Glass-based articles having high stress magnitude at depth

2Forward Citations (#44909680 Global)
0.7/yrCitation Velocity (#12097141 Global)
0.89Citation PageRank (#48225677 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Glass-based articles have a first surface and a second surface opposing the first surface defining a thickness (t) and a center between the first surface and the second surface, the glass-based article containing Li 2 O, ion-exchanged potassium and ion-exchanged sodium. The glass-based article has a stress profile including a hump stress region extending from the first surface (or a point below the first surface) to an apex in a range of 0.001·t and 0.1·t. Compressive stress at the apex is from 25 to 750 MPa. The hump region comprises an area of increasing stress and an area of decreasing stress. Depth of compression is from 0.1·t to 0.25·t. A tensile stress region extends from the depth of compression to a maximum tensile stress.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A glass-based article comprising: a first surface and a second surface opposing the first surface defining a thickness (t) and a center between the first surface and the second surface, the glass-based article comprising Li 2 O, ion-exchanged potassium and ion-exchanged sodium; and a stress profile comprising a hump stress region extending from the first surface or a point below the first surface to an apex in a range of 0.001·t and 0.1·t, a compressive stress at the apex in a range of 25 MPa and 750 MPa, wherein at least one point of the stress profile of the hump stress region between the fi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
WO 0,047,529 A1Strengthening, crack arrest and multiple cracking in brittle materials using residual stresses—25
US 6,472,068 B1Glass rupture disk200240
US 6,516,634 B1Strengthening, crack arrest and multiple cracking in brittle materials using residual stresses200375
EP 1,291,631 A1A glass with functions of sensor for detecting fracture, stress and strain, and corresponding method of fabrication thereof—9
EP 1,593,658 A1Chemically and thermally pre-stressable lithium aluminosilicate float glass of high temperature resistance—43
US 2005250639 A1Lithium-aluminosilicate flat float glass—138
JP 2005320234 ALithium aluminosilicate flat float glass with high thermal stability capable of being chemically or thermally tempered—56
WO 2009/041618 A1Glass substrate for magnetic disk, process for producing the glass substrate, and magnetic disk—16
US 2009220761 A1Ion exchanged, fast cooled glasses—189
CN 101,689,376 AGlass substrate for magnetic disk, method for producing same, and magnetic disk—8
US 2010190038 A1Glass substrate for magnetic disk and manufacturing method of the same—21
WO 2010/147650 A2Treatment of particles for improved performance as proppants—6
US 2010326657 A1Treatment of particles for improved performance as proppants—7
WO 2011/097314 A2Enhanced chemical strengthening glass of covers for portable electronic devices—15
JP 2011527661 A民生用途のための圧縮面を有するガラス—68
SG 178,005 A1Glass substrate for magnetic disk and manufacturing method of the same—1
US 2012088067 A1Non-contact polishing techniques for reducing roughness on glass surfaces—10
US 2012135153 A1Glass substrate for magnetic disk and manufacturing method of the same—16
US 8,193,128 B2Treatment of particles for improved performance as proppants20124
WO 2012/074983 A1Glass with surface and central regions under compression—31
US 2012194974 A1Enhanced chemical strengthening glass for portable electronic devices—85
AU 2011212982 A1Enhanced chemical strengthening glass of covers for portable electronic devices—1
US 2012216569 A1Method of producing constancy of compressive stress in glass in an ion-exchange process—9
US 2012216565 A1Method of producing constancy of compressive stress in glass in an ion exchange process—13
CN 102,791,646 AReinforced chemically strengthened glass for covers of portable electronic devices—12
KR 20120128657 AEnhanced chemical strengthening glass of covers for portable electronic devices—5
EP 2,531,459 A2Enhanced chemical strengthening glass of covers for portable electronic devices—1
CN 103,097,319 AGlass sheet—32

Non-Patent Literature (5)

  • Bradenburg; “Stress in Ion-Exchanged Glass Waveguides”; Journal of Light wave Technology, vol. LT-4, No. 10, 1986, pp. 1580-1593.
  • Chinese Patent Application No. 201980020804.9, Office Action dated Mar. 4, 2022, 18 pages (08 pages of English Translation and 10 pages of Original document), Chinese Patent Office.
  • International Search Report and Written Opinion of the International Searching Authority; PCT/US2019/014838; dated May 7, 2019; 13 Pages; European Patent Office.
  • Japanese Patent Application No. 2020-540793, Office Action dated Mar. 17, 2022, 6 pages (3 pages of English Translation and 3 pages of Original Document), Japanese Patent Office.
  • Japanese Patent Application No. 2020-540793, Office Action, dated Jan. 4, 2023, 6 pages (3 pages of English Translation and 3 pages of Original Copy); Japanese Patent Office.