US 12,203,152 B2#3631182 Most CitedActiveUnited States (USPTO)Utility

Method of preparing biodegradable Zn — Mg — Bi zinc alloy

0Forward Citations (#3631182 Global)
0.0/yrCitation Velocity (#3631182 Global)
0.00Citation PageRank (#3631182 Global)
5Prior Art Cited
6Claims (1 Indep. · 5 Dep.)
2Drawings / Sheets

Abstract

A method of preparing biodegradable Zn — Mg — Bi zinc alloy includes: melting magnesium under an inert atmosphere to obtain a magnesium melt; adding bismuth particles to the magnesium melt followed by reaction under stirring and heat preservation treatment to obtain a Mg — Bi alloy melt; allowing the Mg — Bi alloy melt to stand in a furnace; subjecting the Mg — Bi alloy melt to refining, slagging-off, casting and demoulding to obtain Mg-50 wt. % Bi alloy ingot; melting zinc to obtain a zinc melt; adding the Mg-50 wt. % Bi alloy ingot and pure magnesium or pure bismuth followed by heating to a preset temperature, stirring and heat preservation to obtain a Zn — Mg — Bi alloy melt; allowing the Zn — Mg — Bi alloy melt to stand in a furnace followed by refining, slagging-off, casting and demoulding to obtain the biodegradable Zn — Mg — Bi zinc alloy.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.

Claims (6 — 1 Independent, 5 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a biodegradable Zn — Mg — Bi zinc alloy, comprising: (1) melting magnesium under an inert atmosphere to obtain a magnesium melt; adding bismuth particles to the magnesium melt followed by reaction under stirring and heat preservation treatment to obtain a Mg — Bi alloy melt; allowing the Mg — Bi alloy melt to stand in a furnace; and subjecting the Mg — Bi alloy melt to refining, slagging-off, casting and demoulding to obtain a Mg-50 wt. % Bi alloy ingot; and (2) melting zinc to obtain a zinc melt; adding the Mg-50 wt. % Bi alloy ingot and pure magnesium or pure bismuth to the zinc melt, followed by heating under stirring, and heat preservation to obtain a Zn — Mg — Bi alloy melt; allowing the Zn — Mg — Bi alloy melt to stand in the furnace; and subjecting the Zn — Mg — Bi alloy melt to refining, slagging-off, casting and demoulding to obtain the biodegradable Zn — Mg — Bi zinc alloy.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the Mg — Bi alloy melt is prepared through steps of: melting the magnesium at 650-700 ° C. in argon gas in the presence of a covering agent followed by keeping at 650-700 ° C. for 60-90 min to obtain the magnesium melt; and adding the bismuth particles to the magnesium melt followed by reaction under stirring at 50-80 rpm and 640-660 ° C. for 20-30 min and keeping at 640-660 ° C. for 12-15 min to obtain the Mg — Bi alloy melt.

  3. Claim 3Depends on #1

    The method of claim 1, wherein in step (1), the casting is performed at 580-610 ° C.; and the Mg — Bi alloy melt is allowed to stand in the furnace for 3-5 min.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the Zn — Mg — Bi alloy melt is prepared through steps of: melting the zinc at 420-500 ° C. in argon gas for 60-90 min to obtain the zinc melt; adding the Mg-50 wt. % Bi alloy ingot and pure magnesium or pure bismuth to the zinc melt followed by stirring at 50-80 rpm and 640-660 ° C. for 20-30 min and keeping at 640-660 ° C. for 12-15 min to obtain the Zn — Mg — Bi alloy melt.

  5. Claim 5Depends on #4

    The method of claim 4, wherein the Zn — Mg — Bi alloy melt comprises 6-20% by volume of Mg 3 Bi 2 as main strengthening phase; the Mg 3 Bi 2 is produced by reaction of magnesium atoms and bismuth atoms; and a weight ratio of bismuth to magnesium in the Zn — Mg — Bi alloy melt is less than or equal to 2.2.

  6. Claim 6Depends on #1

    The method of claim 1, wherein in step (2), the casting is performed at 510-550 ° C., and a mold used in the demoulding is preheated to 180-200 ° C.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application is a divisional of U.S. patent application Ser. No. 17/840,871, filed Jun. 15, 2022, which claims the benefit of priority from Chinese Patent Application No. 202111525807.3, filed on Dec. 14, 2021. The content of the aforementioned applications, including any intervening amendments thereto, is incorporated herein by reference in its entirety. TECHNICAL FIELD This application relates to biodegradable multi-component zinc alloy, and more particularly to a method of preparing biodegradable Zn — Mg — Bi zinc alloy. BACKGROUND As a kind of biomaterials with excellent biocompatibility and capable of interacting with living organisms, biomedical materials can be used alone or applied as a complex system to guide the medical treatment, implementation of biological function or diagnosis process. With the rapid development of life science and material science, it is widely expected that the medical devices or implants implanted in the body merely play a temporary or short-term replacement role for rehabilitation, and will be gradually degraded and absorbed by the human body along with the repair of damaged tissues or organs. This therapeutic strategy has excellent biocompatibility, and is free of toxic side effects, adverse biological reactions and harmful stimuli. Consequently, the research and development of biomedical materials has drawn extensive attention. Extensive researches have been conducted on the development of biodegradable medical materials. Traditional bioimplant materials, such as polymers, cobalt alloys, titanium alloys and medical stainless steel, require to be removed through a secondary operation, which will traumatize the human body. In addition, some implant materials will release harmful ions, which will cause secondary damage to the healed tissue, resulting in some human syndromes. By comparison, biodegradable materials will be gradually degraded after being implanted into the human body, and the

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (5)

PatentTitleYearCitations

Non-Patent Literature (10)

  • English language machine translation of CN-109778035-A. Generated Nov. 14, 2024. (Year: 2024).
  • H. R. Bakhsheshi-Rad et al.,
  • “
  • Thermal Characteristics, Mechanical Properties, In Vitro Degradation and Cytotoxicity of Novel Biodegradable Zn
  • —
  • Al
  • —
  • Mg and Zn
  • —
  • Al