Abstract

A method of applying a coating to a substrate includes forming a slurry by mixing elemental precursors of gettering particles, diffusive particles, matrix material, and a carrier fluid; applying the slurry to a substrate; and sintering the slurry to form a composite material. The sintering causes the elemental precursors to react with one another to form gettering particles. An article is also disclosed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method of applying a coating to a substrate, comprising: forming a slurry by mixing elemental precursors of gettering particles, diffusive particles, matrix material, and a carrier fluid; applying the slurry to a substrate; and sintering the slurry to form a composite material, whereby the sintering causes the elemental precursors to react with one another to form gettering particles.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the elemental precursors include silicon and the gettering particles are intermetallic silicides.

  3. Claim 3Depends on #2

    The method of claim 2, wherein the elemental precursors include silicon and a refractory metal.

  4. Claim 4Depends on #1

    The method of claim 1, further comprising the step of applying a topcoat.

  5. Claim 5Depends on #4

    The method of claim 4, wherein the step of applying the topcoat is performed before the step of sintering the slurry.

  6. Claim 6Depends on #1

    The method of claim 1, wherein the sintering is performed at a temperature between about 1000 ° C. and 1400 ° C. in an inert atmosphere.

  7. Claim 7Depends on #1

    The method of claim 1, further comprising the step of subjecting the slurry to a low-heat treatment prior to the sintering step, and wherein sintering step is performed at a first temperature, and the low-heat treatment is performed at a second temperature lower than the first temperature.

  8. Claim 8Depends on #1

    The method of claim 1, wherein after the mixing step, the elemental precursors are embedded in one another.

Technical Overview & Description

BACKGROUND A gas turbine engine typically includes a fan section, a compressor section, a combustor section and a turbine section. Air entering the compressor section is compressed and delivered into the combustion section where it is mixed with fuel and ignited to generate a high-energy exhaust gas flow. The high-energy exhaust gas flow expands through the turbine section to drive the compressor and the fan section. The compressor section typically includes low and high pressure compressors, and the turbine section includes low and high pressure turbines. This disclosure relates to composite articles, such as those used in gas turbine engines. Components, such as gas turbine engine components, may be subjected to high temperatures, corrosive and oxidative conditions, and elevated stress levels. In order to improve the thermal and/or oxidative stability, the component may include a protective barrier coating. SUMMARY A method of applying a coating to a substrate according to an exemplary embodiment of this disclosure, among other possible things includes forming a slurry by mixing elemental precursors of gettering particles, diffusive particles, matrix material, and a carrier fluid; applying the slurry to a substrate; and sintering the slurry to form a composite material. The sintering causes the elemental precursors to react with one another to form gettering particles. In a further example of the foregoing, the elemental precursors include silicon and the gettering particles are intermetallic silicides. In a further example of any of the foregoing, the elemental precursors include silicon and a refractory metal. In a further example of any of the foregoing, the method includes the step of applying a topcoat. In a further example of any of the foregoing, the step of applying the topcoat is performed before the step of sintering the slurry. In a further example of any of the foregoing, wherein the sintering is performed at a temperature between about 1000 ° C. and 1

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (14)

PatentTitleYearCitations

Non-Patent Literature (2)

  • International Search Report and Written Opinion for International Patent Application No. PCT/US2022/28272 dated Feb. 6, 2023.
  • International Preliminary Report on Patentability for International Patent Application No. PCT/US2022/28272 dated Nov. 16, 2023.