethane prepolymer is prepared by the following method: adding xylene and tetrahydrofuran to a four-necked flask with a mechanical stirring device, a thermometer, a constant-pressure dropping funnel, and a condenser pipe, and adding a carboxyl-containing diol to obtain a system, heating the system to 50 ° C.-60 ° C. and dripping isophorone diisocyanate (IPDI) into the system to obtain a first mixed system, mixing the first mixed system and heating the first mixed system to a temperature of 80 ° C.-85 ° C., and maintaining the temperature for 0.5 h-1 h after the first mixed system reaches to a clarified status; cooling the first mixed system to 50 ° C.-60 ° C., adding dehydrated polyether polyol to the first mixed system to obtain a second mixed system, mixing the second mixed system and heating the second mixed system to 80-85 ° C., and keeping a first reaction for 1.5 h-2.5 h; when a viscosity of the second mixed system increases and a — NCO content decreases to 0.5%, cooling the second mixed system to 50 ° C.-60 ° C., dripping the IPDI to the second mixed system to obtain a third mixed system, mixing the third mixed system and heating the third mixed system to 80 ° C.-85 ° C., and keeping a second reaction for 2 h-3 h; adding the pyridine-triphenylborane (PTPB) in first batches to the third mixed system to obtain a fourth mixed system, keeping a reaction temperature at 70 ° C.-85 ° C., adding a second batch of the PTPB after a third reaction is completed and the fourth mixed system becomes clear from turbid, and keeping a fourth reaction for 1 h-2.5 h; dripping polyisocyanate after final feeding is completed, and keeping the temperature at 80 ° C.-85 ° C. for 2 h-3 h until a fifth reaction is completed.
- Claim 3Depends on #1
The polypyrrole-graphene/polyurethane antifouling coating of claim 1, wherein the polypyrrole-graphene nanofiller is prepared by the following method: dispersing ammonium persulfate and cetyl trimethyl ammonium bromide in a hydrochloric acid solution at a molar ratio of (2.5-4):1 to obtain a first resulting solution, ultrasonically dispersing a graphene in the first resulting solution to obtain a second resulting solution, dripping a pyrrole monomer under stirring to the second resulting solution to obtain a third resulting solution, wherein a mass ratio of the graphene to the pyrrole monomer is 1/50-1/200, and the third resulting solution changes from milky white to black blue and eventually to black; upon completion, filtrating the third resulting solution, washing filter cakes with distilled water and ethanol, and performing a vacuum drying to obtain the polypyrrole-graphene nanofiller.
- Claim 4Depends on #1
The polypyrrole-graphene/polyurethane antifouling coating of claim 1, wherein in use, the first component and the second component are mixed at a mass ratio of (30-45):1, heated and cured.
- Claim 5Depends on #1
The polypyrrole-graphene/polyurethane antifouling coating of claim 1, wherein the silane coupling agent is at least one of γ -aminopropyl triethoxysilane, γ -aminopropyl trimethoxy silane, bis-(γ -trimethoxysilylpropyl)amine, N-phenyl- γ -aminopropyl trimethoxy silane, N-phenyl- γ -aminopropyl triethoxysilane, N-butyl- γ -aminopropyl trimethoxy silane, and N-butyl- γ -aminopropyl triethoxysilane.
- Claim 6Depends on #1
The polypyrrole-graphene/polyurethane antifouling coating of claim 1, wherein the chain extender is a liquid amine chain extender.
- Claim 7Depends on #1
The polypyrrole-graphene/polyurethane antifouling coating of claim 1, wherein the catalyst is at least one of dibutyltin dilaurate and dibutyltin diacetate.
- Claim 8Independent Claim
A method for preparing polypyrrole-graphene/polyurethane antifouling coating, wherein the polypyrrole-graphene/polyurethane antifouling coating, comprise a first component and a second component, wherein the first component comprises the following raw materials in parts by weight: 500 parts of a group-hydrolyzable polyurethane prepolymer, 25 parts-50 parts of bentonite, 25 parts-50 parts of titanium dioxide, 60 parts-120 parts of zinc oxide, 15 parts-30 parts of a talcum powder, and 15 parts-30 parts of a polypyrrole-graphene nanofiller, wherein the group-hydrolyzable polyurethane prepolymer is grafted with pyridine-triphenylborane; and the second component comprises the following raw materials in parts by weight: 5 parts-7 parts of a leveling agent, 5 parts-7 parts of a defoamer, 6 parts-15 parts of a chain extender, 10 parts-25 parts of a silane coupling agent, and 1 part-2 parts of a catalyst, the method comprising the following steps: S1, adding the raw materials of the first component to a high-speed dispersion machine, and performing a first high-speed dispersion for 15 min-45 min to prepare the first component; and S2, adding the raw materials of the second component to the high-speed dispersion machine, and performing a second high-speed dispersion for 15 min-30 min to prepare the second component.
