hottub.patents
US 12,201,969 B2#3632197 Most CitedActiveUnited States (USPTO)Utility

Method of forming an inorganic oxide coating on a monolith article

0Forward Citations (#3632197 Global)
0.0/yrCitation Velocity (#3632197 Global)
0.00Citation PageRank (#3632197 Global)
8Prior Art Cited
18Claims (1 Indep. · 17 Dep.)
3Drawings / Sheets

Abstract

A method of forming an inorganic oxide coating on a monolith article to produce a coated monolith article suitable for the treatment of an exhaust gas comprises spraying, as a dry particulate aerosol, inorganic particles and a silicone resin to form a coating layer. The present invention also provides an uncalcined porous monolith article for use in forming a monolith article for the treatment of an exhaust gas. The uncalcined monolith article comprises a dry particulate composition comprising inorganic particles and a silicone resin.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.

Claims (18 — 1 Independent, 17 Dependent)

  1. Claim 1Independent Claim

    A method of forming an inorganic oxide coating on a monolith article for the treatment of an exhaust gas, the method comprising: providing a porous monolith article comprising a plurality of channels for the passage of an exhaust gas, each channel having a gas-contacting surface; spraying onto the gas-contacting surface, as a dry particulate aerosol, inorganic particles and a silicone resin to form a coating layer; and calcining the coating layer to provide a coated monolith article.

  2. Claim 2Depends on #1

    The method according to claim 1, wherein the monolith article is a catalytic wall-flow filter.

  3. Claim 3Depends on #1

    The method according to claim 1, wherein either: (i) the inorganic particles are sprayed onto the gas-contacting surface as a first dry particulate aerosol to form an inorganic particle layer and the silicone resin is then sprayed onto the inorganic particle layer as a second dry particulate aerosol to form the coating layer; or (ii) a mixture of the inorganic particles and silicone resin is sprayed onto the gas-contacting surface as a dry particulate aerosol to form the coating layer.

  4. Claim 4Depends on #1

    The method according to claim 1, wherein the silicone resin has a molecular weight of greater than 10,000, and less than 200,000.

  5. Claim 5Depends on #1

    The method according to claim 1, wherein the silicone resin has a glass transition temperature (Tg) of greater than 30 ° C. and less than 80 ° C.

  6. Claim 6Depends on #1

    The method according to claim 1, wherein the silicone resin has the formula [R x SiX y O z] n, wherein R is an alkyl or aryl, X is a functional group bonded to silicon, and wherein z is more than 1 and less than 2.

  7. Claim 7Depends on #6

    The method according to claim 6, wherein y is less than 1 and/or wherein y is less than x.

  8. Claim 8Depends on #6

    The method according to claim 6, wherein the silicone resin has a degree of crosslinking of greater than 65%, and less than 80%.

  9. Claim 9Depends on #6

    The method according to claim 6, wherein R is one or more of C 1 -C 6 alkyls and phenyl.

  10. Claim 10Depends on #6

    The method according to claim 6, wherein X is one or more of OH and C 1 -C 6 alkoxy.

  11. Claim 11Depends on #1

    The method according to claim 1, wherein the silicon dioxide content of the silicone resin is greater than 80 wt %.

  12. Claim 12Depends on #1

    The method according to claim 1, wherein the inorganic particles are selected from the group consisting of zeolites, refractory oxides, and their mixtures.

  13. Claim 13Depends on #12

    The method according to claim 12, wherein the inorganic particles are refractory oxide particles comprising calcium aluminate, fumed alumina, fumed silica, fumed titania, fumed zirconia, fumed ceria, alumina aerogel, silica aerogel, titania aerogel, zirconia aerogel, ceria aerogel or a mixture thereof.

  14. Claim 14Depends on #1

    The method according to claim 1, wherein the inorganic particles have a d 50 by volume of greater than 0.2 μ m and less than 25 μ m.

  15. Claim 15Depends on #1

    The method according to claim 1, wherein a mixture of the inorganic particles and silicone resin is sprayed onto the gas-contacting surface as a dry particulate aerosol to form the coating layer, and wherein in the mixture, the ratio of inorganic particles to silicone resin, by weight, is greater 0.9, and less than 2.5.

  16. Claim 16Depends on #1

    The method according to claim 1, wherein calcining comprises heating to a temperature of at least 400 ° C., and at most 530 ° C.

  17. Claim 17Depends on #1

    The method according to claim 1, wherein the monolith article comprises one or more platinum group metals.

  18. Claim 18Depends on #1

    The method according to claim 1, wherein the dry particulate aerosol is formed from a dry particulate composition having a tapped density of less than 1.5 g/cm 3.

Technical Overview & Description

FIELD OF THE INVENTION The present invention relates to a method of forming an inorganic oxide coating on a monolith article. In particular, the coated monolith article is suitable for the treatment of an exhaust gas. More particularly, the method comprises spraying, as a dry particulate aerosol, inorganic particles and a silicone resin to form a coating layer. The present invention also relates to an uncalcined porous monolith article for use in forming a monolith article for the treatment of an exhaust gas. In particular, the uncalcined monolith article comprises a dry particulate composition comprising inorganic particles and a silicone resin. BACKGROUND OF THE INVENTION There are concerns about emissions of particulate matter (PM), commonly referred to as soot, from internal combustion engines and especially from diesel and gasoline engines in automotive applications. The main concerns are associated with potential health effects, and in particular with very tiny particles having sizes in the nanometer range. Diesel particulate filters (DPFs) and gasoline particulate filters (GPFs) have been fabricated using a variety of materials including sintered metal, ceramic or metal fibers etc., with the most common type in actual mass production being the wall-flow kind made from porous ceramic material fabricated in the form of a monolithic array of many small channels running along the length of the body. Alternate channels are plugged at one end so the exhaust gas is forced through the porous ceramic channel walls that prevent most of the particulate from passing through so only filtered gas enters the environment. Ceramic wall-flow filters in commercial production include those made from cordierite, various forms of silicon carbide and aluminum titanate. The actual shape and dimensions of practical filters on vehicles as well as properties such as the channel wall thickness and its porosity etc. depend on the application concerned. The average dimensions of the pores

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (8)

PatentTitleYearCitations

Non-Patent Literature (5)

  • Heck, et al.,
  • “
  • Catalytic air pollution control
  • ”
  • , Wiley, pp. 338-340, 2009.