US 12,199,265 B2#3634489 Most CitedActiveUnited States (USPTO)Utility

Method and apparatus for preparing dry electrode sheet for secondary battery, dry electrode sheet for secondary battery, electrode for secondary battery and secondary battery

0Forward Citations (#3634489 Global)
0.0/yrCitation Velocity (#3634489 Global)
0.00Citation PageRank (#3634489 Global)
14Prior Art Cited
10Claims (2 Indep. · 8 Dep.)
3Drawings / Sheets

Abstract

A method of manufacturing a dry electrode sheet for a secondary battery includes providing a dry electrode composition comprising an electrode active material and a binder, a calendering operation of preparing an electrode sheet by passing the dry electrode composition through a calender roll including three or more rolls. The calendering operation includes a first electrode sheet manufacturing operation of manufacturing a first electrode sheet by injecting the dry electrode composition between two adjacent rolls spaced apart from each other by a first interval W1, and an electrode sheet manufacturing operation of manufacturing a dry electrode sheet by inserting the first electrode sheet between two adjacent rolls spaced apart from each other by a second interval W2. The first interval W1 and the second interval W2 have a compression rate of 0.10 or more and 0.65 or less, represented by the equation (1) compression rate=(W1 − W2)/W1.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.

Claims (10 — 2 Independent, 8 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a dry electrode sheet for a secondary battery, the method comprising: providing a dry electrode composition comprising an electrode active material and a binder; and feeding the dry electrode composition directly to a calendering operation wherein the calendering operation includes: injecting the dry electrode composition between two adjacent rolls spaced apart from each other by a first interval W1 to provide a first electrode sheet, inserting the first electrode sheet between two adjacent rolls spaced apart from each other by a second interval W2 to provide the dry electrode sheet, and wherein the first interval W1 and the second interval W2 have a compression ratio expressed by the following equation (1) of 0.10 or more and 0.27 or less, Compression Ratio=(W 1 − W 2)/ W 1 (equation (1)), wherein the two adjacent rolls in the injecting step includes a first roll and a second roll, and the two adjacent rolls in the inserting step includes the second roll and a third roll, the dry electrode composition is introduced between the first roll and the second roll to prepare the first electrode sheet, and the first electrode sheet is introduced between the second roll and the third roll to manufacture the dry electrode sheet, wherein a rotational speed V1 of the first roll, a rotational speed V2 of the second roll, and a rotational speed V3 of the third roll satisfy the following formula (2) V 1 < V 2 < V 3 (2), wherein a rotation speed ratio of the first roll, the second roll and the third roll V1:V2:V3 is 10:11 to 20:12 to 40.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the first interval W1 is 100 to 500 μ m, and the second interval W2 is 60 to 450 μ m.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the two adjacent rolls in the injecting step includes the first roll and the second roll, and the two adjacent rolls in the inserting step includes the third roll and a fourth roll, the dry electrode composition is introduced between the first roll and the second roll to prepare the first electrode sheet, and the first electrode sheet is introduced between the third roll and the fourth roll to manufacture the dry electrode sheet.

  4. Claim 4Depends on #3

    The method of claim 3, wherein the rotational speed V1 of the first roll, the rotational speed V2 of the second roll, the rotational speed V3 of the third roll, and a rotational speed V4 of the fourth roll satisfy the relationship of the following formula (3), V 1 < V 2 < V 3 < V 4 (3).

  5. Claim 5Depends on #1

    The method of claim 1, wherein the injecting and inserting steps occurs at 40 ° C. to 200 ° C.

  6. Claim 6Depends on #1

    The method of claim 1, wherein the binder is a fiberizable binder.

  7. Claim 7Depends on #1

    The method of claim 1, wherein the binder is at least one selected from the group consisting of polytetrafluoroethylene, polyethylene oxide, polyacrylonitrile, polyvinylidene fluoride, cellulose derivative and propionate.

  8. Claim 8Depends on #1

    The method of claim 1, further comprising kneading the dry electrode composition.

  9. Claim 9Depends on #1

    The method of claim 1, wherein the dry electrode sheet has a tensile strength of 0.50 N/mm2 or more.

  10. Claim 10Independent Claim

    A method of manufacturing a dry electrode sheet for a secondary battery, the method comprising: providing a dry electrode composition comprising an electrode active material and a binder; and feeding the dry electrode composition directly to a calendering operation wherein the calendering operation includes: injecting the dry electrode composition between two adjacent rolls spaced apart from each other by a first interval W1 to provide a first electrode sheet, inserting the first electrode sheet between two adjacent rolls spaced apart from each other by a second interval W2 to provide the dry electrode sheet, and wherein the first interval W1 and the second interval W2 have a compression ratio expressed by the following equation (1) of 0.10 or more and 0.27 or less, Compression Ratio=(W 1 − W 2)/ W 1 (equation (1)), wherein the two adjacent rolls in the injecting step includes a first roll and a second roll, and the two adjacent rolls in the inserting step includes the second roll, a third roll and a fourth roll, the dry electrode composition is introduced between the first roll and the second roll to prepare the first electrode sheet, and the first electrode sheet is introduced between the third roll and the fourth roll to manufacture the dry electrode sheet, wherein a rotational speed V1 of the first roll, a rotational speed V2 of the second roll, a rotational speed V3 of the third roll, and a rotational speed V4 of the fourth roll satisfy the following relationship, V 1 > V 2 ≤ V 3 > V 4 (4) where in formula (4), V1 < V4 wherein a rotation speed ratio V1:V2:V3:V4 of the first roll, the second roll, the third roll, and the fourth roll is 10:11 to 20:11 to 20:12 to 40.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATION(S) This application claims benefit of priority to Korean Patent Application No. 10-2022-0062784 filed on May 23, 2022 in the Korean Intellectual Property Office, the disclosure of which is incorporated herein by reference in its entirety. BACKGROUND 1. Field The present disclosure relates to a method and apparatus for manufacturing a dry electrode sheet for a secondary battery, a dry electrode sheet for a secondary battery, an electrode for a secondary battery, and a secondary battery. 2. Description of Related Art Lithium secondary batteries are used not only as an energy source for mobile devices, but also as a power source for electric vehicles (EVs) and hybrid electric vehicles (HEVs), and demand therefor is also continuously increasing. The manufacturing process of a lithium secondary battery is divided into three stages, an electrode process for manufacturing electrodes, an assembly process for manufacturing an electrode assembly, and a chemical process that activates the battery. The electrode process is re-divided into a mixing process of mixing an electrode mixture containing an electrode active material, a coating process of coating the electrode mixture on a current collector to form an electrode mixture layer, a drying operation of removing the solvent in the electrode mixture layer, a rolling process of forming an electrode mixture layer to have a desired thickness, and a slitting process to cut the electrode into a predetermined shape. Generally, in the electrode mixture layer, an electrode mixture slurry is prepared by dispersing an electrode mixture including an electrode active material and a binder in a solvent such as water or NMP, and after applying the electrode mixture slurry to the current collector, it is dried to evaporate the solvent contained in the electrode mixture layer. However, in the process of evaporating the solvent, pinholes or cracks may be formed in the electrode mixture layer, resulting in

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • Extended European Search Report for the European Patent Application No. 23174745.2 issued by the European Patent Office on Oct. 17, 2023.