Patents
US 11,713,282 B2#94830617 Most CitedActiveUnited States (USPTO)Utility

Combustion chamber hot face refractory lining

0Forward Citations (#94830617 Global)
0.0/yrCitation Velocity (#94830617 Global)
0.56Citation PageRank (#94830617 Global)
24Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for producing a refractory lining in a combustion chamber operating in a reducing atmosphere. The lining includes at least one or more Zirconia (Zr)-based refractory lining members comprising one or more Zr-based parts. The Zr-based parts comprise at least 90 wt. %, preferably at least 95 wt. %, of monoclinic ZrO 2 and/or partially stabilized ZrO 2 and/or fully stabilized ZrO 2 , wherein the total content of tetragonal and cubic ZrO 2 amounts to at least 20 wt. %, preferably more than 35 wt. %, as well as Zr based refractory lining members and methods for manufacturing the Zr based refractory lining members.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a shaped and fired zirconia refractory material in form of coating layer on an alumina based refractory material, the method comprising the steps of: a) providing a shaped refractory of an Al 2 O 3 -based refractory material, optionally with a corresponding cleaning of the surface to be coated, b) applying a powder dispersion comprising granular stabilized fused ZrO 2 raw material powder in form of a conditioned carrier fluid onto at least one surfaces of the shaped AI 2 O 3 based refractory material, and c) drying the applied power dispersion followed by a thermal tre

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 2,854,739 AMultiple coated molybdenum base article195811
US 2,906,007 ASintered bearing composition195910
US 3,175,919 AZirconia refractory196520
US 3,887,387 AShaped zirconium oxide bodies of high strength197535
US 4,344,904 ASintering method of zirconia198238
US 4,513,089 ASuperrefractory dry ramming material based on zirconium oxide for the lining of induction-type crucible furnaces198526
US 4,659,680 AStabilized zirconia bodies of improved toughness198742
EP 0,235,936 A1Magnesia partially-stabilized Zirconia—7
US 4,835,123 AMagnesia partially-stabilized zirconia198926
US 4,975,397 ASintered molding, a method for producing it and its use199022
WO 9,015,020 A2High-temperature aerosol decomposition process and products produced—9
JP H0826860 AJig for baking—6
US 5,562,998 ADurable thermal barrier coating1996114
US 5,780,178 AScandia, yttria-stabilized zirconia for ultra-high temperature thermal barrier coatings199821
US 6,284,692 B1t′-phase zirconias for high temperature applications200113
EP 1,772,441 A1Ceramic material and coatings for high temperature service—55
US 2007207334 A1Jig For Electronic Part Firing—3
US 7,601,442 B2Jig for calcining electronic component20092
DE 102008027882 A1Preparing carbon monoxide rich, methane-poor gas, comprises autothermal reforming of hydrocarbon-containing fuel with carbon dioxide, steam and an oxidant—13
US 7,807,098 B2Advanced erosion-corrosion resistant boride cermets20102
US 2011220285 A1Methods and systems for texturing ceramic components—8
US 2013280638 A1Fused powder of yttria-stabilised zirconia—8
US 2018290931 A1Target tiles for an autothermal reformation/secondary reformation unit—3
US 10,370,298 B2Target tiles for an autothermal reformation/secondary reformation unit20193

Non-Patent Literature (2)

  • H. Tsubakino et al., “Effect of Alumina Addition on the Tetragonal-to-Monoclinic Phase Transformation in Zirconia-3 mol% Yttria,” Journal of the American Ceramic Society, vol. 74, No. 2, pp. 440-443, 1991.
  • Harushige Tsubakino et al., “Effect of Alumina Addition on the Tetragonal-to-Monoclinic Phase Transformation in Zirconia-3 mol% Yttria.” Journal of the American Ceramic Society, vol. 74, No. 2, pp. 440-443, 1991.