The disclosure provides a method for preparing a hollow fiber membrane by melt spinning-stretching and selective swelling, including: preparing a nascent hollow fiber by melt spinning in an inert gas protective atmosphere by using an amphiphilic block copolymer as a film forming material, and stretching the nascent hollow fiber in the cooling process, a stretch rate being controlled at 200-540 mm/min, and a stretch ratio being controlled at 150-600%; immersing the obtained hollow fiber in a swelling solvent, and treating the hollow fiber in a water bath at 65° C. for 1 h; and then transferring the hollow fiber into a long-chain alkane solvent, treating the hollow fiber at the same temperature for 1-12 h, and after the completion of the treatment, immediately taking out the hollow fiber and drying the hollow fiber to obtain the hollow fiber membrane with a bicontinuous porous structure. By combining the melt spinning-stretching and the selective swelling, the method of the disclosure can synchronously and continuously improve the permeability and selectivity of the hollow fiber membrane. The treatment in the long-chain alkane solvent can make the polar chain excessively enriched on

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    preparing a nascent hollow fiber by melt spinning in an inert gas protective atmosphere by using an amphiphilic block copolymer as a film forming material, and stretching the nascent hollow fiber in a cooling process, a stretch rate being controlled at 250-500 mm/min, and a stretch ratio being controlled at 300-550%; the amphiphilic block copolymer in 1) is composed of block A and block B (A-B), wherein the block A is selected from any one of polysulfone (PSF), polyethersulfone (PES), polyphenylsulfone (PPSU) and polylactic acid (PLA), the block B is selected from any one of polyethylene glyco

  2. Claim 2Independent Claim

    immersing the hollo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (5)

  • International Search Report (with English translation) and Written Opinion issued in PCT/CN2022/082365, dated Jun. 7, 2022, 11 pages provided.
  • Notice of Grant issued in corresponding Chinese Application No. 202110313177.7, dated Aug. 25, 2022, with English translation.
  • Office Action issued in corresponding Chinese Application No. 202110313177.7, dated Jul. 12, 2022, with English translation.
  • Zhang et al., “Simultaneous zwitterionization and selective swelling-induced pore generation of block copolymers for antifouling ultrafiltration membranes”, Journal of Membrane Science, vol. 599, Apr. 1, 2020.
  • Zhong et al.,“Selective swelling of block copolymer ultrafiltration membranes for enhanced water permeability and fouling resistance”, Journal of Membrane Science, vol. 558, Jul. 15, 2018, pp. 106-112.