Abstract
A method comprising a) drying a support material comprising silica at temperature in the range of from about 150° C. to about 220° C. to form a dried support; b) contacting the dried support with methanol to form a slurried support; c) subsequent to b), cooling the slurried support to a temperature of less than about 60° C. to form a cooled slurried support; d) subsequent to c), contacting the cooled slurried support with a titanium alkoxide to form a titanated support; and e) thermally treating the titanated support by heating to a temperature of equal to or greater than about 150° C. for a time period of from about 5 hours to about 30 hours to remove the methanol and yield a dried titanated support.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method comprising: a) drying a silica support material at a temperature in a range of from about 150° C. to about 220° C. to form a dried support; b) contacting the dried support with a solution comprising methanol containing less than 0.1 wt. % water and a basic chromium acetate to form a chrominated slurried support; c) cooling the chrominated slurried support to a temperature of less than about 60° C. to form a cooled slurried support; d) contacting the cooled slurried support with a titanium n-propoxide to form a titanated slurried support; e) thermally treating the titanated slurried su
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.