- Claim 9Depends on #8
The method for preparing the polypyrrole-graphene/polyurethane antifouling coating of claim 8, wherein the group-hydrolyzable polyurethane prepolymer is prepared by the following method: adding xylene and tetrahydrofuran to a four-necked flask with a mechanical stirring device, a thermometer, a constant-pressure dropping funnel, and a condenser pipe, and adding a carboxyl-containing diol to obtain a system, heating the system to 50 ° C.-60 ° C. and dripping isophorone diisocyanate (IPDI) into the system to obtain a first mixed system, mixing the first mixed system and heating the first mixed system to a temperature of 80 ° C.-85 ° C., and maintaining the temperature for 0.5 h-1 h after the first mixed system reaches to a clarified status; cooling the first mixed system to 50 ° C.-60 ° C., adding dehydrated polyether polyol to the first mixed system to obtain a second mixed system, mixing the second mixed system and heating the second mixed system to 80-85 ° C., and keeping a first reaction for 1.5 h-2.5 h; when a viscosity of the second mixed system increases and a — NCO content decreases to 0.5%, cooling the second mixed system to 50 ° C.-60 ° C., dripping the IPDI to the second mixed system to obtain a third mixed system, mixing the third mixed system and heating the third mixed system to 80 ° C.-85 ° C., and keeping a second reaction for 2 h-3 h; adding the pyridine-triphenylborane (PTPB) in first batches to the third mixed system to obtain a fourth mixed system, keeping a reaction temperature at 70 ° C.-85 ° C., adding a second batch of the PTPB after a third reaction is completed and the fourth mixed system becomes clear from turbid, and keeping a fourth reaction for 1 h-2.5 h; dripping polyisocyanate after final feeding is completed, and keeping the temperature at 80 ° C.-85 ° C. for 2 h-3 h until a fifth reaction is completed.
- Claim 10Depends on #8
The method for preparing the polypyrrole-graphene/polyurethane antifouling coating of claim 8, wherein the polypyrrole-graphene nanofiller is prepared by the following method: dispersing ammonium persulfate and cetyl trimethyl ammonium bromide in a hydrochloric acid solution at a molar ratio of (2.5-4):1 to obtain a first resulting solution, ultrasonically dispersing a graphene in the first resulting solution to obtain a second resulting solution, dripping a pyrrole monomer under stirring to the second resulting solution to obtain a third resulting solution, wherein a mass ratio of the graphene to the pyrrole monomer is 1/50-1/200, and the third resulting solution changes from milky white to black blue and eventually to black; upon completion, filtrating the third resulting solution, washing filter cakes with distilled water and ethanol, and performing a vacuum drying to obtain the polypyrrole-graphene nanofiller.
- Claim 11Depends on #8
The method for preparing the polypyrrole-graphene/polyurethane antifouling coating of claim 8, wherein in use, the first component and the second component are mixed at a mass ratio of (30-45):1, heated and cured.
- Claim 12Depends on #8
The method for preparing the polypyrrole-graphene/polyurethane antifouling coating of claim 8, wherein the silane coupling agent is at least one of γ -aminopropyl triethoxysilane, γ -aminopropyl trimethoxy silane, bis-(γ -trimethoxysilylpropyl)amine, N-phenyl- γ -aminopropyl trimethoxy silane, N-phenyl- γ -aminopropyl triethoxysilane, N-butyl- γ -aminopropyl trimethoxy silane, and N-butyl- γ -aminopropyl triethoxysilane.
- Claim 13Depends on #8
The method for preparing the polypyrrole-graphene/polyurethane antifouling coating of claim 8, wherein the chain extender is a liquid amine chain extender.
- Claim 14Depends on #8
The method for preparing the polypyrrole-graphene/polyurethane antifouling coating of claim 8, wherein the catalyst is at least one of dibutyltin dilaurate and dibutyltin diacetate.
Technical Overview & Description
CROSS REFERENCE TO THE RELATED APPLICATIONS This application is based upon and claims priority to Chinese Patent Application No. 202111248332.8, filed on Oct. 26, 2021, the entire contents of which are incorporated herein by reference. TECHNICAL FIELD The present invention relates to the technical field of antifouling coating, in particular to a polypyrrole-graphene/polyurethane antifouling coating and a preparation method thereof. BACKGROUND An ocean buoy is a kind of navigation mark floating on the water surface. It can measure the wind, pressure, temperature, humidity, visibility in the atmosphere, as well as the wave, current, water temperature, salinity and other parameters in the hydrological parameters. However, as the ocean buoy fluctuates with the waves for a long time and is affected by the light, marine organisms rapidly proliferate on its surface and become sessile, thus affecting the balance and stability of the buoy. If the ocean buoy is of a metal structure, it will suffer accelerated corrosion, affecting its function and service life. Moreover, the antifouling coating of the buoy should not only achieve an antifouling effect, but also further satisfy the requirements of collision resistance and excellent weatherability. Polyurethane protective coating has better impact resistance and collision resistance, but its antifouling property is not favorable. Chinese Patent Publication No. CN105273594A (Patent No. 201510735804.0) discloses a silicone polyurethane/polyurea antifouling material bonded with an antifouling factor as well as a preparation and an application thereof, wherein the silicone polyurethane/polyurea antifouling material bonds an antifouling factor to a polyurethane chain, so that an antifouling ability is enhanced. Chinese Patent Publication No. CN109867765A (Patent No. 201910150377.8) discloses long-acting sustained-release biodegradable antifouling polyurethane and a preparation method thereof, wherein the antifouling polyurethane bind
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.